Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Critique this CNC-cut frameless sink base

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Critique this CNC-cut frameless sink base

10/18/16       
Gene Davis

All parts 3/4" hard rock maple melamine except for the front panel that backs up the falsefront drawer. That part is cut from prefinished maple plywood, the paintable B side out.

Red color signifies edgebanding which is selected to match whatever we are doing on the fronts. The front panel gets finished to match.

Back nailer-stretchers are 4" and inset 1/8".

Blind dados as shown for deck-to-sides, and all the stretchers. Goes together dry, all fixed with zip-r screws.

Open back for ease of plumbing connections.

No toe because we use adjustable legs and clip the toeboards on.


View higher quality, full size image (728 X 737)


View higher quality, full size image (925 X 836)

10/18/16       #2: Critique this CNC-cut frameless sin ...
Chris

Fine, but an open back seems lazy, non cuztom and cheap. We use a full 1/2" plant on back for fastening

10/19/16       #3: Critique this CNC-cut frameless sin ...
Derrek

Im fine with the open back. To many times ive seen installer hack up a back to clear plumbing, so what looks worse? Sometime we project our own vision on something, that to the customer is completely worthless. If its a big deal to the customer put a back on it. If they are beating you up for every last quarter, save some time and materials and go backless.

10/19/16       #4: Critique this CNC-cut frameless sin ...
JM

Not really sure what you want to critique, its a CAD drawing of a frameless box.

If the lack of back is your concern, Im with Derreck. We make ours with a back, but not because we feel its needed, but to be consistent for the guys in the shop.

10/19/16       #5: Critique this CNC-cut frameless sin ...
Mark V.

Sink backs....I would love to go backless, but I always use backs on sink bases because most of my jobs are remodels and the wall looks nasty around the pipes. Inspectors check there too and the plumber has failed numerous times because he forgot to install escutcheons on his pipes. I’d hate to see what they would do with an open back cabinet.

Sink rails…I haven’t finished them in years and never will, unless I am do some super highend cabinetry. Depending on my mood/finish color, the sink rail (made interior material) is either hanging low enough to allow the top of the doors to rest on it, or it is cut to be flush with the bottom of the false front.

Mark

10/19/16       #6: Critique this CNC-cut frameless sin ...
Pat Gilbert

What am I missing there is a back on the upper picture and probably one on the lower picture but it is white?

The only criticism I have is, how do you connect the cabinet with the next cabinet as the screws will show (8^())

10/19/16       #7: Critique this CNC-cut frameless sin ...
jonathan mahnken

looks good. I go backless on sink cabinets as often ans I can. But I do give customers the choice... for an upcharge. A 4" bottom nailer can many times be problematic with plumbing and electrical outlets in a sink area. Check the plumbing situation. If you are trying to set a standard I would go with more like a 2" bottom nailer just to be on the safe side

10/19/16       #8: Critique this CNC-cut frameless sin ...
Mark V.

Pat,

Stop looking at the pretty pictures and read the first post :-)

Op said, "Open back for ease of plumbing connections."

Mark

10/19/16       #9: Critique this CNC-cut frameless sin ...
Pat Gilbert

got me specs trump drawings.

10/19/16       #10: Critique this CNC-cut frameless sin ...
dustmaker1

That is exactly how we have made our sink boxes for the last 20 years or so. No back, 98% commercial work though. We use dowel construction, 90mm nailers, 180mm sub front and CNC cuts screw pockets on parts to attach counter tops.

Paul R

10/20/16       #11: Critique this CNC-cut frameless sin ...
Pat Gilbert

What do you do about ADA?

10/20/16       #12: Critique this CNC-cut frameless sin ...
dustmaker1

We use a modified version of same cabinet only no bottom for ADA, ends are finished inside and go to floor. Change sub front to 128 tall and bottom nailer to 180 tall. at floor. We can put in a removable base or add toe look to doors but a lot of the time customers just chose to leave open at base so they do not need to mess with it. Since there is not really much left of the ADA sink cabinet we usually send it out RTA .

I forgot we do not use 90mm nailer on regular sink box for top, only bottom is 90 and top nailer is 180 tall to mach sub front. We only make the top nailer 90mm if it is a regular cabinet with full top but open back so top and bottom are the same assembly in that case.

Paul R

10/24/16       #13: Critique this CNC-cut frameless sin ...
Bruce H

I'd drop the false front and run the doors all the way up with a valance behind them. I like my valance made of finished material but depends on what is available at the time it is cut. No bottom rail at the back, it would be in the way of too many plumbing issues most of the time. I run my end panels to the ground and put a toe kick piece under the bottom deck 4" inset off the back wall. That and the front toe kick support the deck. I drop my hinges 64mm on a sink base to clear the valance. I do put in a full back if the cabinet is on an peninsula/island or the wall plumbing is a mess. I'll put in a full back on any sink base if I don't have to install it.

10/24/16       #14: Critique this CNC-cut frameless sin ...
Gene Davis

I'm the o.p. and appreciate the comments here. The design, done in eCabinets and meant to be CNC cut, emulates an identical arrangement (almost) we built when buying out RTA packages.

The only diff was with the RTA sinkbases, there was a 1/4" back slid into full dados in sides and deck.

Half the kitchens we did needed the deck cut for plumbing, the other half the back.

As for the spanner across the front, done in species to match the edgebanding and false drawerfront and doors, we were purists enough then to want to see the match at our 9mm top reveal and when opening the doors.

Those RTA jobs had the back nailers for all bases, top and bottom, of 5/8 particleboard, all pre-machined for pocket screws.

As with most people, one tends to learn something one way, and then, good or bad, stick with it.

We've learned from installing plenty of stone tops and sinks that all you want around your top perimeter is one continuous 3/4" band of support, and this design does that. I tossed the 1/4" back because it did not add much and relieves about half of what installers have to do to get the plumbing run.

The rear lower nailer is where the plumber likes to see a surface-mounted work box and duplex power outlet for the disposal and dishwasher.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello