Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: dovetail machine

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

dovetail machine

8/7/20       
daniel wipf

Hey guys i have a question for anybody who does dovetailed drawer boxes.
Id like your guys opinion on a dovetail machine. When doing volume drawer boxes would you recommend getting CNC dovetailer or would just a automatic one be good enough? i know cantek has a nice automatic for around 10k.
kind of a new field for me here...

8/7/20       #2: dovetail machine ...
Leo G Member

I have a manual machine and once it's setup it makes making the parts very easy. 95% of my boxes are from 15mm Baltic Birch plywood.

With the automatic machine you are stuck with specific heights of drawers. In my case on my manual machine it's always a factor of x.365" I can make them a bit smaller, probably down to x.125"

With a CNC dovetailer you can make your drawers most heights because the computer can adjust the spacing.

8/8/20       #3: dovetail machine ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

Speed wise, they're about the same from what I've seen in videos, and what I know from running a Cantek automatic dovetailer. You can only load and unload parts so fast

I don't know if witg any of the cnc options if you have full control of the code or not. You could possibly get way better results being you could score in a climb cut, then finish it off in a conventional cut.

I want to build my own, but have zero time to do so.

The Cantek is painful to get dialed in.

8/8/20       #4: dovetail machine ...
Leo G Member

I have the Grizzly and it too is a pain to get dialed in. But you only have to do the major dial in once and then a minor dial in every time you change the bit which isn't too often.

I climb cut all my drawers, especially the Baltic Birch.

8/9/20       #5: dovetail machine ...
Quicktrim

I nest mine in the router with 1/2" Baltic birch prefinished.

Cut and assembled is about 10 min a box includes CNC time.

If you have a CNC I would recommend this route .

8/9/20       #6: dovetail machine ...
Leo G Member

Do you do anything with the raw wood ends? Finish them or just leave them raw?

8/9/20       #7: dovetail machine ...
daniel wipf

That is one question I was wondering about... how it works with different drawer heights? that part doesn't look like its adjustable on the cantek.

so when your saying nest them with the router do you mean do the dovetails on the router or are you just talking about a dado or blind dado?

and as far as finishing the raw ends... the costumer we are making drawers for wants prefinished baltic birch with prefinished half mill banding. any raw ends stay that way.

8/15/20       #8: dovetail machine ...
Jim Herron

I have a Dodds SE20 that I like a lot.
Perhaps I'm not understanding the draw of the single spindle machines, cnc or otherwise
A friend has a Omec 750 and while it does a good job I don't think it compares to the production capacity of the Dodds

8/17/20       #9: dovetail machine ...
daniel

Hi Jim
i am curious about your dodds machine? what year is it.
I know of a SE25 cnc machine for sale but its a 02 model and the company says the controller is discontinued.
I am wondering if that should be a issue or if its best to just leave it be and look for a newer one?

8/17/20       #10: dovetail machine ...
Warren E Member

Curious about the Dodds as well. Ive seen some of their multipin machines at auctions.

Is anyone running a Brookman 25 pinÉ

Really like to talk to someone running one. I did have a few emails with the last tech in england and since lost touch.

Then the Leigh dovetail jig while way way slow still makes a much nicer looking drawer than the Multipin things. I guess the CNC can do the sameÉ think so speaking as a non CNC guy.

Likely hijacking this thread a bit, apologies on that.

8/19/20       #11: dovetail machine ...
Jim Herron

Funny both of you should ask...
I bought the Dodds from a large cabinet shop that I used to purchase doors from.
They run about 250 employees, and the guys had destroyed one foot actuator and thrown the other away.
The owner said they didn't know how or have time to fix it and they bought a new MereenJohnson
I tinkered with it about half a day, and wound up replacing both pedals and cleaned it and reset all the fences and fixtures on it.
The pedals were about 20.00 ea off Amazon thanks to our reopening trade with Vietnam.
I think I overpaid a little for it at 5k, but it was close (no freight, and next closest one at auction was 900 miles and unable to inspect) and other than the obvious abuse to it, fairly low use.
It does a great job.
I was buying about 4500.00 worth of boxes a month, so payback was pretty quick, and I can produce them on demand and schedule. It is not a cnc machine, but automatic- foot pedal actuated or timed sequence.
I have a Brookman 15 spindle manual machine that I ran prior to buying them and it does a good job, just more effort.
I've done several jobs at 200+ boxes but you feel it after doing that many.
A job around 50 or so boxes is about the sweet spot on the Brookman.
It's complete, in great shape with fairly new Dodds cutters in it and about to go up for sale, as I need the space.
PM me if you'd like information on it.

8/20/20       #12: dovetail machine ...
Scott

I have a Dodd’s single bit manual machine, it is definitely a lot slower as someone has to run it, it does do a really nice job though. For a long time I just purchased drawer boxes as we didn’t do a lot of dovetail, most drawers were for commercial projects and were either a butt joint with dowels or a dato joint.

Quicktrim,
I would be interested in hearing more about the nested cnc for drawers. How is that set up? I assume the tooling would be minimal and not to expensive, The part I am curious about is the accuracy for having a part in position so everything lines up and fits tight. Are you using a jig to hold the parts in position.

8/20/20       #13: dovetail machine ...
daniel

jim
so im wondering on that dodds machine if its not a cnc how do you adjust the spacing of the dovetail if you have different drawer heights? so that on the end you dont have like half a notch or something like that?

i was also curious about about the nesting on a cnc machine as well. if its efficient enough for doing volume drawers?

8/20/20       #14: dovetail machine ...
Leo G Member

I assume you work within the confines of the machine. My manual Grizzly's magic number is always x.365". So 4.365", 10.365" etc. You can get it down to about .125" if you need to squeeze a drawer into a smaller height area, but that's about it before you start to see a free tail.

8/21/20       #15: dovetail machine ...
Jim Herron

I make my drawer heights in one inch increments with the bottom recessed up 1/2"
Typically 5, 6, 8, 9, 11 inch drawer box heights
My standard top drawer is 7 7/16" face with a 6" high drawer box using a Blum 563H slide.
It's a production thing..
I wouldn't even consider adjusting the spacing in a kitchen or bath..I might if I were building high end furniture, but I'd probably expect to hand cut those anyway

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!