Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Toekicks built separate from cabs?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Toekicks built separate from cabs?

2/12/20       
mzelsmannjr Member

The shop I work for builds all the toekicks for base cabinets separate from the cabinets themselves. Our standard base cabs are 30" tall (762 mm) with a 4.5" (114 mm) toekick. The other guys in the shop (much more time in service than I) have suggested that they would prefer to change to all in one piece, but the boss writes the checks ;-)

Input ???

2/13/20       #2: Toekicks built separate from cabs? ...
Paul Member

I had 29 years in the business, many of those as an installer. I always preferred to have separate toekicks. They are easy to make on the bench from stock 4" rips the benchmen have close by. Easier for installers to set and level toes before setting cabinets. Otherwise cabinet install will be out of level. Then the doors gaps will vary and not look good. In the end, more time is spent doing a lousy install job. And it is a good way for machinists to rid of the scrap, rip it up for toekicks.

2/13/20       #3: Toekicks built separate from cabs? ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

I have always wondered why the in house shop figures this is easier or better, Yet the installer (and the shop) benefit from the use of the ladder back toe kick.

at 4.5" tall i imagine you are doing residential, in commercial with RB cove base it is 4" and specified in all of the medical applications here in my area. the AWI specs call for the ladder back so architects spec it.

2/13/20       #4: Toekicks built separate from cabs? ...
Ryan

The main advantage in a shop is that you can get 3 base ends out of one rip of plywood. Its a lot better yield when you get 6 base ends out of a sheet rather than 4. Your shop would have to do test to see how much more time it takes to build separate toe kicks vs. the material savings. With a cnc it is cheaper to build the whole cabinet. Also if your installer works for the business vs. contract. If the installer works for the business and uses them as separate to level, then it also saves time in the field. If he is contract, then who cares as long as he doesn't charge more one way or the other.

2/13/20       #5: Toekicks built separate from cabs? ...
David R Sochar Member

Many years ago, the Indiana shop I worked for had a job for several restaurants in New Jersey. The plan called for all the cabinets to have loose toe kicks. They even stipulated how to build them and a note on the drawings said inspectors were very attentive to this detail.

Only later did I find out why. It seems that the rats in that part of the world knew about those hollow toe kicks and would promptly move in - often before the restaurant opened. So - you would have the restaurant open and happy diners everywhere, including the hairy ones under the drink station..... So the State required all toe kicks be loose and filled with concrete before the cabinets could go on. That should keep those rats at bay.

When we build a run of cabinets, we make as many into one as we can rather than 3-4-5 separate boxes. Then these are placed on a nicely leveled and secured toe kick frame. We don't use concrete, as Indiana rats are content with what they have. Or maybe they are in there, in every toe space, enjoying the access.

2/13/20       #6: Toekicks built separate from cabs? ...
MarkB Member

We do the same incorporating multiple cabs into a single box whenever possible but I see why the production shops dont. Single hinge type, single hinge plate, single drawer front, and so on. I feel its a better job with loose kicks and large boxes and its much faster for the installers, but it is more expensive on the build side.

I cant say I agree that CNC and integrated kicks are better price wise. Its really hard to beat getting 6 sides out of an 8' sheet but for sure the extra parts and the finished ends eat that up at some point.

I rarely get commercial work that wants detached kicks. I dont get to make the decision. Its perhaps 1 in 30.

2/13/20       #7: Toekicks built separate from cabs? ...
Ex-Pat Member

I've actually been playing with the numbers on this myself. Currently we do integral kicks but at my previous place of employment we did ladder style bases. So far, it looks like the material consumption would go down about 10%. Run time on the CNC on routing operations goes down about 6%. Time on the panel saw to cut the additional base parts goes up about the same, so the total machine time is pretty much a wash. The plywood needed to make the bases mostly comes from drop, so the increase in material there is negligible. Making the extra parts does add to labor, but our guys in casework can build faster than parts can be machined, so they have time to do it. We use our own installers, so the labor savings in the field would at least offset the additional shop labor - my instincts tell me it would actually outpace it. In either case, installation is usually our constraint, so adding time somewhere else to take it out of there would be a win. Even worse, we quite often have to hire contract installers to keep up. It gets the job done, but shrinks the margins. As far as finished ends go, when we currently use a ladder style base we hold the base a half inch in from the finished end of the cabinet. Now for the intangibles:
1) The greater part density on the routed sheets actually make each sheet take a little longer to machine - this would give the operator time to start banding the parts while the CNC runs.
2) The CNC is another of our constraints, taking run time off of it to add it to another machine is a win
3) The CNC is vital to our operations. If it goes down, we are down. Taking run time off of it and adding it to a different machine reduces stress on that piece of equipment. If the panel saw goes down, we can cut rectangles on the slider or the CNC. If the CNC goes down, we can't do line bore and dowelling on the panel saw or the slider.
4) Ladder bases are easy to assemble. If another department is short on work, they can be shifted there.

In case you can't tell, I'm a fan of the ladder base. My biggest hurdle is to get past ten years or more of "But this is the way we've always done it."

2/13/20       #8: Toekicks built separate from cabs? ...
Matt Calnen

Ring, ring, ring.....hello, this is the 1980s and we want or way of supporting cabinets back.
Has anyone ever heard of adjustable leg levelers?

2/13/20       #9: Toekicks built separate from cabs? ...
Alan F.

Commercial work, 2-1/2" , 4" and 6" ladder kicks.
Why
1) We can install kicks, they can do flooring and we can comback and set cabinets

2) easier to level long runs, easier to control required ADA heights.

3) required in lots of buildings with connection details to the floor; public works and OSHPOD the connections need to be inspected before the cabinets are set.

4) no water weeping up the bottom of ends

5) 6 ends out of a sheet instead of 4.

6) easier to remodel when the owner changes their mind, you can pull a cabinet out and replace it without having to redo the floor. We just removed and replaced about 20 cabinets in a 4 story budilding before they moved in, they wanted a different layout once they saw it. The hardest part was moving the trash holes in the stone tops.

7) we make toe kicks out of plywood, in 95" lengths and then fillers of odd dimensions.

8) We make kicks 1/4" less and sleepers 1" less than face, if its laminate or wood face we do separate applied face out of 1/4" or 3/4" in the field and scribe to fit, easy to fit before cabinets are set.

9) We tried levelers in the 80's we couldn't get them approved on lots of commercial and we don't want to change the method every job.

A-

2/15/20       #11: Toekicks built separate from cabs? ...
mzelsmannjr Member

Thanks for the input. By the detailed and thought out answers, I can tell I'm hearing from pros. I installed flooring for years, and I can say with regret that no one ever installed toekicks and let me put in the kitchen floors without the damn cabinets in the way.

Yes we are residential, you figured that out by the sizes. Our sheets are 49" x 97" 3/4" melamine, edge banded usually in 1mm maple or alder tape in my little Grizzly.

My previous job was supervisor of a major manufacturing facility. 35 on my crew, 3 beam saws, 5 homag ambition banders, 3 CNC machines, 3 Gannomats. Now I work in a small custom shop doing 3-5 kitchens a month. We have a table saw, a sliding saw, a boring machine, and a Grizzly 820 bander. Major adjustments to say the least. I've also seen major differences in the way designers design and installers install.

2/15/20       #12: Toekicks built separate from cabs? ...
Pat Gilbert

On a related subject.

Should the toe kicks/cabinets go in before or after the flooring?

2/15/20       #13: Toekicks built separate from cabs? ...
jonathan mahnken

Website: http://www.mahnkencabinets.com

I see more and more often the floors going in first.not quite as easy as far as scribing toe skins but you do get a little cleaner, sometimes flatter surface to start with

2/15/20       #14: Toekicks built separate from cabs? ...
Harold

Website: http://Morantzcabinets.com

Euro legs for the past 25years. Fastest and easiest to build and install. One customer had a major flood in house and we only changed the toekicks. Electrical work on island can be run easier as well.

2/16/20       #15: Toekicks built separate from cabs? ...
Edi Silva  Member

Website: silvawoodworking.com

For the guys doing Ladder base, how you handle the cabinetry around the shop/delivery when you have faced frame cabinets that the stile runs down to the floor and/or the frame end panel runs down to the floor? do you build a temporary cabinet base so this parts don't get damage around the shop or in transit to the job? or set the cabinet upside down? We used to do separate base with one base for each cabinet for this reason, so cabinets can seat upright, we end up going back to one piece construction, too time consuming. just wonder how you guys doing in a situation like this, thanks

2/22/20       #16: Toekicks built separate from cabs? ...
Geoffrey Wirth  Member

Website: Possessionwood.com

I use a detached base on every cabinet. They are nested from the same material as the boxes. It’s nice to have a base on the cabinets in shop and during shipping. I can take them off to gang together, or fit to site, but rarely do. I used leg levelers for a number of years, but carpenters on site didn’t understand how to use them. If we have a large face frame cabinet built from several boxes it will get a single ladder style base.

2/24/20       #17: Toekicks built separate from cabs? ...
jonathan mahnken

Website: http://www.mahnkencabinets.com

On FF cabinets we staple skids to the top and flip them upside down

5/8/20       #18: Toekicks built separate from cabs? ...
Al Gerhart Member

Man, using toe kick bases is stone age kind of work.

Start using leg levelers. Cheaper, better, pop off the toe kicks to spray, run wires, or clean out the rats. Had a customer break a 3/8" water line in their house seven years after I installed the cabinets. Cost them $550.00 for two doors and toe kicks, the cabinets were sitting 4" off the floor and came out fine.

Even paying retail the feet are cheaper than the scrap and labor making ladder type toe kicks.

Get the True 32 cabinet system book and follow it. No toe kick notches so your end panels are neither left nor right. True 32 has the feet too, around $1.50 per leg for leg and socket.

If you can import the legs and sockets can be bought overseas for as little as 8 cents. I air freighted a few thousand into the Philippines to my shop there and brought them in on the next container. Cost to the Philippines including freight was 24 cents per leg, maybe a nickle each to get them to the U.S..

Islands need a bit more support so be sure the island end panels hit the floor or once installed cut some 4" pvc pipe and run a bolt, red head, and a long nut/coupler down into the floor so the island is solid. But if you have three end panels sitting on the floor and trapped by the flooring the island isn't moving.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!