Solid wood edge on glass

3/7/18       
Mark B Member

Set of drawings for a home we are doing from the architect and they have several banks of adjustable shelving in the living areas. These all have interior lighting, pre-wired (by us), in the cabs. The architect is wanting to use tempered in the units to allow the lighting to flood the interior of the space but they are wood faceframe units. They are thinking about applying 3/4" thick x 1 1/2" tall edge band to the glass just as you would to a ply shelf. I havent gotten clarification if this would be via rabbet or dado (lip on the front of the shelf). The edge band would run between the stiles (not completely out to the edge of the glass shelves that project past the stiles). We even kicked around the idea of a slip on option with a rubber weather strip channel but that would never work.

I understand what they are trying to do by hiding the edge of the glass shelf and keeping the unit looking like a conventional wood shelf unit with a transparent shelf.

I floated the idea of a ply shelf with a rabbeted pocket CNC'd for a glass panel to drop in but didnt fly and I could see a ton of flaws in that as well.

We will of course disclaim any option we cant be comfortable with.

I dont see issues with wood movement with a small wood applied face to a glass shelf but I somehow do fear a bit of deflection in a loaded glass shelf overcoming the bond bewteen the glass and the wood (clear RTV?).

Google left me hanging.

Any ideas?

3/7/18       #2: Solid wood edge on glass ...
Jon Member

I would put a 1/4 x 5/8 deep dado (you will need to leave a lip sticking above the surface of the glass), and put some silicon in the groove, then push the glass into it.

I wouldn't think deflection would be a problem with the bond as long as the length of the shelves is kept at a reasonable length.

3/7/18       #3: Solid wood edge on glass ...
rich c.

I've done a lot of shelves with 3/4" x 1 1/2" frame all around the glass. The 1 1/2" is the vertical dimension. With the rabbet, there is only 3/8" of wood extending past the glass. You could make the frame a little less and still get a good result. I suggest you make them a couple samples to show there is no light transmission issues through the shelves.

3/8/18       #4: Solid wood edge on glass ...
Paul Miller

Website: http://MCCWOODWORKING.COM

I have never done this, so I do not have a reference for you. However, something I did learn this last year is that when glass is tempered, it warps, and they have no control on how it will warp. That might present a problem. I don't think you have to have tempered for shelves. This is probably a safety precaution.

Silicone is probably your only choice for attaching the wood edge. Silicone is an adhesive. The Crystal Cathedral in southern California, built in the 80's is built with silicone. Some believe silicone is only a sealant, it is also an adhesive.

3/8/18       #5: Solid wood edge on glass ...
Mark B Member

Thanks guys,
The dado/silicone was my thought but I am going to guess they will want no lip at the edge of the shelf so the rabbet would likely be the option. I wasnt sure if we could trust silicone over the long haul in that situation but it sounds like its worth a go.

Paul, we have seen the warp in tempered. We just brought in a crate of tempered for a job and didnt notice much but it was all for interior window units so any warp was dealt with in the stops.

Our local glass shop never uses tempered for shelves but it seems to always be spec'd as tempered. I do feel much more comfortable with the tempered even just around the shop. In my own house we recently had a large 3/8" thick plate coffee table top that broke and its a wonder someone wasnt cut to ribbons.

We will go the sample route with the dado and the rabbet with disclaimer and see what they choose.

3/8/18       #6: Solid wood edge on glass ...
Alan F. Member

try a PUR adhesive, check with 3M.

3/8/18       #7: Solid wood edge on glass ...
rich c.

You could use a compromise between standard glass and tempered. That is laminated glass. Just like a car windshield. I will crack, but not separated from the film in the center. Only downside is the edge always shows the lamination. Not a big deal when it has a wood edge glued on.

3/8/18       #8: Solid wood edge on glass ...
Alan F. Member

I think the real issue is I would want a square edge to glue to and as a practice the last thing we want to handle is glass without polished or swiped edges.

I think the lack of a square edge to glue to will cause issues we haven't even discussed..

3/8/18       #9: Solid wood edge on glass ...
John Member

Tempered glass is not only a lot safer, it will carry something like 8X the load of untempered glass. I would want to use a dado, as Jon described. A rabbet relies too much on the glue bond. I made the glass doors in the attached photo, including the curved glass panels. The glass is glued with polyurethane adhesive into dados in the door frame stiles and mid rails. Note, there is no perimeter frame. The adhesive holds the glass. 15 years or so now, no creep, and no problems.

John


View higher quality, full size image (2048 X 1536)

2/23/22       #10: Solid wood edge on glass ...
Gregg Nelson

I dont see issues with wood movement with a small wood applied face to a glass shelf but I somehow do fear a bit of deflection in a loaded glass shelf overcoming the bond bewteen the glass and the wood.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!