9/16/15       
Bernie

I need to bore a number of 3/4" melamine doors 14"W x 88"T, just not sure on the number of hinges. I'll be using Salice concealed hinges, and the literature calls for 5" for doors over 84", but in looking at these doors I'm thinking 4 would be sufficient, and I'd rather do 4 so the middle one doesn't interfere with the middle shelf in the cabinet. There's also a weight table in the literature, going by that it looks like fewer than 5 works. Which table should I go by?

Thanks

9/17/15       #2: How Many Hinges Per Door? ...
Rich Kuban Member

Website: http://closetexperts.com

In my experience, you will be okay with 4. The chart i used was for up to 24" wide doors. I converted the increment breaks to square footage. I calculated the different door sizes to make that decision. Wider doors undergo more leverage forces, necessitating more hinges. This served me well for many years, on 3/4 particleboard or mdf. Looking forward to what Dennis may offer,

9/17/15       #3: How Many Hinges Per Door? ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Bernie,

Your door size and weight puts it between the range for 4 and 5 hinges. The size puts it close to 5 hinges but still within the range for 4. Four hinges are acceptable.

The number of hinges to use is actually based on a curve. As the weight increases and the door height increases the number of hinges required is determined by a point on the curve until the next level is reached.

Using a weight of 2.5lbs per square foot for particle board/melamine, your door would weigh in at 22.5 lbs. As the height increases to 88” it would put you in the high end of the 4 hinge range. If the size remained the same but the weight was, say 35 lbs then 1 additional hinge would be recommended. See the chart below.

Keep in mind, if the door has a long bar pull, it could add enough weight to change the number of hinges required.

Hi Rich, how's everything in Chicagoland?


View higher quality, full size image (2020 X 928)

9/17/15       #4: How Many Hinges Per Door? ...
al

Dennis,
How many for a maple raise panel door that is 19-1/4"W x 36" L? I was hoping to use two.
Thanks,
Al

9/17/15       #5: How Many Hinges Per Door? ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Al,

Although hardwood will vary in weight from species to species, I normally use 2.7lbs/sft as an average. Based on this and your door size, 2 hinges would be sufficient.

(19 X 36)/144 = 4.75 Sqft.
4.75 X 2.7lbs/sft = 12.8lbs (Door weight)

Below is a door weight calculator based on the material and a simplified chart from the Salice catalog used to determine the number of hinges to use.


View higher quality, full size image (4200 X 1724)

9/17/15       #6: How Many Hinges Per Door? ...
al

Thanks always Dennis.

9/17/15       #7: How Many Hinges Per Door? ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Bernie,

I used the wrong square foot weight in calculating your door weight. Particle board/melamine would actually weigh 3.0 pounds per square foot. This would make your door 25 pounds. The answer, 4 hinges would not change.

That's what I get for trying to think at 5:00am.... before coffee!!!

9/17/15       #8: How Many Hinges Per Door? ...
Bernie

Thanks very much.

9/17/15       #9: How Many Hinges Per Door? ...
Rich Kuban  Member

Website: closetexperts.com

Dennis, awesome that you posted these charts. Makes sense the real issue is weight since that is what affects leverage even more than door width. Important to note hinge location affects it too. The closer to the top and bottom of the door, the better. Learned this the hard way.

We are having some August weather here in the middle of September. Busy organizing the world here!

9/18/15       #10: How Many Hinges Per Door? ...
Chris

Well, I just got an email from sugatsune. They apparently just came out with a cup hinge that is meant for heavy doors. They claim 2 of theirs is equal to 5 of others. Doesn't look soft close though. BOOOOOOO sugatsune!

Sugatsune J-95 Hinge

9/18/15       #11: How Many Hinges Per Door? ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Sugatsune is a great company for specialty items. I recommend them all the time. They are the only supplier I know that offers stainless steel concealed hinges. I get requests for stainless steel hinges frequently, especially for cabinetry in MRI rooms in hospitals, for outdoor kitchens and for marine use. I always refer the customer to Sugatsune for these.

According to the information in the Sugatsune catalog, 2 hinges are suitable for a maximum door weight of 55lbs. This indeed is a higher claim than most. Salice is 20lbs for 2 hinges. Blum specifies 15lbs for 2 hinges. (See chart below).

The Sugatsune specs however call for the use of six #10 screws to fix the hinge and plate (compared to four #6 screws for Salice and Blum). The additional screws and their over-size would increase the load rating possibility. The cup depth is 15mm and it is a 94 degree opening hinge.

I am sure this is a fine product as is everything I have seen from Sugatsune.


View higher quality, full size image (1139 X 518)

11/15/15       #12: How Many Hinges Per Door? ...
mike Member

In the #3 answer by Denis Bean he posted a chart to calculate the number of hinges for the weight of the door. The chart has metric 120 = 22.5 lbs. I can't for the life of me find anything metric that will give me the same results, not even close. I'm doing something wrong for sure, can you set me straight so i can use the chart accurately?
Thanks

11/16/15       #13: How Many Hinges Per Door? ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Mike,

My error, sorry. Actually the engineering chart was originally in "newtons". My error was in the conversion. Actually 22.5lbs = 100 newtons (not 120). (4.45n = 1 lb.). I used an on-line auto conversion that gave the answer "120n" = 22.5lb. I should have double checked it. - the measure twice, cut once rule.

The number of hinges would remain the same however.

11/16/15       #14: How Many Hinges Per Door? ...
mike Member

Thank you Dennis, i never heard of newton before this. I'm glad i can use the chart correctly now. If you don't mind i would like your input on the 165 degree hinge. I want to use it for an inset application with a thicker than normal door about 1 inch to 1-1/8 thickness. How small can i get the reveal between the door and cabinet side?
I found the formula H= (-2+K+A) but i also found another formula for A. where as A=(-2+k-H) but they do not agree with each other! I do appreciate you help, Thanks Mike.

11/17/15       #15: How Many Hinges Per Door? ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Mike,

I agree that the 2 formulas seem to fight each other. Over the years, some Salice publications have presented the solution by solving for a negative number (the gap between the door and the side can be viewed as a “negative overlay”). I have always found this confusing.

Note: These formulas hold true for only Salice hinges. Other brands have a constant (-2) that is different and therefore will result in a different solution.

I prefer Method 2 where you solve for the mounting plate height. It makes much more sense than having a negative number as the answer.
The results, however will be the same. if you use method 1.

A = Gap
K = Edge bore distance (TAB)
H = Mounting plate height

Method I: A = (-2 + K) - H

-2mm = (-2 + 6mm) - 6mm
-2mm = (4) – 6mm
-2mm = -2mm (gap or negative overlay)

Results: Gap = 2mm; Edge bore distance = 6mm; Mounting plate height = 6mm

Method II: H = (-2 + K) + A

Here, you arbitrarily set the gap that you would like to see then solve for the mounting plate height that will give that desired gap between the door edge and the cabinet side. The edge bore distance is determined by trial & error until the formula balances.

H = (-2 + 6mm) + 2mm
H = (4) + 2mm
H = 6mm (mounting plate height)

Results: Gap = 2mm; Edge bore distance = 6mm; Mounting plate height = 6mm

Now, as far as the amount of gap you will need to turn a door that is 1” (25.4mm) or 1-1/8” (28mm) thick using the 165 degree hinge, here is a chart showing the minimum gap required to turn a door of various thicknesses without interference.

Take note that as the edge bore distance (K) increases, the amount of gap required decreases. You can play around with the numbers to get exactly the outcome you would like.

This explanation is in context to your application being frameless or face frame with the side built flush to the edge of the frame.


View higher quality, full size image (1324 X 449)

6/29/17       #16: How Many Hinges Per Door? ...
arsim

HI....I have a shutter sized 20" wide and 13" height. What would be the recommended number of Auto hinges and the distance in between...Why I am asking is because in every chart it says that the distance between them should be greater than the width of the shutter. Kindly help!

6/29/17       #18: How Many Hinges Per Door? ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Arism,

The rule of spacing of the hinges is very important. I would not recommend hinging a door on the side that is only 13" tall and 20" wide using European concealed hinges.

Can you hinge it at the top and make it a lift-up door (shutter)?


View higher quality, full size image (626 X 800)

11/5/17       #19: How Many Hinges Per Door? ...
Bernie

Dennis,

On the example of the original door that was 88" tall, wouldn't that convert to 2235mm (88x25.4) which would put it into the range of 5 hinges, instead of 4?

11/5/17       #20: How Many Hinges Per Door? ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Bernie,

You are correct it is close to 5 hinges and I would normally recommend this.

Since you mentioned that the center hinge would interfere with a shelf and that the range is still within 4 (high end) I believe you are safe with 4.

Also, it is quite a narrow door which gives you some breathing room too.

11/5/17       #21: How Many Hinges Per Door? ...
Bernie

Thanks Dennis, I just wanted to make sure I was doing the conversion right. The charts are great, thanks so much for posting them.

12/24/21       #22: How Many Hinges Per Door? ...
Irene White Member

Website: https://www.yigii.com/

The door height and weight will make great effect on teh number of hinges.
Doors less than 40inches high and below 5kg need 2 hinges.
Doors that are 40-60inches high and weigh 6-9kg need 3 hinges.
Doors that are 60-80inches tall and weigh 13-15kg need 4 hinges.
Doors that are 80-85inches tall and weigh 18-22kg need 5 hinges to secure.
If you would like to replace the kitchen cabinets hinges by yourself, here are more informantion for you: https://www.yigii.com/replacing-hinges-on-kitchen-cabinets/

Best Methods for Replacing Hinges on Kitchen Cabinets

11/8/23       #23: How Many Hinges Per Door? ...
Lisa

Hi,

Stumbled upon this treasure box of wisdom in my search for answers.

We have a custom wardrobe cabinet and will be ordering doors ~ 104” tall. They will be 15” wide and made out of mdf.

Been doing some math, and weight wise 4 hinges should be enough (if I’m not completely mistaken), but height wise I keep seeing I need 5. I’ll be using the Blum 110 degree soft close hinges.

Both the weight and the force placed on a single hinge should be smaller than a shorter but wider door that requires 4 hinges… or am I completely lost?
Is the reasoning to use 5 hinges solely for the stability of the door?

The distance between the hinges won’t be even as there are drawers in the bottom section, it’s an IKEA wardrobe and that’s how they place their hinges. It’s really just an added foot on top of the cabinet. There will be a larger distance between the two bottom hinges and the remaining 3 (or 4) hinges will be evenly placed.

Super grateful if anyone could help me out. Also, pardon any spelling/grammar errors as I’m not a native English speaker.

11/8/23       #24: How Many Hinges Per Door? ...
chris

Personally, when in doubt I do 5 so there's no call back.
I often put 2 hinges closer to the top and move the "center" hinge up as well.
Often hinges are placed where you can due to pullouts or corner cab organizers etc.
No more thinking, just decide and keep building :-)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello
    Today's Sponsors
    • CabinetCRUNCHER
      3D Cabinet Design and Construction Software Powered by SketchUp and Excel, Precise Cut List Calculators with Highly Adjustable Construction Options for Cabinetmakers and Woodworkers of All Levels
    • Holz-Her US Inc.
      Custom Edgebanders, Vertical Panel Saws, CNC Beam Saws, Wide Belt Sanders, CNC Point to Point Boring Machines, CNC Routers
    • Excel Dowel and Wood Products Inc.
      Plain and Pre-glued Dowel Pins, and Wood Parts - Servicing Small Hobby Shops to Large OEM's
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • GreCon
      Spark Detection and Extinguishment Systems and Quality Assurance Measuring Equipment
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Original Saw Company
      Industrial Radial Arm Saws
    • JKL Machinery
      US Exclusive Importer Casadei, Busellato, Vitap, Bonacin - Machinery Dealer representing New & Used Woodworking Machinery
    • Impact Search and Placement
      Professional Employment Recruiting Specialists
    • Safety Speed Manufacturing
      Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands

    Become a Sponsor today!