Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Moving melamine???

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Moving melamine???

10/20/16       
JeffD

Wanted to see if anyone else has experienced this before? Was cutting up a stack of six sheets of basic white melamine today and had a horrible time with it. First ripping them in half on the table saw they kept stalling the blade, as if the material was closing on the cut! Never had this happen before....though I don't use a whole lot of melamine anyway. By the time I had the 6 sheets split the blades teeth were completely glazed with brown gunk....again, never saw that happen before.

But the real problem....the panels moved! The 24"w panels I ripped in 2 pieces are now bowed about 1/32" over 8' of length. The smaller 15"w pieces are bowed a good 1/8"! I know it's not the saw/fence setup because the opposite factory edge has the reverse bow, and it was not there at the beginning!

Anyone else experience their material moving like this before? It's pretty unsettling to be honest. And as I don't have a full sized slider it's going to be a real PITA to straighten the edges....so I'm not a happy camper either! Don't know if it's some kind of low grade product or if something else is causing it?

thanks,
JeffD

10/20/16       #2: Moving melamine??? ...
Mark V.

Jeff,

Happens all the time. Sometimes a lot, sometimes a little, rarely not at all. I have a vertical, so I always rip oversize, then re-rip to straighten one edge and finally rip to final width.

People have said that it is manufacturing stress in the board, but I think that the edges absorb moisture and try to expand and can't till the board is ripped. Btw, the kerf never opens up when the board is ripped. When I drop the top piece on the lower piece (remember I am cutting on a vertical panel saw) there is always a gap in the middle.

I hope this helps...maybe in the future?

Mark

10/21/16       #3: Moving melamine??? ...
door shop guy

I have had it happen the last two times in about the past 6 years and those are the only two times i used melamine...so 100% failure rate for me. Made me want to cuss and throw stuff. Major pita to get everything strait and square. I think its called a banana cut.
I dont do much cabinet work at all but just recently priced some melamine garage cabinets for a good customer. I included a LOT of extra time for the major hassle that i probably would face with the melamine. Didnt get the job and i am glad.

10/21/16       #4: Moving melamine??? ...
Kevin Jenness

I have had the same problem, also occasionally with plywood. Best to be conservative and plan to rip oversize and straighten the rough rips unless the material proves stable enough to do otherwise. Without a saw that can true up a long edge you have a few laborious options:

1. Use a router and straight edge
2. Rough out parts by crosscutting first
3. Get a long aluminum extrusion, clamp it to your fence and run the concave ripped edges against that to true them up.

I see a full size panel saw in your future.

10/22/16       #5: Moving melamine??? ...
jonathan mahnken

Its possible you have some odd sheets, you didnt tell us the brand, but its not likely. Slow down, rip oversized and correct. Dont blame the melamine. All things considered its usually a pretty stable product. Its only a problem on long pieces( over 50" or so) and frameless cabinets. Cross cutting first can be a great solution as long as you have thought out your cuts well. A riving knife or blade spliter will help a little too. Make sure you are using the correct blade for melamine and that its sharp. I notice an increase in this effect when my blades start to dull. If your blade teeth are loading up that quickly try using a blade cleaner, then spraying a dry coat lube on them.This will help you last a little longer before you have to clean the resin off again.

10/22/16       #6: Moving melamine??? ...
JeffD

Thanks for the responses guys, good to know it's not just me! As I said I don't use melamine very often, but I don't remember this happening on the last job about 2 years ago. However that particular batch was a non-stock woodgrain that came directly from Canada, so maybe a better grade? I have no idea what brand this was, I didn't specify when ordering as I didn't think it was necessary. I will bring it up with the rep when he comes by next time though.

Jonathan, what else can I blame if not the melamine....it's moving! I thought the stuff was more stable than this but I guess that's my own ignorance. These are all tall Euro wardrobe cabinets at roughly 87" tall so as bad as it gets I suppose. I couldn't feed any slower, as it was I had to back the sheet out of the saw after cutting about 10" or so and start over as it just wouldn't feed. After the initial rips I replaced the blade with a freshly sharpened blade, (all fairly expensive double sided melamine blades fwiw), and still had problems even on the short crosscuts!

Anyway I used the track saw to straighten the initial edges and then re-ripped on the table saw to get a clean front edge. Ended up spending a good half a day just to get the parts cut for 6 tall wardrobe cabinets.....but I did get them cut!

thanks again,
JeffD

10/22/16       #7: Moving melamine??? ...
jonathan mahnken

If your feed rate was as slow as you say and you were binding a fresh blade then there was probably something wrong with the melamine. My melamine is usually made by AmLam or American forest products. I use melamine in both 5/8 and 3/4 all the time and can not recall ever having a tension/warping problem that bad. So yes i guess you could blame the melamine. The only way to know would be to get in touch with your supplier to see what they sold you, then possiblys test a sheet from another brand. The brand is usually stamped on the edge of the sheet

10/24/16       #8: Moving melamine??? ...
Adam B

Jeff,

check with your supplier to find out what product/quality they are sending you. 90% of the cabinets we build come with white melamine interiors. We have cut 1000's of sheets over the years both on a cnc and regular table saw, and have never had any issues close to what you have described. Minor bowing maybe, but never so bad it couldn't be dealt with. The majority of white melamine that we use is 5/8" Roseburg Duramine with a particle board core.
You really should not have to be dealing the issues that you mentioned above.

10/24/16       #9: Moving melamine??? ...
Matt Krig Member

Banana Boards!! Talk to Rudy at Colonial Saw in MA and he'll explain the science of hot press laminating melamine and how it affects the stability of sheet goods and what you can do. It may be looking for a different melamine supplier.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello