Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Painted Kitchen Cabinet Doors

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Painted Kitchen Cabinet Doors

6/3/19       
Howard

Previously I asked opinions on veneer species for kitchen cabinet doors. Now my client has changed the job and I need to make new slab doors that will be painted. This would be my first at painting kitchen cabinet doors. First, I assume that to get the best result I will need to spray which is fine since I have a spray booth, but do you agree with this? Second, from checking around it looks like I need to use a very specific primer and color coat product, is that true or will a good quality primer and enamel color coat be sufficient? Some of you preferred mdf to baltic birch if they were to be veneered, but for painting is one better that the other? THanks.

6/4/19       #2: Painted Kitchen Cabinet Doors ...
rich c.

Shouldn't you be asking this in the Finishing section?

6/4/19       #3: Painted Kitchen Cabinet Doors ...
Ryan

Slab doors will be a good thing to learn to spray on as they well are flat and you lay them flat to spray. I would use lacquer based paint. It will give the best finish. MDF will paint the smoothest and stay flat. If you want to see a little grain through I would use MDF core maple. Either way just make sure to sand the edges good. This is give a lot better finish than baltic birch and you don't have to edge band the edges.

6/4/19       #5: Painted Kitchen Cabinet Doors ...
Robert Member

I thought that Lacquer based coatings on Kitchen Cabinets were a no-no due to it having no protection against water nor the ability to last very long.

Is a Poly or a Conversion Varnish or 2K coating a better choice over a Lacquer based coating ?

6/4/19       #6: Painted Kitchen Cabinet Doors ...
rich c.

I agree with Robert. Lacquer based around the sink, dishwasher, stove and range hood will produce a short life finish. Especially on MDF end grain. Even Precat doesn't hold up in those locations. My personal 27 year old kitchen is a fine example of Precat failure.

6/4/19       #7: Painted Kitchen Cabinet Doors ...
Ryan

Pre cat has come along way in 27 years. This is also dependent upon the paint manufacture. I good quality product from MLC or another top brand will be perfectly fine.

6/5/19       #8: Painted Kitchen Cabinet Doors ...
Robert Member

Lacquer has come a long way in the past 27 years, no doubt about it. Other types of coatings however have far surpassed the longevity of any Lacquer coating, be it a pre cat or a post cat.

I venture to say that any Manufacturer of a Lacquer based coating would strongly suggest against using their product in a kitchen environment.

6/9/19       #9: Painted Kitchen Cabinet Doors ...
Vince Member

Website: http://MusserContracting.com

I am preparing to do a job like this. Full kitchen with flat slab doors.

Thus far, I have only done frame-and-panel cabinet doors. Flat slab doors will be new to me.

It seems a good material to use for the doors would be pro-core, which is an MDF\Ply hybrid panel.

Planning on solid-edging the panels with 1\4" maple.

Go to "substrates" on this page to see an example:

https://www.timberproducts.com/products/panels/hardwood-plywood

As for paint, I have had good results with pigmented conversion varnish for "painted" cabinetry. Pre-cat looks good, but is not nearly as hard in my opinion.

My only concern at this point is applying conversion varnish directly over MDF. I have never done that at any large scale. Does anyone have experience? Sand to 150?

6/9/19       #10: Painted Kitchen Cabinet Doors ...
Robert Member

Vince, keep your eyes open for a Primer to use under the CV. There are many types available.Its also possible to tint the Primer to get closer to the final color.
Id gently sand the MDF with a fine paper, but don't over do it.

6/9/19       #11: Painted Kitchen Cabinet Doors ...
Vince Member

Is there a reason for the primer?

I sometimes use a catalyzed vinyl sealer under CV, is this considered primer?

The CV I use (Sherwin Williams) is self priming.

One other thing to note is that, in my experience, when CV is tinted, the sheen is lessened.

6/10/19       #12: Painted Kitchen Cabinet Doors ...
Robert Member

Oh;Ok then.

5/8/20       #13: Painted Kitchen Cabinet Doors ...
Al Gerhart Member

Pre cat lacquer is fine for kitchens, been using it for twenty years. Use a color coat made from a sealer tinted to match the color swatch, clear coat of pre cat over the top. Buy a good Kremlin spray rig and a spray booth and do it right.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello