Cabinets on a boat

8/9/17       
Bob

I have a customer that needs cabinets in a galley on a push boat. The boat is used to push/guide barges on the coast of GA. They will be subject to the high humidity and salt air. I realize that all hardware & screws should be stainless steel to avoid corrosion. Where is the best place to get SS hinges & drawer guides? Should a special plywood be used for the cabinet boxes? The customer was showing me pictures of cabinets with 5 piece doors but I know these will not hold up long term. Going to suggest a vernier slab door. What would be a good finish for the cabinets. I have been building cabinets 30+ years and this is a first for me. I would normally turn this job down but this is a good friend and also a very good repeat customer that I have done a lot of work for in the past. Any suggestions will be greatly appreciated.

8/9/17       #2: Cabinets on a boat ...
rich c.

Plenty of outdoor cabinets being made now. All from different plastic or PVC. If you are worried about that much humidity and salt air, I wouldn't use wood.

8/9/17       #3: Cabinets on a boat ...
Leo G

I've made wooden cabinets for boats. Everything gets coated with West System Epoxy before finishing. If you do the epoxy coating properly and thoroughly it will be impervious to the conditions.

8/10/17       #4: Cabinets on a boat ...
Bruce H

A five piece door would be traditional in a boat such as your description. Not that it now would need to be so. A marine grade plywood might be easier in the long run, some balk at the cost. Jamestown Distributors will have some of what you are looking for. SS drawer guides might be a little harder to come up with.

8/10/17       #5: Cabinets on a boat ...
Alan F. Member

Lamp Sugatsune has stainless slides and hinges.

Years ago wood on boats was either Teak or Mahogany.

Look at Marine grade plywood or Medex cores for cabinet parts.

All materials need to be well sealed, and finishes and maintained regularly.

You could also look at solid phenolic/compact laminate for interiors.

A-

If its

Lamp Website

8/10/17       #6: Cabinets on a boat ...
Keith Newton

West Marine is a good source for plenty of boating needs, from hardware to finishes. Their catalogs always have a couple of pages of tips for what to use in each category like finishes to caulks or specialty things. There are some nice Teak trim pieces if your going to round corners to keep them human friendly in rough seas.

West Marine Link

8/14/17       #7: Cabinets on a boat ...
Luke

Website: http://www.calwoodinc.com

Go polymer (King Starboard) with stainless hardware.

These guys are great and they'll even build it and ship it to you:

https://www.boatoutfitters.com/before-after-projects

8/14/17       #8: Cabinets on a boat ...
Matt M

Starboard is nice, we just built an outdoor kitchen with it, but on a boat it's going to be supremely heavy. Client may not care for that.

The handful of boat/ship projects we've done required us to use light materials.

Personally I'd be OK using an exterior grade wood, sapele is particularly nice (although it is somewhat heavy as well, but not as much as Starboard).

8/14/17       #9: Cabinets on a boat ...
The Cajun Craftsman Member

I have done several boats and have a friend that does boats exclusively for 25 years. From push boats to 150' supply boats. They really don't do anything different except putting stainless hardware and additional catches on doors and drawers. Some not even that if they stay in inland waters. They use no special woods unless requested. Most of theirs are maple. Each cabinet box is independent of each other to allow for movement. It is no different from having cabinets done in a beach house.

8/20/17       #10: Cabinets on a boat ...
cabinetmaker

birch plywood is fine hell, I bet the new UV would last in the galley

We made tackle boxes and laminated them with exterior grade contact cement and color code p-lam would last about 4 years between the sun and weather......

Interior use, I would put the fixed shelves about 1/4 below a face frame or attach aluminum cleats to keep glasses and such on the shelves euro hinges and positive lock latches would do the trick to keep the doors shut and stuff in the cabinets


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello