Subject: Re: how to create inverse profile of ogee door/window trim

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

how to create inverse profile of ogee door/window trim

3/19/18       
Dirk

i have a question about using standard primed 3.5" MDF door/window molding (w/ same profile in the image) in rail and style configuration over beadboard.

my problem is how to create the vertical stiles (i can use standard trim because the horizontal pieces only need 1 edge routed); i found a router bit that matches the trim profile, so i can make the vertical stiles using 3.5" wide strips of ~1/2" MDF (planed to same thickness) w/ both left and right sides routed.

however, i'd like to cut the inverse profile for the top and bottom pieces of the vertical stiles so they just sort of melt into the rails (very similar as to how raised panel doors are made).

simply put: can i buy a router bit that is basically just the inverse profile of the router bit to which i linked (or do i have to just get creative using several different router bits to make it)?

let me know if anything needs clarified. thanks!

3/19/18       #2: how to create inverse profile of og ...
David R Sochar Member

It appears that you are describing what is called 'cope and stick joinery'. Stick being the profile that comes out of a sticker or molder, and is on the edges. Cope being the opposite profile and is on the ends of rails. Or female cut, if you are into the whole gender specific thing. It is also called stile and rail paneling.

Cope and stick sets are available for shapers and larger equipment. There are a few patterns in router bit, 1/2" tooling, usually lighter in profile as used for window sticking.

Typically, cope and stick tooling is used with a mortise and tenon to complete a joint. You are describing a mock or fake joint, buy you do see the benefit of the cope joint.

I suggest you rethink the project and use solid wood with mortise joints and cope and stick joinery. This will reward your efforts with fine woodwork instead of some stapled mdf that has just stopped by on its way to the landfill.

Simply put: you can have a router bit made for any profile, to your specifications. There are several advertisers here on Woodweb that would be happy to set you up.

3/19/18       #3: how to create inverse profile of og ...
Dirk

thanks for the prompt advice; i'm going to reconsider my options, now.

just out of curiosity, are there any scenarios wherein you might prefer the "cope and stick" method to traditional wainscoting (if you could be assured that the cope and stick joints would keep tight and age well)?

thanks again.

3/19/18       #4: how to create inverse profile of og ...
John Member

You have at least two other options, if you are motivated. You can create cope and stick joints from a single router bit if the pattern is a mirror image around the mid-point. You run the sticking face down against the bearing, and the cope face up with the bearing flush with the front face of the fence.

Another way is to use a jack miter.

John


View higher quality, full size image (3648 X 2736)


View higher quality, full size image (3648 X 2736)


View higher quality, full size image (640 X 480)

3/20/18       #5: how to create inverse profile of og ...
Steve Member

David and others have answered the issue but apparently you haven't entertained yourself with the manuf. catalogs where browsing will find for you the similar or perhaps matching cutters you need off the shelf.

3/20/18       #6: how to create inverse profile of og ...
Dirk

David, it's funny you should mention this way of mitering, i just saw this a few hours ago in a random video (it was about odd woodworking techniques and tools used in making cabinets in Asia). i'll see if that works for me. as far as the router bit being a mirror image, i don't think it is; however, this time i just uploaded the picture of the router bit and profile, so hopefully you can now see it tell me if i'm wrong about it not being able to be used to mirror my trim w/ the same bit.

also, Steve, i'm now looking through some router bit catalogs to see if i can find what i need. pouring through hundreds of bits seemed almost impossible before i knew it was an ogee bit (and inverse) that i was looking for.

thanks again, everyone. i wasn't expecting such a quick response; i'm very appreciative for the help!


View higher quality, full size image (600 X 600)

3/20/18       #7: how to create inverse profile of og ...
Dirk

i think this is what i'm looking for (a double door cutter router bit set), although for what i am planning, the lower mortise and tenon portion wouldn't be necessary (because i would basically just be coping the inverse profile of the MDF trim i was planning on using). i hope that makes sense.


View higher quality, full size image (720 X 720)

3/20/18       #8: how to create inverse profile of og ...
Steve Member

John, just a question of curiosity. Your third pic looks like it was made with a beaded face frame bit as part of a Beaded Face Frame Jig (Kreg) or perhaps others, given both the two matching radii and the width of the rail insert?

3/20/18       #9: how to create inverse profile of og ...
John Member

Steve, the miters were cut with my RAS, not a face frame bit like the Kreg you mentioned. You cut the miters, then use a dado blade or router to clean out the waste. No reason a flat bottom 45 deg router bit wouldn't work, too, I just don't have one.

I think jack miters was how it was done long ago, before cope and stick was invented. I've used the same approach for fitting stile/rail joints on doors.

John

3/20/18       #10: how to create inverse profile of og ...
Warren Member

you can cut your mitres on the table saw then clean out between and have a mortise and tennon joint without buying a cutter set. Or run any profile you want then do the mitered profile


View higher quality, full size image (809 X 609)

3/20/18       #11: how to create inverse profile of og ...
Steve Member

Well, Warren while I don't want to hijack this thread I appreciate your showing this beaded frame's results. I struggled with doing these on the saw etc as you have described without satisfactory results so I gave up and bought the Kreg jig when it was first introduced around 2008 or 09, and I have to give you credit for the fine work particularly with multiple rails. I notice you have produced haunched tenons which adds to the production steps. Thank you for showing that.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello