3/14/16       
matthew

Anyone have experience veneering a luan door? Any do's and dont's? I don't see an issue but i thought i'd check here. Thanks

3/14/16       #2: Veneering a Luan door ...
Mr Obvious Member

Is this door:

Interior or exterior?

Solid core or hollow core?

Passage or cabinet?

Finished or unfinished?

How will you attach the veneer?

Glue type and process?

Veneer is raw, paper backed, two-plied or?

3/14/16       #3: Veneering a Luan door ...
matthew

Right. Info helps, lol.

these are interior doors

client is looking at solid core

these are all passage doors to match the kitchen we are building them

they will be finished

veneer glued and vacuum bagged

probably would use 10mil paper backed veneer. 8x4 rift white oak

3/14/16       #4: Veneering a Luan door ...
Peter Rawlings

Seems you've got a handle on it, Matthew.
I'd go solid core for sure for a couple reasons. A more satisfying closing experience (marketing hype!) and won't squash them in your press.

I've never tried bagging a hollow core, but many I've seen are kinda wavy which I assume is the fault of coring material. Plus they sound....well, hollow when closing!

3/14/16       #5: Veneering a Luan door ...
jake

I would build my own core for this. Custom veneer work deserves, a quality custom built core. Agree with going solid.

Don't throw away your reputation because the client insists on having you veneer a $20 box store door slab.

3/14/16       #6: Veneering a Luan door ...
matthew

I agree Jake. However this is my neighbor and they are already spending $80k on cabinetry and have asked me to help them with this. They know it's low quality but don't want to spend the $1300/per to have us build them. thx

3/14/16       #7: Veneering a Luan door ...
Kevin Jenness

Years ago I was handed a couple of solid core oak faced doors from a major manufacturer to veneer with red birch to match a kitchen I was building. I sanded them, put them in the bag, and when they came out the veneer was loose on the ends because the door shop's sander had left a major snipe I failed to detect. Peeled it off, sanded flat and did it again, it worked and no callbacks. Make sure the blanks are flat enough to work with your press.

They will not think you are helping them out if the doors are not up to the quality of the rest of the work. I would pass on it unless I was sure I could do it well.

3/15/16       #8: Veneering a Luan door ...
Snaglpuss

My father did a bunch of them using 1/8 oak door skins.
Might have to move the stops of shave them down.

3/15/16       #9: Veneering a Luan door ...
rich c.

I hate paper backed veneer. More than a few times there have been issues with adhesion talked about on this site. I agree with the door skins, two wood plies. I'd be cautious of even throwing a solid core in the vacuum bag. No idea what kind of voids and conditions under the skin. I get a kick out of what they call solid core. Usually just a slab of particle board these days. Lucky if it is really solid.

3/16/16       #10: Veneering a Luan door ...
David R Sochar Member

If you look around a bit, I bet you will find that a local solid core vendor can get you some R W Oak faced doors off the shelf for a reasonable price. I often forget that some things are common, and then go about making it by standing on my head, etc.

Last I got some doors like that, they were about $180 each from the wholesaler.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello