Subject: Re: Cabinet doors expanding from humidity.

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Cabinet doors expanding from humidity.

5/4/24       
Perry Vavra Member

Never experienced this before. Did a job at a lake house where customer wanted 1/8" reveals between doors and drawer faces. Doors are shaker style frame and panel made from beech with 1/2" mdf panels. I returned to install hardware couple weeks later after painting was complete to find that the doors and drawer fronts were rubbing. Expanded from excess humidity.
I told the customer that we should wait till AC is turned on and see what happens. If they go back, no problem, but if not then what? Has anyone had to deal with a situation like this? If I have to go back, remove and resize,
then reinstall should it be on my dime? Appreciate any feed back.

5/4/24       #2: Cabinet doors expanding from humidi ...
Dave Edgerton  Member

Beech is notorious for rapid expansion and contraction. Did you testhumidity in your shop and of the wood before manufacturing?
Sorry you are faced with this.

5/4/24       #3: Cabinet doors expanding from humidi ...
RichC

Really, you've never experience solid wood movement? How many years have you been woodworking? It's one of the most basic rules of woodworking.

5/5/24       #4: Cabinet doors expanding from humidi ...
Perry Vavra Member

Thanks for the response. I have been building custom cabinets for over 40 years and have never seen this much expansion on cab doors. Not sure that knowing humidity in my shop would have made a difference. I made all the doors for the kitchen cabinets in my shop using cherry with no movement. I outsourced all bathroom and utility doors to help me move the job along a little quicker. The door shop I used makes paint grade doors with beech. Painter came in same day that I was finishing install to start prepping so doors were painted within a couple days. We've been getting a lot of rain here in Texas, but this is not unusual
for this time of year. I'm sure being on a lake had something to do with it. Hoping once the house is climate controlled they will shrink back.

5/5/24       #5: Cabinet doors expanding from humidi ...
chris

Our shop is in the High desert of California. We can get as much as a 40* swing in temp. in a day. Never had much trouble with stain grade stuff just made sure to get the stain deep in between the panel and the stile & Rails. Now everyone wants paint, white to be specific. We have our door manufacture build with a paint grade maple for the stiles & rails then use a 3/8" MDF for the panel (It's paint right!). I also let the unfinished pieces sit for a couple days.
So Far so Good.
Sorry, doesn't help u much after the fact

5/6/24       #6: Cabinet doors expanding from humidi ...
Tom Gardiner

Beech is a problem wood. You probably are experiencing worst case here. Wood dried in the winter dropping to something like 6%. Fit at that or close MC, spring humidity hits and add the water based paint on site.
It won't be as extreme in the next seasonal cycle and less thereafter. But it will never not be there.
I would ask the client to hold off for a couple of weeks to see where the doors are at then make the decision on what if anything needs to be done.

5/7/24       #7: Cabinet doors expanding from humidi ...
JimHerron

I'm here in NE Texas as well and recent convert to beech as well, after using poplar for many years.
The architect's "designer" specifies "Beech" and specifically prohibits poplar, for reasons unknown.
Between the rain, humidity, tape/bed/slick finish walls, being lakefront, and subs leaving the house doors and windows open with the wind blowing thru the house 24/7 and now a switch to water based primer and topcoats...I have a house full of cabinet doors that are 1/8 to 3/16 oversize with most of the rails swelled past the stile ends.
I've insisted on a being operational the last several jobs, which has helped. So much so that the builder now feels its not necessary again.
Prior to my recommendation for ac, the builder lost wood floors, overlapped ceiling crown and stuck
passage doors.
I'll have to resize and edge sand every door and front in the house, and of course the painter is raising he'll about the repaint.
I'm doing time and material on resizing, but still a schedule killer.

5/13/24       #8: Cabinet doors expanding from humidi ...
Bruce H

I am in Oregon and have had issues with Beech. It moves when you least expect it. Drawer fronts that were flat and stored on paint racks with equal air to both sides, warped. I made new ones. Checked the material with a meter, 6%-7% which I thought was good. This was new material, what I have had for several years didn't move. Was thinking about buying some ahead.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!