Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Painted cabinets

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Painted cabinets

1/19/17       
Justin H

I have a large new house of cabinets coming up that are all painted. I have only done a few small jobs in the past with painted cabinets. Most have been cherry with a dark stain. Almost to the point I cant wait to do something different.

For finish product I use gemini conversion lacquer. My process was spray inside of boxes with clear, tape off and spray 2 coats of tinted finish on face frames. (stained cabinets always 3 coats but the sales rep said no more than 2 is recommended)

My biggest question is at what price upcharge should painted be at? Comparative to cherry? On a small job I couldn't really get a great time calculation on it. I plan to use soft maple for ff and door styles and rails with mdf center panels. Mdf will be used for all finish ends as well. It seems as I add up my material list of which I generally double (with outsourcing doors and drawers) my total materials are a bunch lower than if it was cherry (obvious) So when I double that figure I am way short of labor. So I added back in about 25% of then double to make up for the extra time involved.

Am I on to the right track? I just want to be competitive on this project as I know they are getting other bids.

Next question would be, what extra time is needed and in what detail/ precaution with painted cabinets. Am I underestimating what it takes compared to a stained cabinet? It seems for the time I save from staining I can tape a lot of cabinets off. But my concern is what steps pry to finishing are more important with painted cabinets than stained? Any insight would be greatly appreciated!

1/19/17       #2: Painted cabinets ...
Briana Banks

Price wise I have a baseline sq-ft price for a natural finish. I tack on about 25% more for a stain and 50% more for paint.

Process wise, I try to avoid masking and spraying. If I can, I will pre-finish entire sheets for the cases, pre-finish the frames and then assemble frames to cases.

1/20/17       #3: Painted cabinets ...
dub

Justin,

We used to do a lot of cherry jobs, but 90% of the jobs over the last 2 years have been painted. Couple of thoughts

1. Conversion varnish: depending on your mil thickness and how aggressive you sand, 2 coats may not be enough coverage. I prime, flatten with 220 grit and then do 2 coats. You have to make sure your not getting it too heavy on areas that overlap. (CV to thick will be prone to cracking at the joints).

2. Pricing: As you see, material cost is much lower, but your finish time is much higher. I charge the same for "painted" or stained (exceptions for Walnut and high gloss). I also have an up charge for very dark colors and black. Is your total price materials x2? I try and keep my materials at 1/3 or under depending on install factors.

Good luck.

dub

1/20/17       #4: Painted cabinets ...
Joel

MDF is a poor choice for finished ends especially on lowers. Mars way to easy.

1/20/17       #5: Painted cabinets ...
Justin h

Dub

When I say materials times 2....that's figuring the cost of my doors and drawers outsourced into all the other materials. So not far off from materials times 3 I suppoce?

1/20/17       #6: Painted cabinets ...
Justin h

And install is added on top of that.

1/20/17       #7: Painted cabinets ...
rich c.

How much you going to charge for your learning curve? I'd hate to do my first painted job on a big project. You should probably sub that part out. You won't have to learn on this job, the cost would be set, and you won't get any call backs in a couple of years if you make some mistakes with materials. It doesn't bode well that you have ignored manufacturer recommendations in the past.

1/23/17       #8: Painted cabinets ...
Jason Balm  Member

Website: waukeecabinetworks.com

Justin, Have you considered just ordering in the doors and FF's finished and building the cases out of UV Ply or melamine?

I am always amazed at how reasonable it is to just outsource those components.

1/23/17       #9: Painted cabinets ...
Justin H

Jason

I have thought about going that route except it would change how I build cabinets. I do all flush ends and bottoms so I don't exactly know the right way to address that in a way to not totally change the way I build. This job will have lots of finished ends so trying to match up color would be a nightmare I think.

From what I can see, the additional time is spent filling in joints that arnt perfect with bondo besides the extra time to deal with crown ect. It seems as if the time that is saved from staining would cancel a lot of that extra time spend on prep out. Taping off boxes goes pretty quick over all. I'm just trying to see if I'm missing bigger issues that could stand out more on a large job than an occasional island or hood.

1/23/17       #10: Painted cabinets ...
Mike Fuson

We do a lot of painted work, I'll give you my thoughts on it. First thing is start using prefinished ply for the interiors, no way you can put the finish on yourself for the price difference of the ply. I rarely have to mask anything off. We have carts with casters, all my faceframes get primed and painted laying down on the carts. We have a large table with soft carpet for assembly. And I've never built a box and attached a faceframe, we lay the frame face down and build the box to it. As far as painting, we prep as good as possible and then prime. Fill any imperfections, scuff and prime again, scuff again and then paint. Make sure the second coat of primer is perfect, don't leave any imperfections thinking that the paint should cover it. In the end there's almost always a mosquito that will land on the wet paint and start doing push-ups ...

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello