Problem with Square parts from Edgebander

12/8/17       
John Garth Member

I have worked in three fabrication companies now and there have always been intermittent challenges with parts not being square coming off the edgebander. They all have pre-mill stations. I believe it is mostly, if not completely operator error when loading the parts not flush to the fence. When doing as many parts as we do I can see where some percentage of the parts will be mishandled. Although, in an effort to reduce rework I am looking for ideas or solutions that my help us ensure square parts 100% of the time.
As an example, is there an attachment or jig that any of you have used to create a moving 90 degree fence to help hold the parts true to the fence of the equipment?
thanks for your help,

12/8/17       #2: Problem with Square parts from Edge ...
Stuart Douglas

No Jig, just operators that aren't stoned or hungover.

We've been through 3 edgebanders in my career, two with pre-milling stations. You are describing operator error. Operators need to be cognizant of each operation, each time. Get complacent and the work suffers. Simple as that. The only piece that an operator should struggle with is something long and narrow, like banding the end of a back-splash. Even in that instance, if you match the approach speed with the conveyor speed and keep the infeed fence waxed (SlipIt, Bostik, wax) then parts should be 100%. The edgebander can be a sleeping pill for large jobs, but just like anything else in the shop this is what separates us from the chimps.

12/8/17       #3: Problem with Square parts from Edge ...
Chad R  Member

Website: http://www.northwayind.com

Are your parts square going to the edgebander?

12/8/17       #4: Problem with Square parts from Edge ...
John Garth Member

Chad R.,
The parts are square for the most part. Parts are measured and checked for square post cutting and pre-banding. I do not believe this is always happening. Basically the reason for my question. I would like to dumb down the edgebanding process as we run thousands of parts. This would also help us to understand more quickly where the squareness issues are occurring for accountability purposes.

Hey Stuart,
I agree with your appraisal of the situation. You are on the money and follow the procedures noted for the most part. The challenge specific to our company is not only do we do thousands of parts normally, but the schedule expands to tens of thousands of parts for 3 months out of the year. We double our capacity, with primarily temp labor, so dumbing down the process to chimp labor would be helpful. Also, you can only imagine what the cost of rework is to the milling department for 2 or 3 boards when they are running thousands.

12/8/17       #5: Problem with Square parts from Edge ...
Stuart Douglas

I would make a cheat sheet. Print it on heavy card stock and laminate it and hang it by the bander control. Step by step, with benchmarks for acceptability and a team leaders name @ the top who checks the parts periodically. You'd be amazed how effective this simple piece of paper is. The hardest part is setting the protocol in writing.

It is JUST AS IMPORTANT to have the person tailing to be as competent as the person feeding. The feeder can't see how the finished board comes out without taking a walk. If the pair of operators are both trained to run, then they can switch positions to prevent brain fatigue.

We run hundreds of thousands of parts a year and while this process seems simple to someone in the biz, if you are using temp labor, then you will likely have to accept a certain percentage of rework. I have veteran guys here that haven't (wont) been able to pickup competency on our newest machine, I can't imagine bringing in someone super green. Good Luck!

12/8/17       #6: Problem with Square parts from Edge ...
John Garth Member

Thanks for the help Stuart.

12/8/17       #7: Problem with Square parts from Edge ...
Chad R  Member

Website: http://www.northwayind.com

We don't normally have a problem with squareness either, but we mainly use our double sided for squaring. We do have a squaring fence mounted on one of our Homags though. It works well when it is used.


View higher quality, full size image (2219 X 1801)

12/8/17       #8: Problem with Square parts from Edge ...
Stuart Douglas

Thats neat, Chad. I've never seen a squaring arm on a machine like that.

12/8/17       #9: Problem with Square parts from Edge ...
John Garth Member

I had not seen a squaring arm either. Why I asked. Assuming the arm came from Stiles?

12/8/17       #10: Problem with Square parts from Edge ...
Chad R  Member

Website: http://www.northwayind.com

Yeah from Stiles. I have seen them on IMA's also. Its in the Homag edgebander brochures also.


View higher quality, full size image (1741 X 1625)

https://www.stilesmachinery.com/files/assets/files/1503075157_98-450-00149.pdf

12/8/17       #11: Problem with Square parts from Edge ...
John Garth Member

Thanks for the information Chad!

12/24/17       #12: Problem with Square parts from Edge ...
Lee Johnson  Member

I have worked on many machines with pre-milling units and have seen this problem before. If it is an inconsistent issue, i.e. it occurs on some panels but not on others, then I believe some panels are "slipping" outwardly on the track. One way to check this is to mark the front of an 6" x18" panel then pre-mill one 18" side. Flip it over and run the opposite 18" side with the front still at the same end. If your panel is slipping on the conveyor track then your panel will now measure wider at one end: something like a parallelogram. To correct this issue call me at 803 517 4131 for free advice. There are several things that can cause this and I'm too slow of typist to give them all to you here.

2/23/18       #13: Problem with Square parts from Edge ...
Todd

Not meant to be sexist but have you staffed the job with women. Often women are more process and detail oriented than men. I knew a fellow that had a painting and finishing and he ended up almost entirely hiring women because they did a better job on that type of work. Now maybe someone has or can do a study on this topic for their PHD thesis...


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello