Methods of attaching finished sides to face frames

4/29/16       
Mike Fuson

Wondering how you guys that build face frame cabinets attach the finished sides to the face frame? I've always milled a dado down the edge of the frame that sits 1/4" over from the edge. I'm happy with it just exploring different options. Thanks

4/30/16       #2: Methods of attaching finished sides ...
Nick Cook Member

Website: http://www.cedarrivercabinetry.com

We glue and clamp, using combination core 3/4 ply. Just a butt joint. Then flush cut the edge of face frame.

4/30/16       #3: Methods of attaching finished sides ...
Mike Member

I'll also glue and clamp but where it will be butted by another cabinet i will use pocket holes. If its a painted cabinet i sometimes will pocket hole all around and skin the sides that show. I do not do production work so this works for one of a kind jobs.

4/30/16       #4: Methods of attaching finished sides ...
JeffM

I did integral finished ends for years (I presume this is what you're talking about). I switched to applied finished ends a few years back and would never do it differently after seeing all of the advantages.
I build all of my boxes out of prefinished 3/4 ply and screw the complete box to the faceframe. I leave the box back from the edge of the faceframe 3/4 when I have a finished end and apply the ends on site when installing.
One of the biggest advantages to building this way is loading and hauling the cabinets as you have not finished ends that can be damaged when lugging those boxes in and out. The end panels are seperate and never get damaged.
Finishing is also much easier as your box is prefinished and you can spray your finished end laying down separate from the box. Makes everything much easier and cleaner.
You don't have any clamp marks on your faceframe or glue or other hassles to deal with.
Give it a try.

4/30/16       #5: Methods of attaching finished sides ...
Nick Cook Member

Website: http://www.cedarrivercabinetry.com

A consideration in doing applied ends is that
you will have an intentional seam between the end and the face frame. We build all our finished ends with an extended stile to the floor so in our case the stile would be vulnerable in transporting. I personally like the look of a seamless end to face frame look. We also bevel or round over the corner from the bottom of the top rail to the top of the bottom rail to give a furniture like end.

5/1/16       #6: Methods of attaching finished sides ...
JeffM

I guess if there is a drawback to applied end panels, It could be the small joint between the back of the face frame and the panel edge.
However, if you detail the joint correctly most of my customers prefer the look and the benefits far outweigh any personal preference for not seeing the joint. My guess is 95% of homeowners could not pick out the difference if shown the two side by side.
I put a small 1/8" round over on the back of the ff and the front edge of the panel. When they come together, it looks very clean and professional.
Like I said in the earlier post....it's much easier to transport a box with plywood sides that will be covered that trying to protect the finished ends when loading, unloading and installing. They can be banged together, rubbed together or even put a huge gouge in the side of them when moving and none of it matters because the finished end will cover it.
Just my 2 cents after 25 years experience.

5/1/16       #7: Methods of attaching finished sides ...
Kevin Jenness

Miterfold.

5/2/16       #8: Methods of attaching finished sides ...
Adam Spees

Yeah, what he said

5/2/16       #9: Methods of attaching finished sides ...
Pablo

since the late 70's I've used biscuits to attach frame to boxes. And where the finished ends are plain I use a chamfer joint. not with paneled ends.I like them tight.

5/2/16       #10: Methods of attaching finished sides ...
Mike Fuson

Kevin, what are you calling a miter fold?

5/2/16       #11: Methods of attaching finished sides ...
Kevin Jenness

MIke,

I miter the edges of the face frame and end panel and use packing tape to hold the seam together as I glue and fold the joint. No clamps required except to hold the panels square to one another. It's not the most wear resistant corner with a plywood return, but the joint is very strong if the angles are correct and is clean in appearance and easier to accomplish than clamping a butt joint with frame and panel ends.

5/2/16       #12: Methods of attaching finished sides ...
Kevin

I do the same as JeffM. Biggest benefit for me is being able to scribe a loose panel vs the panel attached to a cabinet. I tend to build cabinets as big as I can, and often need a few attempts to get a perfect scribe. Easier than dealing with the whole cabinet when working by yourself.

5/2/16       #13: Methods of attaching finished sides ...
Mike Fuson

Jeff, how do you attach the applied end? Screws from the inside?


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello