Osage Orange

7/28/17       
Kevin Member

I have an upcoming kitchen in which the homeowners would like to use some osage orange from their property. Right now it looks like it would be used as an island top. It will be milled and kiln dried by others. The logs look like they may net 5" or so. Having never worked with this wood before, is there anything I should be concerned about? Is it any more or less stable than other species?

7/28/17       #2: Osage Orange ...
David R Sochar Member

I have used some air-dried Osage for handles and things. It is very hard. The yellow does not last, but is fun at first.

5" logs will not yield much in the way of lumber. Make sure the kiln guy knows how to dry it.

I don't know about stability.

7/28/17       #3: Osage Orange ...
Larry

I have also only used it for smaller items. You will have narrow strips and I suspect if it is dried properly you shouldn't have stability problems. The yellow will turn to a rich brown with time. I would try to use mostly heart wood. The sap wood is off white & if I remember correctly, softer.

7/29/17       #4: Osage Orange ...
rich c.

I do know the sapwood has much different characteristics than the heart wood. During drying it really shrinks. It will cup a board really badly. Not uncommon to have star shake in the heart. I hope you bid it high, you are in for a rough time!!!!

7/29/17       #5: Osage Orange ...
ranliker Member

It is very, very hard.

7/31/17       #6: Osage Orange ...
Matt M

Agreed with the above, it's exceedingly hard. It is, however, great fun to work with. All the Osage I've ever done (one maaaaaaassssiiive tree) I did on a lathe, and to date it's some of the most fun I've ever had in woodworking. Grain is super smooth once you sand it.

You can expect, however, for it to warp, shrink, or crack if you do it as a large single slab.

If the clients require any warranty, the only way I would warranty it would be to have it milled up as 8/4 and kiln dried, and produce it as butcher block 1.5" strips.

Even then I'd have a moisture meter handy before gluing up.

It should glue up fine. I've never had problems with wood glue sticking to it.

Should make for a fantastic countertop, honestly. Hard density, smooth texture.

8/1/17       #7: Osage Orange ...
Keith Newton

Kevin, While this isn't mission impossible, it's probably one of those jobs that your going to wish onto someone else.

A 5" d log isn't going to yield anything useful for an island top.
It might however could be used whole at the corners of the lower case to support another slab top.

I did just that on a rustic island a couple of years ago, where I stripped the bark, including out a couple of branches, which became grown in braces to support the outer edge of the bar-top.

I cut a 90º inside corner out down the length, which fit around the corner of the island carcase. The work side of the island was 36" T, with a 42" bar top.

Keep that thing wet until you strip the bark, and it' will be easier.

While I love this wood, I have a small log that size which has been laying out by my Wmizer LT15 for over a year which I haven't bothered to saw due to that small size.

Drop me an email, and I'll send you a pic of what I described above.

8/1/17       #8: Osage Orange ...
Kevin

Thanks for the responses. I wasn't clear on the log size; I meant that the boards end up 5" wide after milling. I planned on having them milled to 8/4 and kiln dried.

8/2/17       #9: Osage Orange ...
rich c.

8/4 osage is going to be a tough kiln schedule. Be prepared for a long wait!

8/2/17       #10: Osage Orange ...
chris

not sure where you are located, but realistically you will not be able to cut the osage, go straight to the kiln and have lumber in a couple months. I would look for someone with a vacuum kiln if it's needed right away. It's a tough drying wood. But beautiful

8/3/17       #11: Osage Orange ...
Kevin Member

Thanks for the input. I know very little about the drying process so I will check with the guys who are handling that end. Not sure what type of kiln they use. We have until thanksgiving to finish, so maybe they can get it dry by then.

8/7/17       #12: Osage Orange ...
Matt M

I would not warranty something dried that quickly, just to be honest. If they demand it, I'd probably do it, but I would not warranty it. I'd make sure they understood the risks.

As said above, Osage is a persnickety lumber for drying.

Still one of my top favorites.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello