Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Hot air edgebanding - can you get edgeband

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Hot air edgebanding - can you get edgeband

10/21/22       
bob

I am looking to buy a new edgebander for a small to mid sized shop that does commercial work. It seems to me the hot air edgeband concept is a great idea....no glue, no joints. The only drawback seems you cannot get edgeband in small quantities (say single 600lf rolls pvc) unless you want black or white. Am I missing something? Does anyone out there use hot air and what are your thoughts on it?

10/22/22       #3: Hot air edgebanding - can you get e ...
RichC

What is your idea of a mid sized shop? Lots of money to be saved with a commercial edge bander.

10/22/22       #4: Hot air edgebanding - can you get e ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

What is a mid sized shop is an interesting question.

To me, 0-10 on the floor, small

10-25, medium

25-50 big

50+, BIG/fricking huge.

I know less than nothing about hot air banders.....

10/23/22       #5: Hot air edgebanding - can you get e ...
Thomas Gardiner

You will not only be limited on what you can get in banding without ordering a custom run of thousands of feet, but also you will be limited in the bander's abilities. I would guess that you won't be able to find a hot air bander that can process 3mm banding so you will have to outsource for any jobs that will require it. Other options like scraping, buffing, fine trimming and corner rounding eliminate tedious hand work after banding. This can be a massive improvement in productivity for a commercial shop. I have a very basic bander without the bells and whistles. Even with it running well, I spend as much time banding as I do tuning up the edges. Banding is not a big part of my shop process so I; just deal with it.
Glue pots or Holzher cartridges are nothing to fear. Shops run thousands of feet a week, week in week out on a regular maintenance schedule. A bander with all the options needed for your type of work will be the biggest productivity improvement to your shop.

10/23/22       #6: Hot air edgebanding - can you get e ...
Mark B Member

You can get most common bandings in hot air but keep in mind your product will suffer because the hot air will expand PVC banding and then down the road (weeks/months) the banding will shrink back leaving a less than desirable glue line and gaps at the ends.

Hot air, in my opinion, is fine for low temp wood tape. It still a ton of work but for a super small shop (shelves or a few doors here an there) I guess.

If you expected, or expecting, to delivery any type of commercial cabinetry hot air isnt going to fly. Not only is it too slow, its going to land you with a mile of call backs and you could likely wind up remaking entire jobs.

10/23/22       #7: Hot air edgebanding - can you get e ...
Matt Calnen

I run a hot air bander and mostly run prefinished or unfinished maple on plywood. It works great for that. I have also ran pvc wood grain on prefinished plywood with no issues. I use a company called Edgeco. They are awesome to deal with and I believe the minimum order is 250’. Goggle them and you will find they have a great website and customer service.
Not sure what you are doing, but as a small shop owner that does his own banding, I have never had an issue as everyone says you will with a hot air bander. Maybe because I give a $hit about the final product? I don’t hire dopes to work for me? Not sure but how I use it works for me.

Run some cabinets for your own house and see how they stand up.

10/24/22       #8: Hot air edgebanding - can you get e ...
bob

Sorry for not being clear. I am looking at a commercial automatic edgebander with premill, cornerround,scraping, buffing,etc.....e.g. brandt, scm, $70-100K range.

what I am wondering about is all the new banders either have standard or as an option the ability to use hot air edgebanding - e.g. no glue at the machine.

https://www.rehau.com/us-en/zero-joint

The bander sales people note this as a wonderful thing - no glue, seamless edge, etc. It does seem like a great idea if you can get the edgebanding - from what I can tell it is only available if you buy large quantities.

So, does anyone out there have a commercial edgebander with hot air capability and are they able to get edgebanding in small lots?

10/24/22       #9: Hot air edgebanding - can you get e ...
Joseph Stahl

Long story short...It depends. Locally ,next to impossible unless it a large order.
This is what I use.
https://www.rehau-marketplace.com/store/en/Rehau/Furniture/Edging/ABS/Zero-Joint/c
/Zero-Joint

The local guys will only get it from them anyways. We have airforce on a Biesse Akron and I think its a waste of 40k. Doesn't work as well as they say. Not even close. Spend the money on a separate glue pot and a freezer and use PUR . Or get their dedicated PUR system if they have one.

10/26/22       #10: Hot air edgebanding - can you get e ...
Rob Young  Member

Website: http://www.nutekmachinery.com

Joseph Stahl- this is what I have heard over and over from my customers regarding hot air.

Bob- I'm happy to introduce myself and share my knowledge on this topic as well. I have worked as a maintenance technician since 1982 both employed as a maintenance technician or maintenance manager and as an independent technician working on every brand and type of machine out there. Salesmen typically think anything their machine has on it is a great idea, simply because they don't "know" what they "don't know". The factories manufacturing the machinery we are using are typically in Europe or Asia. Hot air may have been a hot thing for a short period of time in Europe but the demand has waned. There was a lot of money spent on R&D and the inability to offer anything else has kept it alive in the minds of salesmen here in the U.S. When it was first developed, hot air was marketed as a way for companies to achieve a better edge without investing a lot of money into a laser but there are several insurmountable issues with hot air that have turned users away from it.
1. Coextruded edgebanding is expensive and you typically have to buy large quantities.
2. If you aren’t using coextruded edgebanding you are using pre-glued edgebanding and the finish looks worse than a glue pot machine.
3. Hot air lacks versatility. Veneers, HPL, and hardwood edges are not coextruded, and you simply won’t pre-glue these if you are looking for an invisible glue joint. Most end up using the gluepot far more than they use the hot air.
4. Hot air is loud and an annoyance to employees
5. Hot air machines use large amounts of compressed air and shops often find they need to upgrade their compressor to a larger size to accommodate the increased cfm requirements on their systems.
Laser is a much better alternative, but it is expensive and once again limited to coextruded edgebanding.

As a technician working on every manufacturer out there, I decided to seek out high quality production efficient machinery that produces high quality products with little to no setup time. Our lines are Ott for edgebanders, Stema for drilling, doweling, and hardware insertion, Modesta for dust collectors, and KRC CNC for machining centers.
Ott is our edgebander line producing invisible glue joint panels and depending on the machine setup the most an operator may need to do is change the edgebanding roll and keep the gluepot filled. The salesmen you are talking to have probably tried to steer you away from using PUR glue and I don’t blame them. Their machines are poorly designed for PUR and very problematic when trying to run PUR on them. Ott on the other hand is perfectly designed for PUR with a top driven glue roller that eliminates the possibility of leaking seals in the lower end of the pot that will ruin bearings and drive mechanism, something that will eventually happen with bottom driven glue rollers. Glue dosage is servo controlled making the glue joint invisible to the eye. The PUR glue joint exceeds the strength of coextruded systems like hot air and laser. The already used PUR glue can be stored in the service station dry box for up to 7 days eliminating daily purging associated with other machines. The glue pot and hopper can be removed in about 30 seconds with zero disassembly of the machine.
Since 2011 more than 95% of the machines Ott sells are used strictly for PUR glue with some shops running less than 20,000 meters a year. Salesman will tell you; PUR can be run on their machines but do their best to talk you out of it simply because their systems really are poorly designed for PUR. With an Ott I would do everything I could to talk you out of running EVA and once you start running PUR on an OTT you’ll never go back to EVA.
Feel free to contact me if you would like to know more or arrange a demo at our showroom.

Rob

https://nutekmachinery.com/ott-combimelt.html

12/17/22       #11: Hot air edgebanding - can you get e ...
Jesse Beaverson Member

Website: https://instagram.com/jessebeaverson

Rob, could you explain what coextruded edge banding is? Do I understand correctly that coextruded edge banding is another option besides preglued edge banding that can be used on an inexpensive hot air edge bander? Thank you!

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors

    Become a Sponsor today!