1/16/18       
John B Member

Website: http://woodmanseewoodwrights.com

I currently specialize in mainly face frame style kitchen cabinetry, mostly inset doors but some overlay, and use 3/4" pre-finished maple for the box construction. I have bought from a couple of suppliers that will deliver to our location, but see some fluctuations in quality at times. I prefer Columbia product with an aspen/poplar core but it does run more than some other brands with what appears to be a fir veneer core. I'm interested in what others are using, average pricing, brand/mills, in different parts of the country. Here, it runs from the low to mid $60's per sheet to the mid $80's for a more premium product. Also wondering if anyone has found 3/4" prefinished maple with the mdf veneer layers under face. Seems like it would give a smoother face for the times we are doing solid color finishes on end panels exposed.

1/17/18       #2: prefinished plywood ...
Family Man

John, There is a pretty wide variety of products and brands on the market. The price point if they haven't jumped in your market will. A tariff just removed over half of the prefinished plywood on the market- Chinese and that is causing not only price jumps but shortages.

I have found the classic/armor core type product you are speaking about to be a little flatter, less rippling in face veneer. But usually for the client that isn't too much of an issue, especially since it's inside a box with goods stacked on it. Hard to get a real good visual on it.

1/17/18       #3: prefinished plywood ...
chris

I use Garnica, an all poplar core, 2 extra ply's than typical 3/4. Light weight, flat. White birch and in the low $60 UV1S. I have yet to have a sheet delam or not lay flat for me in the 2 years I've been machining it.

1/18/18       #4: prefinished plywood ...
Pdub

So that Garnica is only UV finished on 1 side and it still lays flat?

1/18/18       #5: prefinished plywood ...
chris

Like all other plys, it comes in UV2, but yes the UV1 lays flat. When I run the next batch on the CNC I'll take a picture. Of course ply isn't MDF or PB, but then again I cut PB all the time that has tension in it and moves. I have never had an issue with Garnica UV1 laying flat on the CNC. I also can count the voids I've seen on one hand. It's a WPF white birch, I personally like the prefinished maple. The WPF birch is kind of bland to me but it is the inside of a cabinet and I'm not worried about the bland part. The other issue I have, and it might only be my supplier but my supplier does not carry it in 1/4". So we started cutting the backs 1/2" with no nailers on the backs.

1/19/18       #6: prefinished plywood ...
Hen Bob Member

I 2nd the Garnica

1/19/18       #7: prefinished plywood ...
Adam

We've always used Columbia 3/4" prefinished 1 or 2 sides. Our backs are always 1/2' prefinished 1 side. 16 gauge staples.

I bought a few sheets of the imported stuff about 10 years ago. It was so bad we chopped it up and used it for ladders & kicks.

1/19/18       #8: prefinished plywood ...
John B Member

Chris,
Is this imported from Spain? I'm trying to see if there is a dealer in the NE I could get it from. Atlantic Ply, Richeleiu and Wurth are my closest suppliers.

1/20/18       #9: prefinished plywood ...
chris

It is from Spain, yes. I believe Antlantic ply carries it. They use to be near me. There should be one in ME and MA

1/20/18       #10: prefinished plywood ...
Hen Bob Member

Wurth has it by us.

1/20/18       #12: prefinished plywood ...
Michael Eftink

I tend to use chinese import on the inside of my cabinets...it does vary in thickness and voids, but it is the inside of the cabinets. It runs in the mid 40's per sheet for 3/4" for 1 side finished..add $3 bucks for both sides. I use a higher grade non-import for finished areas on the outside of the cabinet. It will normally run mid $60's for birch or maple.

1/22/18       #13: prefinished plywood ...
Ken Member

We used Columbia for years but have switched to Garnica and been using that for a couple years now. It is about $7-$8 less per sheet and the quality is better. When using Columbia UV1S, we always had a least 2 sheets in a unit that would be scratched badly. I don't think that I have seen one yet in the Garnica. The finish on the Garnica is noticeable smoother and the weight per sheet is less (they claim 30%) which make a big difference for us since we make a lot of really large units that we have to haul up multiple flights of stairs. We buy the Maple UV1S, Maple unfinished, and Maple UV2S.

1/22/18       #14: prefinished plywood ...
Kevin Jenness

I also have had good results with the Garnica line, sourced from Atlantic Plywood. It is not formaldehyde free, if that makes a difference, though it does meet a certain standard (CARB 4?) for emissions.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello