Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Omal Hinge Borer Troubleshooting

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Omal Hinge Borer Troubleshooting

2/5/21       
Jeff S Member

I recently inherited an almost functional Omal Hinge Boring/Insertion Machine. I believe it is the "Easy Bore" model.
I've been using it at our cabinet shop for the past 10 years. It's been a solid workhorse.
The issue it is having is with the boring head not returning back up the cylinder. When the machine is turned on with air supply, you have to manually slide the head back up the piston (which is hard and heavy). When you depress the bore button, everything functions correctly except it stays at the bottom of it's path and keeps rotating the bits. Any help would be greatly appreciated. Thanks,
Jeff


View higher quality, full size image (475 X 404)

2/5/21       #2: Omal Hinge Borer Troubleshooting ...
Oggie Member

I believe that green button controls pneumatic valve(s) for the main piston, as well as two small pneumatic clamps.

It could be an electrical button in which case valves controlled by it are most probably some solenoid controlled valves (i.e. they open or close with electrical signal).

It could also be just a push button of the pneumatic valve that is controlled mechanically by that button, and the rest of it is inside the control box.
I believe this is more likely than previous case.

Starting and stopping of the drilling motor is probably controlled by some electro-mechanical limit switches that get mechanically triggered by the head traveling up and down somewhere along the way.

Your pneumatic cylinder is double acting so the problem is with the air supply at the bottom side of it (that's why it's not going up). I would suggest opening that control box and see what's inside, or try to peak from underneath it.
Just follow the air hose from the bottom of the cylinder backwards to the control box and see what gives it its air.
The cheapest try would be to replace that thing first and see if it helps (I assume you don't hear any air leaks at this time and some hose is not pinched somewhere so that air can not flow through).

If possible try to read the name of the part, find out what it is and than find locally available equivalent replacement. Save yourself money and time by not trying to find the original part.
Local rep from www.smcusa.com was extremely helpful in my case.

2/5/21       #3: Omal Hinge Borer Troubleshooting ...
Oggie Member

"I believe that green button controls pneumatic valve(s) for the main piston, as well as two small pneumatic clamps."

Not the two small pneumatic clamps. That's the black switch bellow :) Sorry.

2/6/21       #5: Omal Hinge Borer Troubleshooting ...
Jeff S Member

Thanks for your help.
I noticed one other important thing that the machine is doing. When air is hooked up to it, there is a constant flow through the "clean out" hose. The hose I'm referring to is right over the boring head and it's function is to blow away the shavings created by boring.
I know this machine (when functioning) only would put out a stream of air from that "clean out" hose momentarily during the boring process.

I am with you on thinking this is an air flow/valve problem, I will follow the air lines as you suggested.

For further explanation, here is how the machine is supposed to work. There is a switch you turn 90 degrees to engage pneumatic hold clamps (that works).
Then you depress and hold down the green bore button until the boring is complete. Upon release, the boring head travels back up and I believe that's when it shot the stream of "clean up air".

I'll post if I find anything out.

2/6/21       #6: Omal Hinge Borer Troubleshooting ...
Oggie Member

If there's a constant flow of air through the clean-out hose than most probably that is where the machine is loosing pressure and there simply may not be enough of it to pump the piston up.
In that case check that thing first before anything else.
If you can, close that hose somehow and see if the rest of the machine works as it should without it.

2/6/21       #7: Omal Hinge Borer Troubleshooting ...
Tom Gardiner

Sticky valves is my guess. Have you ever added air tool lubricant to the air supply? How clean is the regulator filter? Try plenty of drops of oil in the supply line and numerous cycles to free up the mechanism. Next step is disassembling the works for a deep cleaning and checking the seals.

2/6/21       #8: Omal Hinge Borer Troubleshooting ...
Jeff S Member

Thanks Oggie and Tom for your time and responses. I will try everything you all suggested and let you know how it turns out.

To answer you Tom, likely was not maintained with oil.

2/8/21       #9: Omal Hinge Borer Troubleshooting ...
Jeff S Member

Tried multiple cycles of oil and it didn't change it's behavior.
I opened up the control panel and had a look. The green bore button goes to a mechanical valve which has multiple air lines running to it. See photos for part.

Is it likely enough that this has failed and that it warrants buying a new one and swapping it out? Depending on where I purchase, it's around a $40-$50 part. Would I be better off doing some further diagnostic before I begin throwing money at it?

I have never worked on pneumatic tools like this and don't have an understanding of how they operate. Once again - appreciate the help!


View higher quality, full size image (2016 X 1512)

2/8/21       #10: Omal Hinge Borer Troubleshooting ...
Oggie Member

It depends how much you value your time.
I would not blink over $50 if it could save me few hours or bring my machine "online" today instead of, like, next week.
The loss in time (and time = money) caused by machine not working or me fiddling with it instead of building and installing cabinets is ridiculously disproportional to that part's cost.
However, if you have some spare time or want to learn more about your machinery (which is always a good thing), then why not.

Replacing that part is straight-forward operation. Those are quick connectors (just push-in to connect the hose, and depress the ring and pull-out to disconnect it), and everything should go very easy. Just make sure you buy new ports (those things that accept that black air-hose); they need to have the right thread size that will fit into your new part and have to accept exactly that diameter of your black air-hose).

I'm not expert on pneumatics, but it looks like every major industrial country has it own standards regarding the threads used in pneumatic/hydraulic industry.
I think if you send that photo to smcusa.com and measure the diameters of those black air-hoses someone will give you exact part numbers that will fit with each other.

Or, if there's some pneumatic supply shop in your area it may be even faster.

2/8/21       #11: Omal Hinge Borer Troubleshooting ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Hey Jeff,

There are a few possibilities;

The seals in the cylinder are the most likely cause.

The green push button valve may not be functioning properly. It is simply a pneumatic valve to route the air pressure to the top or bottom cylinder chambers.

The guide bearings on the posts may be gummed up with dust, debris, rust, etc., but that is highly unlikely

Dennis

2/12/21       #12: Omal Hinge Borer Troubleshooting ...
Jeff S Member

I swapped out the pneumatic valve behind the green push button and am still having the same problem.
Are the seals in the cylinder something I can purchase and replace? There are no markings on the outside of the cylinder.
The only other component I see in the chain is another small valve (directional valve I think). Attached photo. I'm leaning towards the cylinder seals.
Appreciate any other thoughts or info on sourcing seals.
Thanks


View higher quality, full size image (2016 X 1512)

2/12/21       #13: Omal Hinge Borer Troubleshooting ...
Oggie Member

I'm suspicious about the seals being the problem, because there would probably be some problems with going down operation and drilling too since it's the same piston that goes up and down.

However, it should not be a problem to open the cylinder.
First detach the piston from the drilling head then just unscrew the round tube from the square aluminum base. Make sure to support the drilling head with something when doing that, because it will fell down otherwise. Also, be very careful with unscrewing and screwing back the cylinder since those will be some fine threads in aluminum and it is very easy to ruin those since aluminum is soft and if you start screwing the cylinder while it's not exactly perpendicular to the base you may ruin those treads before you notice that something is wrong. In other words, don't use too much force when screwing it back, it should go easily if you align the threads correctly. Start tightening only when you're sure everything is aligned.

If I was in your place I would check if that valve at the bottom gets correct control signals.
Most likely that is some directional valve controlled with "pilot signal". In this case the controlling signal is pressured air that comes through (most probably) that black hose connected at the top side of the valve.
So, it's either that valve is no good or it does not get good pilot signal, then trace back that signal and see what supplies it.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!