Dowels in cope and stick joints

6/1/17       
Vince Member

I am considering using dowels to aid in strength in some cope and stick hard maple cabinet doors.

The infinity cutters I have give a 3\8" tenon, which is not quite what I would prefer depth-wise on the larger and glass doors.

I do not want to invest in any new tooling at this time. Also, I would be glad for the extra ease-of-alignment the dowels would provide.

The doors are to be 3\4" thick, 2 3/4" wide rails and stiles with solid wood panels.

Should I be worried about the dowels "telegraphing" through the finish?

Possibly dowel thickness would be the important thing.. 1\4" 5\16, 3/8?

Any input is appreciated.

6/1/17       #2: Dowels in cope and stick joints ...
Jr Lee  Member

Website: http://www.leecabinets.com

Vince I have been making cabinet doors as you describe with the 3/8 tenon and have never had any issue in 10 years. Mostly oak and maple and birch hardwood. Numerous large doors for pantrys also. I think the dowels are not needed. I am trying to get new tooling with longer tenons but only because I think they look a little better.
Jr

6/1/17       #3: Dowels in cope and stick joints ...
Larry

I'd bet the dowels would cause you more problems than they would solve. As long as you have a nice slip fit on your cope/stick they will hold fine.

6/1/17       #4: Dowels in cope and stick joints ...
Vince Member

That is reassuring guys.

What is the size relationship we want between a mortise and tenon? My cutter is making the tenon 6-7 thousandths less than the mortise opening.

6/1/17       #5: Dowels in cope and stick joints ...
Larry

That's pretty lose. Is your set adjustable? Most have some way of shimming to adjust fit. .004" should be max for most fits. .002 will give a nice sliding fit and keep from wiping too much glue of when slid together.

6/1/17       #6: Dowels in cope and stick joints ...
al

1 dowel 3/8"x 2" per joint. Once you have a good set up you will wonder why you never used the dowel before. So much easier to assemble.
Is it stronger, not even close. Much better with dowel.

6/1/17       #7: Dowels in cope and stick joints ...
Vince Member

Interesting Al. Do you ever notice an imprint telegraphing through the door where the dowels are located?

Larry, I can put shims in between the rail set to give a larger tenon. So is a tenon 3 thou less than mortise the goal? I though I read somewhere that a bit more space is preferable for a strong yellow glue joint.. like 5 to 6 thou.. I could be wrong.

6/1/17       #8: Dowels in cope and stick joints ...
Larry

Vince, We may be splitting hairs here. If your joint has some friction when you slide it home that's probably a good fit. It shouldn't take a lot of force.

As for the doweled cope, it may be stronger if perfectly executed but it may also harm the fit by off setting the tenon to one side so all the slack is on the other and the tight side gets its glue wiped off. At any rate strong enough without the extra step. Want it stronger yet? Put two dowels in.

I used to travel fixing other peoples equipment. You wouldn't believe some of the terrible cope & stick joints that some of the big operations put out. Brazed tooling, that had been horribly sharpened way to many times, was a big problem.

6/2/17       #9: Dowels in cope and stick joints ...
Adam

The scientific answer to your question is destructive testing. Take one of your 3/8" coped doors and drop it on the ground on the corner. Take another one and securely clamp the stile to a workbench push on the other stile door until it breaks.

Our Freeborn sets are 1/2". I would not trust a 3/8" tenon on a glass muntin. The 1/2" allow you to use space balls or the equivalent. The cabinet door companies typically use 5/8" or some metric equivalent.

It also depends on the wood. If you think about it the tenon is not the weak part. The long grain of the profile is the weak part. I remember having all kinds of trouble profiling vertical grain cedar for some project. The shaper would rip the profile off occasionally. If the panel was a wee bit thick it would likewise break the back of the profile. In some ways the deeper the groove the weaker the door.

If you are doing ply or mdf panels, glue them into the stile and rails. We've been doing this for over 30 years.

6/2/17       #10: Dowels in cope and stick joints ...
al

Dowel does not telegraph through. No different than doweling a frame together.
Everyone has their own methods, after doweling the doors for several years now
I would not go back to doing them without. The trick is to make drilling your holes accurately which takes some time to get the right set up.

6/2/17       #11: Dowels in cope and stick joints ...
eric zeszotarski

lots of good advice from the previous posts.
i don't have a proper dowelling setup but often use dominoes (as long as possible, often 8x80) to reinforce these joints in cabinet doors- especially when they have a glass panel or are particularly large. telegraphing has not been an issue. otherwise glueing in the panel (unless it's solid wood of course!) increases the doors integrity quite a bit.

6/2/17       #12: Dowels in cope and stick joints ...
Jim Clark  Member

Website: http://s51.photobucket.com/albums/f386/jcquack/Fur...

Telegraphing is usually the result of sanding
the face before the glue dries.
this can happen easily with biscuits that hold
a lot of glue, it swells the wood around it
and shrinks back after sanding the face smooth.
I've never had dowels telegraph but if you're
concerned, just allow it to dry a couple of days
before sanding the frame flat.

6/2/17       #13: Dowels in cope and stick joints ...
Vince Member

This is what draws me to wood working; so many intricate (potential) problems to solve.

I agree that dowels could cause a lot of trouble in relation to a cope and stick joint if they were not indexed to within a couple thousandths.

As far as destructive testing goes, sounds fun, but I never seem to have the time to do that sort of thing, especially while trying to learn so much on the finishing end.

I will need to dowel the large glass doors for sure. The standard doors have solid panels with space balls; the larger ones of these could use a bit more strength as well.

I will get some 3\8" drill guides and make some clamp blocks for quick and accurate alignment. One 3\8" x 2" dowel should give me peace of mind on the larger units.

Thanks everyone for the honest input.

6/3/17       #14: Dowels in cope and stick joints ...
David R Sochar Member

I used to teach a weekend long beginning course in mortise and tenon joinery. We all made several cabinet door type frames, no panels. Some were coped with integral tenon, some were square edge with longer tenons, and some were cope and stick with a long tenon. We did dowel joints with a funky jig, nothing to proud of in the final result.

On the second day, we destroyed one of the frames we made the previous day. They were all amazingly strong (excepting the dowelled joints), and taught the students a good lesson on putting two pieces together in proper fashion.

The governing factor to strength is surface area of glued joint, as seen by destructive testing.

6/3/17       #15: Dowels in cope and stick joints ...
Vince Member

Except the dowel joints?? Explain!

6/3/17       #16: Dowels in cope and stick joints ...
Adam

One of my old school craftsman guys used to put (2) 1/4" dowels in all of his door and face frame joints. He had built a dedicated low tech mortiser back in the 60's and was still using it when he passed away in 2008.

I wouldn't use a 3/8" dowel in a 3/4" piece of wood. Regardless if it was edge gluing boards or a door joint.

6/4/17       #17: Dowels in cope and stick joints ...
Vince Member

That makes sense. It seems like the 3\8"tenon is not so bad, with many people using them alone. I will just dowel the glass doors since I am using custom trim cleats (not silicone) to hold the glass in.

What glass does everyone use in their doors? 1\8" tempered? Un-tempered?

6/5/17       #18: Dowels in cope and stick joints ...
Larry

Tempered, lawyer protection! Cost is very little more and the glass company delivers every week.

6/5/17       #19: Dowels in cope and stick joints ...
Vince Member

Gotcha

6/6/17       #20: Dowels in cope and stick joints ...
Adam

We use laminated

6/9/17       #21: Dowels in cope and stick joints ...
Vince

I took one of the 3/8" cope and stick doors apart, just breaking it with slow pressure over the edge of the work bench. (Most of the door on the bench, pushing down on the stile).

The door was 15" wide x 23.5" tall.

The surrounding wood broke. Looking at it, I agree that 1\2" tenons would not be much stronger. They might make the doors go together flat a little more, they might make it possible to do deeper profiles, but when it comes to strength, if you get a good fit between the parts, and fill it with glue, the groove breaks along the whole length of the stile.

While doweling the joints would only make them stronger, I am skipping them on this project.

6/9/17       #22: Dowels in cope and stick joints ...
Jim Clark

The real question is,
How strong does it really need to be?
I've used coped joints and 3/8" doweled
frames in cabinets and furniture for over
35 yrs now and never had one break.
If someone breaks one of these, they're
abusing the cabinet.

6/12/17       #23: Dowels in cope and stick joints ...
JR Rutter Member

Website: http://harmonicdesignworks.com

Are you talking about doors with a profile on the inside edge, or shaker/mission style where the tenon itself is the only long grain glue joint?

For cope and stick with a profile, there is plenty of good glue surface with a shorter tenon. For a simple square stub tenon alone, a longer tenon/deeper groove gives you more glue surface area.

6/13/17       #24: Dowels in cope and stick joints ...
Jarvis

Vice have you ever reglued a door with a dowel you won't ever have to.
We used to use a 3/8" dowel till we got a doweling machine now we use an 8mm dowel both work great.I wouldn't ever build a door without one.

Jarvis


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello