Subject: Re: Edgebander glue issues

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Edgebander glue issues

10/10/19       
Brent Member

I'm running a Biesse Lato 23S and I am getting on some of the pieces run what looks like a dry lump of glue under the banding. Wondering if anyone knows what is causing this?


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (4032 X 3024)

10/10/19       #2: Edgebander glue issues ...
Matthew

I don't have an answer, but I've been meaning to post the same question. I have a brand new scm bander doing the same.

10/11/19       #3: Edgebander glue issues ...
Oggie

Not sure, but I've read somewhere that edgebanding glue has not so long shelf life and that it deteriorates quickly once the air gets into storage container.
Maybe try with fresh glue, or try glue by different manufacturer.

10/11/19       #4: Edgebander glue issues ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

We keep ours in a container with a lid after opening

10/11/19       #5: Edgebander glue issues ...
Dan

We got this on occasion over the years.
It can be a number of issues but I believe the most common are temperature, contamination or volume.
Watch your material pass the application roller. Look for stringy glue as the panel leaves the roller. This can build up until it becomes thick enough that an unfortunate panel picks it up as it passes.
Cause may be temperature too low in the glue's range or excessive glue on the roller.

10/11/19       #6: Edgebander glue issues ...
Nathan W Member

We have the same issue sometimes on our Brandt. The cause of ours was we were applying to much glue. As the part was coming off the glue roller it was leaving "strings" behind. While there is a rod that is supposed to pull the strings off and push them back into the pot, it wast doing so. The strings would stick and build up on a different section of the machine and let go once they got to big. You might also want to check that the edge isnt dragging on anything after the glue is applied and leaving build up somewhere to fall off.

10/14/19       #7: Edgebander glue issues ...
Brent Member

I will adjust the glue roller and see what that does. I hate messing with it as it is really touchy on this bander. I am running Jawat 288.70 and I am running at 200 degrees on the roller and 190 degrees on the pot.

10/14/19       #8: Edgebander glue issues ...
Brent Member

After looking really close I found that the material was in fact dragging on the unit that holds the tape in place just before the pressure roller. When changing tape that gets adjusted and it was out of the slot.

-Thanks for all the help

10/16/19       #9: Edgebander glue issues ...
Matt

Nathan W is spot-on correct about the Brandt, we have one too. Fantastic machine, but if we have the glue temp too high or too low, it tends to develop a lot more of the "cheese pizza strings" as the glue comes off the roller onto the material face.

At the first sign of string buildup, we start dropping glue temp by about 5 degrees, or increasing glue temp, depending on the ambient temp. Winter=hotter glue, summer=colder glue.

12/5/19       #10: Edgebander glue issues ...
Derrick Keisel Member

Website: http://www.awcarter.net

What glue manufacture are you using? We use a Visual zero joints with PUR glue - HOLZ-HER and haven't had any issues yet. I hope this helps..


View higher quality, full size image (4032 X 3024)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello