Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Assembling Face Frames

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Assembling Face Frames

5/2/19       
Stewart Member

We are at a point in our business where we need a better strategy for face framing as we are doing more of it these days. I'm looking for two solutions in particular - one for beaded face frames and one for quick assembly of normal face frames. I've been looking at the Hoffman system and, while it is expensive, it looks like it could possibly be the quickest and most accurate system (in my research so far) for the beaded side of things. I know I could get set up with a face frame table for all the normal stuff but don't really want to buy both systems if I don't have to. Could you use the Hoffman system for "normal" face frames as well? Does anyone here have experience with this? I'm a little worried about getting all the rails registered to the stiles in the right locations and would love to not have to make spacer blocks for every project like what I see guys having to use on face frame tables. Please weigh in!

5/2/19       #2: Assembling Face Frames ...
Ryan

I would think that it would be very time consuming to build face frames without having a face frame table and a pocket hole machine. Unless you make tons of beaded frames I would buy a table now and make your own bead. Run the bead inside the openings as soon as you build the frame. Then in the future look into one of the other systems. In the past we did a lot of beaded inset and never had a fancy machine it was all done by nailing baed on the inside of the openings. As far as cutting spacers it helps a little but as long as you can read a tape then you are good. Once you lock the rail to the style on the table then you can knock it a little one way or the other with a hammer.

5/2/19       #3: Assembling Face Frames ...
Dustin orth

Website: http://customwoodmontrose.com

I built our frame table, no vertical arm with cylinders on it. 8/4 soft maple around 4 by 8 with dog holes everywhere for post type clamps if needed. We use vice grip clamps with wide jaw pads on the bottom rail. We have the castle pocket screw system, do the frames so you are screwing down, not sideways and I can do around 50 plus frames in a day including multi opening vanity or giant fridge boxes. Beaded frames are something we rarely do so no opinions there.

5/2/19       #4: Assembling Face Frames ...
Dennis Adrian

The Hoffman system can do all types of face frames , very quickly and accurately.
It is by far the best way to build beaded FF
and having done beaded and non beaded
I prefer it over pocket screws. Having said that the Hoffman system is more expensive than pocket screws but this tool can be used for many other applications besides face frames and can become a very valuable tool in the shop.

5/2/19       #5: Assembling Face Frames ...
Adam

From a cost perspective its hard to beat a Castle machine for square edge ff.

It all depends on the quantity of beaded cabinets you produce. We have done them many ways over the years. Tablesaw, router jig, handsaw, sliding mitersaw.

We will not do nail on beads. They are a waste of time. All the cutting, glueing, nailing, filler, extra sanding. Total waste of time. The quality is definitely lower as well. On clear finish the color grain never matches. You have visible putty holes when you open the doors.

Now there is a Kreg router jig available. I would look into that. Personally, I can cut piles of frames quickly with slider, tablesaw, and a chisel. You need a wee bit of skill.

5/3/19       #6: Assembling Face Frames ...
Stewart Member

I may still end up just doing a face frame table but I have to look at all sides first. I like the idea of the Hoffman being able to precisely register the rails to the stiles (when used with a Razor Gage) but I'm not sure yet if CV can output what I need to make that happen. Dennis, when using the Hoffman, do you have any squaring issues? In one of the product videos, it just shows a guy pounding the dovetails in the back with the frame laying loose on the table - no squaring clamps like a FF table. Also, what kind of tolerances are you able to get? I'm always looking to stay within .004" no matter what process we are doing. I'm also assuming that you would glue each joint or maybe just the dovetail piece? How does it compare time wise to assembling on a FF table? Thanks for all the help!

5/3/19       #7: Assembling Face Frames ...
Dennis Adrian

If the FF pieces are cut square and straight the dovetails will pull the assembly together square. The dovetail machine needs to be set up properly to cut tight joints but this is an industrial quality tool and can hold the setting even with constant use. I don't build many FF these days (outsource mostly) but when I do the occasional frame I just place face down on a flat glue up table and apply some glue to the ends of the rails and hammer the dovetails home to pull the joint tightly together. I don't build face frames to 3 decimal place accuracy, happy if I can keep it to a 64th of an inch.
As a side note this tool has become irreplaceable for putting miters together, all sorts of mitered joints can be done very quickly and accurately.

5/3/19       #8: Assembling Face Frames ...
Pat Gilbert

The thing I don't like about the Hoffman is that it indexes off of both ends which creates double the error in distance for aligning the bowtie cuts

TBH I think the Hoffman machine is overrated other than the most basic one

The pocket screw will create a small amount of creep but is easily fixed in the drum sander.

5/3/19       #9: Assembling Face Frames ...
Redneck

What is your time worth? What are your clients willing to pay for your time and knowledge? My Lawyer can't afford me... and I pay that over-educated dirtbag $300 an hour...

5/16/19       #10: Assembling Face Frames ...
Larry

Good one Red.
I've had a Hoffmann machine for many years. It's the table top pneumatic version.
Excellent machine, fast, accurate. You need a top quality miter saw. We've got an Omga, stay away from things like Dewalt. Buy a top of the line stop system for the saw.
I bought this system when we had a long string of jobs with short time frames. Did 2500 doors for that job. We have used the Hoffmann for many other things over the years. Keys come in many sizes and colors. I think they still sell aluminum keys. I've had brass ones made and now have the capability of making them in shop. Some pretty interesting design work can be done. Hoffmann also sells wood ones but I wouldn't use them for structural.
The plastic ones produce a very strong joint! 2 keys to the corner, always reference the same edge.

5/16/19       #11: Assembling Face Frames ...
Pat Gilbert

The decorative keys are thinner and used on top of the plastic ones

You can index the same edge but it is still indexing off of the opposite end

5/17/19       #12: Assembling Face Frames ...
Larry

The decorative keys come as long strips that you cut as needed.
Assuming your frames are uniformly made and we are talking about a mitered frame perfect alignment is done by using a spacer block to make the 2nd key slot. We've made frames with more than 4 sides, works the same way just using a different V guide. I machine those out of 1/4" aluminum & key to the table slot.
I don't do face frames but do have a Morso miter machine, that's the brand sold by Hoffmann for their beaded FF system. The Morso is an excellent machine.

5/20/19       #13: Assembling Face Frames ...
Pat Gilbert

It would appear you are talking about picture frames?

I thought the OP was talking about face frames.

2 different things or am I missing something?

5/22/19       #14: Assembling Face Frames ...
Stewart Member

Yes, this was originally to deal with face frames. I see Pat's point about having to index off of both ends. Has this been an issue for those of you with this machine or do their stops prove to be accurate without a lot of fussing?

5/22/19       #15: Assembling Face Frames ...
Larry Schweitzer

Hoffmann sells long stop bars (or buy 8020) & I'm guessing you could easily adapt electronic stop systems. I haven't made a face frame cabinet in 30+ years so maybe I no longer understand the problems. I like to cook so I avoid kitchen designs that make it difficult to keep clean.

5/23/19       #16: Assembling Face Frames ...
Pat Gilbert

I don't know about the stops that Hoffman has for the machine you are considering.

The machine I had was for doing bevel miters, the stops were terrible as in could not have been worse.

In any case when you are indexing off of the ends you double the error of the stops.

I see the problem with using the castle or similiar with the face not being flush.

OTOH are you not going to run the frames though a drum sander?

But using a castle machine would solve the indexing problem, if it is one on the machine you are considering

Not to mention that the castle type machine is half the boring time and has been the go to for face frames for decades.

5/23/19       #17: Assembling Face Frames ...
Stewart Member

I am considering their bowtie machine, however, it appears that you have to get into the stop set-ups which is what I would like to avoid for the very reasons Pat mentions. I was hoping it could be set up in conjunction with razor gauge for auto positioning but I am seeing that only their notchers can do that...bummer! Using a face frame table, I would pre-sand the individual "sticks" and then assemble hoping to barely have to touch the joints with a random orbit for final sanding. I'd rather not send them through the drum sander if possible to avoid the cross grain scratches.

5/24/19       #18: Assembling Face Frames ...
Pat Gilbert

I asked a friend who has done a lot of beaded inset kitchens he said that he uses the castle machine.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello