Subject: Re: 84” round solid oak table top

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

84” round solid oak table top

8/9/20       
Harold

Website: http://morantzcabinets.com

I have a 2” thick solid oak table top to build that will be 86” round. We are a panel production shop with Bander, sliders and boring machines , but no solid wood machinery, any suggestions on how we could build this or best place in south Florida to order it? Thanks, harold.

8/9/20       #2: 84” round solid oak table top ...
TonyF

Harold:

I'm sure someone will build it for you if you give them the money, but consider that a solid oak top of that size will tip the scales at about 290 pounds. It might be difficult to maneuver, even with a muscular shop crew, to say nothing of the wood expansion issues in a solid wood table of that size that you may likely encounter, which will have to be accommodated for in the tabletop to base interface design. Although you may need nothing more than gravity to hold it in place. :^)

What is the tabletop for? Could it possibly be constructed using veneer with a built up perimeter?

TonyF

8/9/20       #3: 84” round solid oak table top ...
Harold

Website: http://morantzcabinets.com

It’s a dining room table. The base will have a cross shape that would is quite large as well which we can make. Has to be slid wood although I may be able to make it 1.5.

8/10/20       #4: 84” round solid oak table top ...
rich c.

Hope they have an oversized entrance door to get it in the house! But the title says 84" and the explanation says 86" so hard to say.

8/10/20       #5: 84” round solid oak table top ...
Harold

Website: http://morantzcabinets.com

Sorry, it to s 84” my typo, but in either case , this is a hugh estate on inter coastal with 9’ high entrance doors and base will be seperate section, so no problem with access.

8/10/20       #6: 84” round solid oak table top ...
Oggie Member

I would most likely build two rectangular tops 85" x 85", 1" thick and then glue them together on top of each other, with oak boards on the top one going in perpendicular direction to the bottom one.
(Before gluing try to get individual boards planed to the same thickness and squared as good as possible and then use biscuit joinery to align them when gluing.)

Since I don't have some giant press I would clamp them with a bunch of clamps around the perimeter and a bunch of 1-3/4 screws screwed through the pre-drilled holes in bottom board.
Then I would roughly cut round shape from that, and use a manual router suspended on a piece of wood that orbits around the center of the board (like a propeller) to fine trim the edge.

But before all that I would have to build nice flat and level working table of that size that can support this building process and provide necessary flatness.

Anyway, a lot of improvising type of work for a shop not equipped for such projects.

I started my journey with custom build solid wood / steel tables, but once I learned that in two days of building lowest grade cabinets with almost zero mental effort and stress I can make the same profit as in few weeks of very stressful work of custom made projects, something clicked in my head and you know the rest of the story...

8/10/20       #7: 84” round solid oak table top ...
Bill

Oggie, if you glue the two layers with the grain perpendicular to each other won't they fight the glue line and eventually delaminate? I have never tried that?

8/10/20       #8: 84” round solid oak table top ...
MarkB Member

Barring sub'ing this out to someone (which is likely your best bet) you could likely pull the whole thing off in-house on the CNC in two pieces with a very small amount of handwork at the end. Of course if you dont have in-house finishing thats another step.

We do far more surfacing and solid wood work on the CNC than I'd ever have thought. Doesnt sound like an overly complicated top to make regardless and a perfect match for the CNC.

8/10/20       #9: 84” round solid oak table top ...
David R Sochar Member

I think it wise to request a retraction from Oggie. The method he describes is doomed.

If the table is to be anything other than 1-1/2" to 2" thick, it would have to have some sort of balanced construction.

Solid construction is fine. Sort thru your lumber to get color and grain alike. Face and edge the boards so the planks lie together and will clamp up without using the clamps to pull the boards where you need them.

There seems to be some sort of mystery or fear regarding solid wood with some people on the forum. There are no mysteries or magic. There is more science on solid wood than many other materials.

8/10/20       #10: 84” round solid oak table top ...
harold morantz morantz custom cabinetry inc

Website: http://morantzcabinets.com

Your right about the two layers. sounds like a disaster. I dont have any solid wood machinery to joint or square. all my bladers are 80Tooth for panel material. dont even have clamps this big. as i said in my shop description, we build euro cabinets only. will probably farm it out. any one know someone in south florida who could do this for me? thanks.

8/10/20       #11: 84” round solid oak table top ...
pat gilbert

Not in Fla but it might be worth an email to Paul Downs

8/10/20       #12: 84” round solid oak table top ...
Oggie Member

Yeap, the gluing alone could be problematic, that's why i said:

"and a bunch of 1-3/4" screws screwed through the pre-drilled holes in bottom board"

Perpendicular direction suggestion was to minimize warping/bending/twisting of the finished tabletop.

I know it's not the proper way to do it, but the advice was for the tools and equipment available in his shop.

I once built tabletop 12' long and 4' wide out of 12' long 4''x4" douglas fir lumber straight from the lumber yard, i.e. not very straight ones.
Didn't had planer, didn't had joiner, so I drilled holes every 10" through the middle of the boards and put I think 13 threaded roads through 15 boards side by side and "screwed" them together for gluing.
It took tremendous amount of force to bring everything together; at one point I thought the nut/road threads will worn themselves out from how hard I was screwing them, even if it was 5/8" threaded rod diameter, so I had to lubricate them to be able to continue, and the big flat 2.5" over sized washers were sinking into the wood and getting into the shape of a bowl.

At the end I glued them together but the result was far from flat. Luckily the boards were thick enough for the tabletop to still appears thick when it was sanded down to make it look flat.

There were some massive boards underneath running across tabletop width that surely helped in keeping it flat over time, but I'm not sure if it would remain flat on it's own.

Anyway, would not recommend anyone now to do it this way on a regular basis.
For me it was the time of experiments and time of learning, surely not the time of doing business :)

When I inquired some local woodworking shops for manufacturing solid oak tabletops 1.5" thick the price was over $100 per square foot (maybe around $130 if I recall correctly) , don't remember now if the material was even included in that price.
And that's how I got into cabinets :)

8/10/20       #13: 84” round solid oak table top ...
rich c.

Why are you doubling down on that construction Oggie? And even describing an even more disturbing method of construction. All your methods just ignore every accepted construction method. Steel, and screws will not restrain wood movement. It's either going to bow, or split.

Harold, if you don't have a jointer or thickness planer, why even ask about building it yourself? To go 2" thick, you'll have to buy 10/4 stock and that's nearly impossible in white oak. But then you don't mention what species of oak either. Hopefully you haven't already bid it, since you have no idea what it will cost to buy from someone else or having to buy several thousand dollars worth of machinery and clamps.

8/11/20       #14: 84” round solid oak table top ...
Oggie Member

Rich

I think my posts have been misunderstood.

I've described something I would have done and had done in the circumstances where I didn't have proper tools/machinery to do it right, but for whatever reason (that is beyond this scope) I still had to do it somehow.
Especially the second example was an anecdote of poor man ridiculous attempt to build a tabletop out of non-straight, non-squared, longitudinally twisted, 4" x 4" solid boards.

Hopefully, Harold is not in a position to have to do it despite not being equipped for it, so he can choose the other (proper) ways of doing it or not to do it at all.

Sorry for the confusion I brought into the thread.

8/11/20       #15: 84” round solid oak table top ...
TonyF

Harold:

See what these people can do for you.

Good luck.
TonyF

https://www.ecustomfinishes.com/shop/round-dining-tables/large-84-round-table/

8/11/20       #16: 84” round solid oak table top ...
harold morantz morantz custom cabinetry inc

Website: http://morantzcabinets.com

Thanks Tony. Just the ticket! appreciate it.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!