Mike Member

My question is this, if you use pocket holes to attach the face frame to the box do you also use glue? I know glue will be a better job but is it really necessary. I make my face frames with 2 pocket holes at each joint and i also use glue. I started using pocket holes to attach the F.F. to the box a couple of years ago but before that i always just glued and clamped them. Lately I've been just using pocket holes to attach the F.F. to the box but always wondering if I'm making a mistake by doing that. So lets say an upper box 24 inches wide and 30 inches tall and i am able to put pocket holes on all 4 sides 3 across the 24 and 4 up the 30. Has any one had problems with just pocket holes for this?

2/7/16       #2: Do you glue face frames to box? ...
Dustin orth Member

Website: http://customwoodmontrose.com

I think I have one more screw per side but we use the same method and have for years.

2/7/16       #3: Do you glue face frames to box? ...
Leo G  Member

Website: http://www.lrgwood.com

I'd put the glue on it. I rarely use pocket screws for face frames. On my lowers the top rail is attached by PS but with lots of glue. Just to limit the amount of clamps I need. Usually I use full clamp and glue for FFs because I do a full flush corner.

2/7/16       #4: Do you glue face frames to box? ...
Kevin Jenness

How much time do you save by not running a bead of glue around the perimeter? Your screw pattern seems a bit light to me even without glue. I don't suppose the face frame will actually come off without persuasion, but a little glue is cheap insurance. Just my $.02.

2/7/16       #5: Do you glue face frames to box? ...
Mike Fuson

Mike I've used pocket screws to attach boxes to face frames for years and without glue. Never had a failure. On a 30" upper I would probably use 5 screws. Honestly, with that many screws around a cabinet what on earth could pull it off?

2/7/16       #6: Do you glue face frames to box? ...
Leo G

Website: http://lrgwood.com

Because over time, with the expansion and contraction of the wood, screws can loosen over time. I use the screws as clamps.

2/8/16       #7: Do you glue face frames to box? ...
chris

Website: http://www.hofmannjoinery.com

I use these clips from Lamello to put my face frames on. You can flat finish at the shop, especially when FF is a solid color and needs to be finished separately from box. I also use them to connect face frames to each other on adjoining cabinet boxes, and for my scribes. AND... I use them for building frameless cabinet boxes too. They're pretty awesome.

Lamello Clips

2/8/16       #8: Do you glue face frames to box? ...
Mark  Member

For face frames, I use the pocket screws as clamps while the glue dries also; I usually don't use more than 8 a box, less if I can. Sometimes I get away with 4.

2/8/16       #9: Do you glue face frames to box? ...
Dustin orth Member

Website: http://customwoodmontrose.com

I should clarify, we only use pocket screws, no glue and about every 6" or so. Never had one come loose and even when someone does something stupid, like drop the cabinet, it doesn't come loose or break.

2/8/16       #10: Do you glue face frames to box? ...
Mike Member

I appreciate your responses and thank you. I'll add glue when i can with the pocket holes and not worry so much when i don't use glue I'll just add more screws. I think it would be just fine. Thanks

2/12/16       #11: Do you glue face frames to box? ...
JeffM

The only weight the face frame bears is the doors. Really no need for glue. The life of an average kitchen these days is much less than what it would take for the screws to lose any holding power.

2/12/16       #12: Do you glue face frames to box? ...
Mike Fuson

I agree Jeff.

2/12/16       #13: Do you glue face frames to box? ...
Leo G Member

So this is were you guys want to cheap out? 1/2 cents worth of glue and 30 seconds of time? Really?

2/12/16       #14: Do you glue face frames to box? ...
Dustin orth Member

Website: http://customwoodmontrose.com

No this is not where we cheap out. All of our face frames are stained, glazed and finished off the cabinet box. Glue doesn't stick to finish. Look at my website and you'll see I don't cheap it at all. No melamine or mdf at all. All 3/4 ply core with 1/4 backs and 1/2 nailers behind those for pulling the crappy framing and drywall straight. More often than not we pop drywall screws when we tighten our cabinets to the walls.

2/12/16       #15: Do you glue face frames to box? ...
Mike Fuson

Leo, I mean no disrespect at all to you. You've given me good advise on here several times. There are places where glue on a cabinet is necessary. I started glueing face frame joints several years ago to prevent shift. End grain to face grain will tend to shift. It's not a matter of being cheap, nor a matter of saving time with me. I just think it's overkill on this particular application.

2/12/16       #16: Do you glue face frames to box? ...
Jeff M

Here's the other question...How much does glue really matter when it's being applied to plywood edges.? I say not much. It's a small step above end grain.

2/12/16       #17: Do you glue face frames to box? ...
Bill Hagers

We do glue dado's and clamp the sides, flat face glue for upper and lower. Staple at 45 degrees and pull the clamps out. Never had a call back and it's incredibly strong. There are a lot of ways to go about this but I prefer to build the box on the frame. You just have to find what works best for you and your resources. However nothing is worse than those on site 'cabinetmakers' that just nail the face frame parts onto the box with no pocket screws like their are building cheap wainscotting. That's an excellent way to see every joint you make open up in short order.

I would say if you are going to pocket screw it on with sufficient fasteners glue is unnecessary. It's an extra few cents maybe but the argument I would make is cleanup. If you're doing stain grade glue squeeze out wiped up can be a real pain. Sometimes I will go with just pocket screws to avoid any cleanup. If you can't physically pull the frames off the box with your bear hands I seriously doubt it will ever come off under normal conditions.

2/12/16       #18: Do you glue face frames to box? ...
Dustin orth Member

Website: http://customwoodmontrose.com

No this is not where we cheap out. All of our face frames are stained, glazed and finished off the cabinet box. Glue doesn't stick to finish. Look at my website and you'll see I don't cheap it at all. No melamine or mdf at all. All 3/4 ply core with 1/4 backs and 1/2 nailers behind those for pulling the crappy framing and drywall straight. More often than not we pop drywall screws when we tighten our cabinets to the walls.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello