Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: wide belt questions

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

wide belt questions

7/5/16       
John Member

Website: http://woodmanseewoodwrights.com

I recently picked up a used SCMI Uno 36" wide belt, single drum with platen. After replacing a couple switches it's running fine. I have made up a 3' wide slab using 3/4" melamine with a 80 grit section of belt and have trued up the rubber drum. The platens were wore down pretty bad so I replaced the felt with new from McMaster Carr and new graphite. I'm having trouble getting the rebuilt platen to leave me a smooth final pass when running cabinet doors through. The initial passes using just the drum I do at 100 grit. I am trying to use both 120 and 150 with the platen, light passes, but I'm getting slight ridges/valleys. Nothing huge but more than there should be. Is there such a thing as trueing up the graphite on the platen? Also, I'm not that happy with the belts I've been using, don't seem to last long at all. I think these were from Klingspor. What does everyone else use and like? I've heard 3M makes good ones but would like some input before investing in many more. I'm a small, one man shop so not a huge volume of material goes through.

7/5/16       #2: wide belt questions ...
Duster

You might want to take a look at the felt on your platen. If that's not flat, don't expect the graphite cloth to fix it. I've seen sanders with abused platens give the same results you're describing. You could probably pull the platen and run it through the sander to level out the felt, then recover with graphite.

7/5/16       #3: wide belt questions ...
John Member

I have run the felt through to flatten it up and seems good. The graphite seems to be somewhat rough so wasn't sure if it needed any break in time or smoothing up. Are there different grades of graphite rolls?

7/5/16       #4: wide belt questions ...
Duster

I don't know if there are different grades of the graphite cloth, but I wouldn't be suprised if there was. I do know from experience that getting the cloth stretched smoothly and tight over the felt is the hardest part. You definitely don't want any slack or wrinkles.

7/7/16       #5: wide belt questions ...
Kevin

We used the Klingspor belts for years. 3M gave me a few sample belts and after giving them a try i starting buying 3M. Very big difference.

7/7/16       #6: wide belt questions ...
John Member

Website: http://woodmanseewoodwrights.com

Thanks guys, I think I will try 3M's belts. After changing to a new belt I checked the ridge pattern on a sample wood block and it's different than the first belt. It seems like there's a little inconsistency in the belts, not as noticeable if it were a coarser grit but at 150 it needs to be better. My platen may not be the main culprit although I may try and get that smoother too.

7/7/16       #7: wide belt questions ...
Jim

On my old single head timesaver we ran Hermes belts with the zip seam. We had chatter marks with the butt seam belts. It went away with the Hermes belt.

7/30/16       #8: wide belt questions ...
Adam West  Member

Website: http://www.surfprepsanding.com

There is always some inconsistency in sanding belts, especially in cloth. The substraight in cloth is not as flat as paper so the height of the grains is not as accurate as paper.

Graphite cloth often has lumps in it that need to be smoothed out before use. It really depends on the grade used. 303 graphite is the best for consistent finish. The heavy duty is the worst. I often sand it down a bit to smooth out imperfections in the cloth.

If the ridges are running with the direction of feed and not against it, then these two factors will be the most prevelant causes.

When you set your platen to the drum you want to start by lightly sanding a piece of material with the platen retracted. Without moving the machine height you want to stop everything and put the part back underneath the platen. Lower the platen until it very lightly touches the part so you can feel a bit of tension between the part and the sanding belt. Your goal is for the platen to only take a couple thousandths of an inch.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello