Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: prime walnut yield

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

prime walnut yield

6/14/22       
JEREMY SETZKORN

I needed 26 pieces of 100% defect, knot and sap free walnut stiles 2 1/4"/ x 75" long. I It took 170 board feet of PRIME grade material to get this.
$11.70/ board foot. Walnut is tricky but iv never had prime grade that bad.

6/15/22       #2: prime walnut yield ...
Mark B Member

That doesnt surprise me really based on my experience. Especially if your supplier is steamed material. I'd guess our average at 1 in 10 or perhaps even more for dead clear, all heart, straight grained, boards.

6/15/22       #3: prime walnut yield ...
RichC

I've never seen "prime" used as a walnut grade. Beef yes, walnut no.

6/15/22       #4: prime walnut yield ...
RichC

How long have you been a professional? Walnut has always had its own grading rules and has always taken a higher percentage of offcuts. For the last 50 years anyway. Big walnut trees are getting incredibly rare now and it will get worse. The really good logs go to the veneer mill.

6/15/22       #5: prime walnut yield ...
Mark B Member

Rich,
We've been seeing a lot of varying grade names especially in Walnut but also in a number of other species. In Mid-Atlantic Ive seen and heard prime several times though our suppliers dont grade as prime. What Ive been seeing with Walnut is it being graded off the standard Walnut grading rule so the mill can allow more defect/sap and especially as I said when the material is steamed.

Sourcing lumber out of Ohio is most commonly where Ive been hearing the prime the most. No idea where the OP is pulling from or the thickness but at 11.70/bf I'd say its not in this area if its 4/4 because that is sky high for here.

6/15/22       #6: prime walnut yield ...
Mark B Member

For reference:
https://northwesthardwoods.com/products/appalachian/walnut/prime/

https://northwesthardwoods.com/products/appalachian/walnut/prime/

6/15/22       #7: prime walnut yield ...
Mark B Member

Here is even "SUPER Prime"
https://www.baillie.com/walnut-super-prime

https://www.baillie.com/walnut-super-prime

6/15/22       #8: prime walnut yield ...
Duncan Member

" him " donteth knoweth everything.

6/15/22       #9: prime walnut yield ...
Mark B Member

He's just old and grumpy. We all get that way. Im pretty much a reclusive grump wanting to kick everyone out of the shop (that doesnt have a pocket full of cash). Is what it is.

6/15/22       #10: prime walnut yield ...
RichC

Hard to find people with a sense of humor here. When I tell a joke from now on, I'll label it so you don't have to come on and attack me. It's not like you have a lot to weed through on this site to see new content! LOL

6/15/22       #11: prime walnut yield ...
RichC

Doing more research. I find no prime listed in the NHLA grading book for walnut. So far it only appears with private companies. Does that make it an acceptable grade if only used to sell something at a higher price since there is not official rules?
This is not a joke, asking questions only.

6/15/22       #12: prime walnut yield ...
Dick

6/15/22       #13: prime walnut yield ...
JEREMY SETZKORN

Sorry guys, its listed as PREMIUM walnut on my invoices. I just always ask for prime. Yea walnut has always been very difficult but this batch not as good as usual. Very picky customer means i get a stack of free walnut lumber. Not going to try to return it because i dont want my supplier unhappy with me. Most people dont care if the back of their doors has sapwood. Thing is they are staining all these doors near black but still request perfect material. Go figure. Couple stiles were perfect except for bullets. My other supplier was $2 more per BF. I am finding big differences in pricing on hardwoods between suppliers where they always used to be really close.

6/16/22       #14: prime walnut yield ...
RichC

Always a challenge to understand some customer requests. But in this case don't worry about the price. Just mark up the material at your regular rate and let the customer pay for their desires.

6/16/22       #15: prime walnut yield ...
Mark B Member

I'd say you didnt do too awful bad considering my experience. Just rounding up and using 4/4 as an example, 3" x 84" x 26pcs hits at 45.5BF and pulling dead clear from 170BF lands you at about 40% which is much better than our yield for dead clear/straight material. The bummer in my world is we only have the option to buy pack sizes so depending on what our mill has on-hand we may have to buy several hundred board feet just to get a pack in-house and even then its a roll of the dice and you may have to grade through that entire pack to get pristine boards. The next pack may be gold bars but its just a roll of the dice.

6/16/22       #16: prime walnut yield ...
Bruce H

I just finished a walnut cabinet project. I ask my supplier for the most expensive material they had. All in all it was good. The boards with knots I filled with epoxy and made the panels out of them. Customer was very happy. I did pay about $12.00 per board foot for the material.

6/17/22       #17: prime walnut yield ...
RichC

For panels, you don't need high grades. The short cuttings can come from #1 common if the customer doesn't mind some sapwood on the back side.

6/17/22       #18: prime walnut yield ...
RichC

This might help.

https://www.mcilvain.com/news/walnut-grades-explained/

6/17/22       #19: prime walnut yield ...
Mark B Member

Those grading standards only apply to mills that adhere to the NHLA grading, hence prime, premium, super prime, etc.. Even my main mill doesnt grade any FAS because the yeild would be pretty much zip. My guess is they will revisit the Walnut grading again in the not too distant future due to ever shrinking supply.

6/17/22       #20: prime walnut yield ...
RichC

Funny to me that wholesale distributors can make up any marketing name they want. Makes buying tough since you have no idea about the cuttings you can get. Basically the whole point of this discussion I guess. With no rules and made up names, the future for hardwood buying is going to be really difficult. I wonder if any exporters are making up grade names for selling in Europe. Doubt it! Lucky us.

6/18/22       #21: prime walnut yield ...
Mark B Member

Its not like its a free for all... walnut is the prime suspect for all the reqsons youve directly mentioned. I think its pretty easy to see that suppliers are trying to show clearly what one can expect with pack images etc as to avoid bs.

People who deal in walnut regularly this isnt much of a shock.

6/18/22       #22: prime walnut yield ...
RichC

You win MarkB.

6/20/22       #23: prime walnut yield ...
Dave Edgerton  Member

One of the biggest problems is the trendy slab tables where we see tons of walnut getting cut and stabbed and so less available for dimensional lumber. An out fit in Ontario canada was shocked I could buy select and better shorts for 9$ bfm as his slabs were running 12$ a bf. I would buy everything he can cut if his price was reasonably in line with the market. 1 com for me is 7.85$ right now net.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!