Panel Genie

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Design flaw ooops...

5/19/15       
Steve Member

I had quite a surprise when installed these cabinets the other day! Any creative or hardware solutions that might help? I could just hinge them on the other side but it would make the knob placement a little odd ball. Over 3" would have to come off that door to make it work with a blum 86deg. angle restrictor. I'm still cussin....


View higher quality, full size image (1600 X 1200)


View higher quality, full size image (1200 X 1600)


View higher quality, full size image (1600 X 1200)

5/19/15       #2: Design flaw ooops... ...
Dave Edgerton  Member

put the hinges on the taller side of the door. Thats a whoops! Made a top in solid surface last week that i could not get into a room. Had to cut it and re-seam it in place. Happens to the best of us.

5/19/15       #3: Design flaw ooops... ...
Mark Vierno

Maybe attach the doors to a shop made, pull-out spice unit or similar?

Mark

5/20/15       #4: Design flaw ooops... ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

I'm probably (definitely) venturing outside my area of expertise but the topic caught my interest.

Would it be reasonable to do something like this? It doesn't seem like you would loose much usable access to the cabinet.

I also like the pull-out idea.

Ok, back to my own work area....


View higher quality, full size image (1133 X 934)

5/20/15       #5: Design flaw ooops... ...
Rick

Or, you could hinge the top "fixed panel" also but on the opposite side and place a fixed shelf to divide the two sections.

5/20/15       #6: Design flaw ooops... ...
Rich Kuban Member

A pullout would have access only on one side. Is the radius shallow enough the doors above the micro open sufficiently? Would have been well thought out if the sides and center were hinged on the other side, then mount knobs on the center of the rails.

Wondering if the geometry works for a pull down door as compared to a lift up door.

Dennis, your idea is interesting except your proportions are off. If the cabinet were longer, your idea would have more value.

IMHO, I would prefer hinging opposite.

5/20/15       #7: Design flaw ooops... ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Rich,

This is what I was thinking. (Here I go again, outside my box).


View higher quality, full size image (1200 X 1600)

5/20/15       #8: Design flaw ooops... ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Rich...now that I see it here, I know what you mean about the proportion.

BTW, I was at your shop last week with Paul from Salice....small world.

5/20/15       #9: Design flaw ooops... ...
Mark Vierno

If you hinge it on the opposite side, you still only have access from one direction, strait in.

Also, when you take into consideration the brick wall and the door that opens to 110° +/-, you will be reaching into a deep, narrow space to access anything in the cabinets (it looks like it is 24”+/- deep).

And finally, what are you going to do with the 35mm & 8mm hinge holes that are already bored in what would be the wrong side? Anything other than a re-make of the door runs the risk of looking bad.

If necessary, a complex pull-out with the doors attached, could be designed that still allows the doors to be hinged to gain better access, although they would still have to be limited to prevent any accidental contact with the brick. The OP has used inset euro hinges, so they could be changed to full overlay hinges to gain 17-19mm of space for some sort of modification to overcome this challenge. I already have a design pictured in my mind that would work, but would be difficult and time consuming to put into words and in the long run, probably not be cost effective.

At the end of the day, I would go for the simple solution of a standard pull-out.

Mark

5/20/15       #10: Design flaw ooops... ...
Tom Gardiner

Do you have stove to M/W clearance room to drop the whole gang of cabinets and add a scribe to the top arch enough to allow the doors to swing?

5/20/15       #11: Design flaw ooops... ...
Mike Fuson

My thought was along the lines of what Tom just suggested, drop it down and re-trim the top.

5/20/15       #12: Design flaw ooops... ...
Rich  Member

Website: http://www.hausmann.com

Can you have the door pivot up. You would loose some space in top of cabinet but it should work, you would just need a stay to hold open.


View higher quality, full size image (1242 X 856)

5/20/15       #13: Design flaw ooops... ...
Steve Member

Thanks for all the input and creative solutions!
I'm going to meet with the customer tmrw and show her what its like if i hinge it on the other side. I did a mock up and its not a problem accesing the side cabinets at all from the range area. The only issue is the knob placement.....

5/20/15       #14: Design flaw ooops... ...
John Langley

Used Touch catches or finger pulls with the knob on the hinge side

5/21/15       #15: Design flaw ooops... ...
Rich Kuban Member

Nice suggestion John!

Yes it is Dennis. Hope you had a good visit.

5/21/15       #16: Design flaw ooops... ...
Mike

Mark,

A few things...

1. Couldn't he use a 170 deg opening hinge mounted on the tall side to gain more accessability?
2. If he's not familar with doing touch up, you can hire a refinisher who does onsite work, bondo the holes, use blendals, aresol a base color, then toners, seal with a sanding sealer, come back with graining pencils.

I spent many years being a custom cabinetmaker and now i work for a refinisher doing in the shop and onsite touch up and repair. I wouldn't trade the experience I've gained for anything.

5/21/15       #17: Design flaw ooops... ...
Mark Vierno

Mike,

I guess a 170° hinge might work, but it looks to me that the doors would hit the microwave. Also, have you seen a 170° inset hinges? They are massive articulated contraptions that have too much slop in my experience, but hey if they work and the client is happy, I see no reason not to use them.

There is no doubt acceptable touch-up could be done to the resulting unused hinge holes, but I would venture that it is beyond the talent of most cabinetmakers, and to involve another trade would only raise the price of what could be a simple modification.

When I am faced with similar situations I always look for the simple solution that will cover all of my bases.

Mark

PS: I am not a fan of finger contact on cabinet doors through finger pulls or touch (and then grab the door) latches. I have seen too many instances where the finish is ruined over a short amount of time because of this. Sorry John, I’m going to have to disagree with you on this one :-).

5/21/15       #18: Design flaw ooops... ...
Larry

What I'd do: Remake the doors and an upper fixed panel. 165 degree hinges are a bust, sag in a short time. Touch latches tend to go out of wack also. No use compounding the problem.

5/21/15       #19: Design flaw ooops... ...
Mike

Mark,

Being a cabinetmaker for the past 21 years, i would totally agree with you. Until i had this opportunity to work for a refinishing friend that I use to work for when I was 18, i too struggled with color work.

After speaking to other trades people who do a form of remodeling that deals with woodworking, along with homeowners and other cabinetmakers, people who can successfully do touch up and repair is "a dying art" and there aren't many people left. Here in Chicagoland, there are only a handful of refinishing shops left.

I'm thinking about advertising my touch up and repair services on Woodweb, to try and build a different type of business, so I won't need to lug 100lbs sheets of wood on the tablesaw when i get into my older years.

5/27/15       #20: Design flaw ooops... ...
Glenn Pope

repairing the holes to hinge on the other side should just be a matter of plugging, filling, running the doors through a widebelt, and repainting. I think the split door idea is the nicest solution, even if the top part doesn't open. A small gap between them may not be very noticeable, or objectionable.

6/18/15       #21: Design flaw ooops... ...
Mark Vierno

What ever happened with this? Pictures of the repair/rebuild/modification?

Mark


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello