Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Raised Panels

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Raised Panels

3/9/21       
Troy R Beverly

Hello all!
Probably a common question but I have been making paint grade raised panels for years and still wondering what the absolute best material for the routed areas taking paint with excellent results? I have lately used Medex and double primed all exposed routed areas. Any ideas of an upgrade to this material or application?

3/9/21       #2: Raised Panels ...
Mark B Member

When we run MDF (doors or raised panels or anything that needs exposed/machined edges painted) we've run double refined and then when we prime we dust a couple of very light coats first before laying on a good prime coat. My experience has been when the first coats go on heavy its a lot more work. I use to try to saturate the prime coats thinking it would lock up the machined areas but never worked.

3/9/21       #3: Raised Panels ...
Bill

I have not tried this but heard it from one of the biggest door makers. PVA diluted in water painted on cut areas.

Makes sense.

3/9/21       #4: Raised Panels ...
Adam

Plum creek double refined
Sand the cut faces with 320. Seal the cut face only with BIN shellac primer. Just brush it on. The mdf soaks it up like water. Once it dry sand it with 320 again. Prime the whole door with your regular primer.

3/9/21       #5: Raised Panels ...
Troy R Beverly

The PVA diluted idea seems like it might work great. I know you said you heard it from second source but I am assuming I still need to sand thoroughly first then brush the diluted PVA then resand. Is the Plum Creek super refined a lot better than Medex?
I prefer a waterproof core in my kitchen applications but if the routing is better I can live with it.

3/9/21       #6: Raised Panels ...
rich c.

If you do a search on here, you'll get 44 hits on sealing MDF edges. https://www.woodweb.com/knowledge_base/Priming_MDF_Edges_for_Finishing.html

3/9/21       #7: Raised Panels ...
rich c.

Sorry, should have made it a link

Knowledge Base - Priming MDF Edges for Finishing

3/9/21       #8: Raised Panels ...
Jim Herron

I used double refined PlumCreek and spray the machined areas with clear precat lacquer reduced 50% then sand the raised areas on a Larick profile sander prior to assembly, then go with regular finish schedule.

3/10/21       #9: Raised Panels ...
Leo G Member

Plum Creek/Weyerhaeuser double refined MDF is what I use. I spray MLC Clawlock on the bevel a little heavier than I should and let it dry so it powders when you sand it back hard.

Then do your normal finishing schedule.

3/10/21       #11: Raised Panels ...
Troy R Beverly

Thanks form the input. It seems like Plum Creek double refined is popular choice. It's just that after so many times in homes seeing raised panels either below sink, at dishwasher panels or even down at any area where the owners or cleaning staff accidentally leave excess water on the top horizontal raised lip there can be swelling after time. I know the finishing process should take care of this but it's not a perfect world. Double refined does not have any water resistant resins in the core and Medex is supposedly a double refined product. Also in regards to the PVA duluted mixture any idea the ratio?

3/10/21       #12: Raised Panels ...
Leo G Member

I find that MEDEX acts like double refined until you mill it. The inside acts like normal MDF that sucks up the finish. I was pleased the first time I used it that the surface only needed one coat of primer like the Plum Creek. But once milled you have to work it like normal MDF.

I would suggest using the MEDEX only where you think it's needed. Under the sink and at a prep station. The rest you can use the Plum Creek to make your life easier.

Normal MDF got two coats of MLC Clawlock, both sanded back hard before they are put into the door frames. Then finish as normal. I suspect the same for the MEDEX.

3/10/21       #13: Raised Panels ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

Anybody ever try using wood for raised panels?

3/10/21       #14: Raised Panels ...
Bill

MDP is a superior product for paint in my opinion.

3/10/21       #15: Raised Panels ...
Leo G Member

You use Medium Density Particle Board for raised panels? I can't see that being easier than MDF style products.

Please elaborate.

3/10/21       #16: Raised Panels ...
Mark B Member

Karls response was my default but if your needing dead smooth, no glue lines telegraphing in the panel, no woodgrain telegraphing, it sucks but it is what it is. If I had to run some water resistant material or process for a wet cab I'd just move that to every RP door period.

When I apprenticed in the trade in my teends (80's) it was pounded in that particle board, press board, whatever you want to call it, was dog $hit, and now 30+ years later, I guess with more advanced glue and manufacturing,.... fashion always repeats and we are again regurgitating particle board/mdf/pressboard on the masses.

Sucks to pay the bills with the acceptable standard but it is what it is.

3/10/21       #17: Raised Panels ...
Warren Member

Didnt read the thread and will later. Gerry Metz always pushed Glue size and so did the old guys I knew. Metz used glue and old guys sprayed on a mix with sanding sealer or other stuff. I think Metz sponged it on and maybe 1:7 was his ratio. I had times where i had to do a fair bit of MDF stuff and it did make a difference.

One lac supplier told me way back to greatly reduce the first coat, sand lots lots to most of it off, then second coat is really your first normal primer coat. I was doing ply stuff at the time and using Ml Campbell then before Becker and it worked well on the ply doing that. Filled the pores.

3/10/21       #18: Raised Panels ...
Mark B Member

Anything other than spraying what your normally spraying sounds like a gloppy mess. A brush has zero place in my bankroll for MDF work.

3/10/21       #19: Raised Panels ...
Warren Member

I do whatever is faster and or works better based on the work.

3/10/21       #20: Raised Panels ...
Adam Spees

I can't imagine sanding glue saturated mdf goes well. You are painting. Use paint to seal it. BIN, catalyzed primer's and the like seal the grain. Then you are sanding primer.

Back in the day when mdf first appeared, people would fill the coarse grain with wall compound & bondo. They would also glue size it and put piles of paint on it to fill the grain.

Double refined changed everything. Use paint.

3/10/21       #21: Raised Panels ...
Troy R Beverly

So in conclusion if I use double refined I still need to follow the same prep as MDF or Medex correct? Or is double refined a miracle and if I use it I can just do a good sanding? If I still need to do same prep I will opt for water resistant Medex to avoid any possible swelling later if a panel is dinged or chipped. Ratio of PVA to water is 40% water to 60% glue? That's what I heard earlier but just now 1:7 ? I like the thought of sponging it on for time but a brush might be less messy.

3/10/21       #22: Raised Panels ...
Leo G Member

I don't sand after milling. It goes straight for priming of the bevel. I also do the back so the color gets on the tongue of the panel so if there is any movement you don't get a bare line. Plus I have my thickness of my tongue setup to take two coats of primers added thickness of about 4 thou.

I found that sanding the raw Plum Creek to not help out at all for the 1st prime coat. Another reason to prime the panel out of the frame is ease of sanding the bevel

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors

    Become a Sponsor today!