Panel Genie

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

bowed cabinet door

10/18/17       
John B Member

Website: http://woodmanseewoodwrights.com

I have had a callback on a year old custom kitchen job that involves a slight bow in a 5' high cabinet door. These doors are 3/4" thick hard maple with a 3" wide stile and rail and 3 separate panels with 2 intermediate 3" rails separating them. It is one of a pair of double inset, flush doors on a pantry cabinet. The left side door has stayed very straight, while the right side has developed about a 3/32" bow so there is just a slight misalignment when shut. I'm hesitant to make a new door, with no guaranties that it will stay perfectly straight in a 5' height either, plus it was a custom color pigmented finish and they have been very picky about finish issues to begin with. What type of tolerances do you guys allow for door bow in this tall of a door and any suggestions for trying to correct this bow without resorting to a new door? I had thought about a kerf on the back, top to bottom with a 1/8" thick metal flat stock epoxied in or even an angle piece. These doors have 5 hinges each, and I have tried adjusting the stops to split the difference but they are looking for something better.

10/18/17       #2: bowed cabinet door ...
Matt M

I dont' recall the maximum height that we will warranty but I'm pretty sure we don't warranty anything over 5', and the client is made fully aware of it.

If you've exhausted all your other options, your best bet is the door straightening kit from somewhere like Hafele. A 3" wide stile should be plenty of room to put one in.

The ones I'm familiar with use two 35mm hinge bore holes and dado connecting them (along the approximate center of the stile). The straightening comes from adjusting the nuts on a long piece of all-thread included. They work very well. Just tedius to do.

You'll need one of your more detail oriented team members to do this, it's not a task for an apprentice to tackle.

Biggest hurdle is locating where you will dado it without interfering with the screws for the door pull.

10/18/17       #3: bowed cabinet door ...
David R Sochar Member

Website: http://www.acornwoodworks.com

I have inlaid a piece of 3/8" th x 1/4" wide x full length solid wood into the back that has an 'opposite' curve sawn into it. The advantage here is that you can make a piece with 1/2" bow to it, dry clamp it to the door top and bottom (after the plow) and see how it pulls the door stile straight. Increase or decrease the spline bow if needed. When you glue and clamp, be sure to have a straight edge on the exposed face of the door, just under the spline, so that it goes into a straight stile.

This is a real fix, that will pass under most 'no compromise' situations. No water or sun, no cross clamping, no butchered chickens or full moons required.

10/18/17       #4: bowed cabinet door ...
Jared Emery

Website: facebook.com/moduswoodworks

I feel your pain. When 3 doors that were somewhere around 112" tall warped on me, I dadoed a 1/2" wide slot on the edge similar to what David did with his hardwood strip, but used 1/2 x 1/2 steel bar stock bent to the opposite curve. The dado's tight enough that the bar can be pushed in and bend the door back straight, but not so tight that I couldn't get it out to get the bend just right and try again. Once it was dialed in, I shot some 5 min epoxy to keep it in place and repainted the back side. These were paint grade doors that were pretty fancy for us, and I really didn't want to remake. It's now our go-to solution when an expensive door doesn't cooperate.


View higher quality, full size image (480 X 640)

10/18/17       #5: bowed cabinet door ...
DS

A few years ago I was browsing the Conestoga Wood catalog when I came across their house doors section. They are selling interior house doors by glueing two of there cabinet doors back to back. I'd been looking for a solution to keep tall cabinet doors straight because we do a lot of them, so I decided to try it. We've done dozens of taller cabinet doors this way now and they are perfectly flat and they stay that way. Every door we do now that exceeds about 60" gets done this way. I factor the cost into my bids, but compared to the call backs and other alternatives it's the most economical solution I've found.

10/19/17       #6: bowed cabinet door ...
Adam

The regular Blum clip hinges are 3/4"-1 1/8"

In the future, you could make them thicker and use more hinges to keep it straight.

10/19/17       #7: bowed cabinet door ...
Paul Miller

Website: http://MCCWOODWORKING.COM

I would try the angled steel if you have room. If you do use the steel, I would put a piece on the other cabinet door as well.

I have also used All Thread rod to straighten panels. If you dado a slot into the back of the door, put a length of All Thread rod into the slot and fill the void with epoxy. I have used West System epoxy. I mix some sawdust with the epoxy to thicken it. Of course, put the door on a flat surface, clamped down.

I have done this on wooden tops. I use 1/2" All Thread. This might be a little more difficult on a 3/4" door. You would be routing most of the way through the stile.

Good luck. These things happen.

10/23/17       #8: bowed cabinet door ...
Matt M

I really suggest you guys look into the door straightening hardware I mentioned above from Hafele, and I'm sure it's avail elsewhere.

The real benefit to it is that it's fully adjustable. You don't have to guess at it.

And if, for whatever whack reason, you get a call back that the door warped again, just a couple turns of a small wrench and the door is straight. We've never had a call back on one of these but it's still very adjustable if we did.

10/24/17       #9: bowed cabinet door ...
David R Sochar Member

I have heard about the Hafele product and its success. I have no doubt it works.

But:

I like a shop made fix for several reasons: It is available now, or in a few minutes, it works, it blends in and covers up so it is an invisible fix, it does not alarm the customer by being visible and 'adjustable', it is local - you do it in your shop with your ingenuity, giving rise to a higher level of craft and self-worth.

10/27/17       #10: bowed cabinet door ...
Pat Gilbert

"self-worth"

That is funny.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello