Panel Genie

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Blum hinge mixup

11/5/15       
JoeLena Member

I have Blum 120 degree half cranked clip on hinges and 0mm plates right now that do not fit. I have 1/2 overlay doors on 3/4" material and frameless boxes. It appears the bore was drilled incorrectly- too far from the edge. I am looking for a solution that is best and not sure how to proceed.

The issue is, since the bore is too far in on the door they will not open far enough and the edge of the door impacts the hinge. Opens to about 80 degrees.

Right now the bore is 10mm and it looks like it should be 5, but the blum chart is confusing to me.

Would changing to straight hinges work with this bore? Looking at the blum chart I can not tell. Hoping someone who has installed a lot of hinges can help out with this. Or if there is another hinge that will work with the 10mm bore? Not looking to re-bore the holes as that would entail re-veneering all of them.

11/5/15       #2: Blum hinge mixup ...
Jim Herron

Can you glue in 8mm dowels and rebore?
The hinge plate should cover the 8mm bores and quite possibly the 35mm as well.
Might try laying one out to see.
Otherwise a 155 degree with thicker baseplate perhaps?
Maybe Dennis Bean will chime in here. He's on the Salice team but may have a solution.

11/5/15       #3: Blum hinge mixup ...
JoeLena Member

Thanks for that help. I would have no trouble going to a different hinge if the bore would match. That would be the easiest. The ones I have now are screw in, so the holes are not 8mm, so that is a little better. Really trying to not re-bore.

I have some older Salice hinges that appear to be a better fit as far as the bore of 10mm, but they are press in and I need screw in hinges. They do have a straight arm though.

11/5/15       #4: Blum hinge mixup ...
ed

6mm is about max from edge. You could get some salice thick door hinges that require a 40 mm hole and overlay the existing hole.
Ed

11/5/15       #5: Blum hinge mixup ...
Marty

Hey Joe,
You should be able to configure Blums 155 deg hinge with a 3mm plate.

Cheers Marty

11/6/15       #6: Blum hinge mixup ...
JoeLena Member

Thanks guys, I will look at both those options.

11/6/15       #7: Blum hinge mixup ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Joel,

The Salice B Series hinge can be used with an edge bore distance up to 18mm. In your case, if your edge bore is indeed 10mm then you can use this hinge with a 2mm mounting plate and it will be a drop-in for you. The screw holes will align and you will get an overlay of 9mm. There is plenty of side adjustment if you need it a little.

Hinge: CBP2A99 (110 degree, screw-on)

Mounting plate: BAR3R29 (2mm plate for wood screws)

Here is a drawing showing the application. If you need a source, drop me an email and I can let you know who the distributors are in your area.

Best of luck


View higher quality, full size image (1169 X 1630)

11/6/15       #8: Blum hinge mixup ...
duster

Try a Blum half cranked thick door hinge. I've used them in applications like yours and was able to get it to work.

11/6/15       #9: Blum hinge mixup ...
JeffD

I can't help you with your problem, but have run into my own trying to figure out Blum hinges in the past. Now whenever I do a new setup I use a piece of scrap material to do a test fit instead of drilling a door. Takes a couple extra minutes but I've found its worth it.

good luck,
JeffD

2/17/16       #10: Blum hinge mixup ...
Mike Member

I had the same problem with a loose fence. Some of our doors were drilled up to 27mm. I used a "0" protrusion hinge, and had to use different plates to get it to work. One door had 3mm, another had 6mm. I hope this helps. MIKE


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello