I know this has been discussed many times but...
We are running one ceros sander and one Deros. Using the pads that have all the small holes in them. I’ve went through a box of the Abranet and wasn’t really impressed. I’m looking to go back to paper. What do you guys recommend as far as brand, sterrate, how many holes, backing, where to purchase, I’d also be interested in the final grit you use before finishing. Thanks for the info.

3/15/18       #2: Sanding preferences? ...
Mark B Member

Basically same as you. Same equipment. Never found any advantage to Abranet and just ran the last of it out of the shop a month or so ago and went back to Mirka Gold. We run 5" 8 hole because it works on some of our non Ceros sanders. 6" is only run on a PC angle grinder type RO. We dont find any issue with DC because with a vac and dust deputy cyclone there seems to be a good bubble of vac around the head of the sander.

On stain finish we try to stop at 150 but often go to 180 go close it up a bit on things like cherry and hard maple. Pigmented is generally 120. Natural finish like oils are way higher than 180 but very rare.

3/15/18       #3: Sanding preferences? ...
Greg Member

We use carborundum sticky discs from E Roko or Richelieu, no huge issues so far. Usually 150 grit or 180 for stain. Greg.

3/15/18       #4: Sanding preferences? ...
Leo G Member

The Abranet is great when you are sanding finishes.

Also the HD lower grit (40-80) Abranet is nice for chewing wood when you need to.

I like the Mirka Gold 8 hole.

3/16/18       #5: Sanding preferences? ...
Stewart Member

We've had really good success with the heavy weight Klingspor stearated 6 hole - a lot of sanding before changing out discs. If we are staining, I find I have to sand to 180 grit to avoid seeing swirls. I almost never have to sand finer than this.

3/17/18       #6: Sanding preferences? ...
door shop guy

Mike, how are you liking the Deros?
I have a Ceros and i LOVE it and wish they still made them but i need another sander. Deros looks too bulky...is it?

For discs, have you heard of 'multi hole'?
My favorite discs for the Ceros are Wurth Emerald velcro Multi Hole. There are a bunch of small holes that allow for excellent dust collection. They are expensive and i get them from Baer Supply.
3M makes a purple multi hole disc but i have found 3M products to be hard to get.
Not many people know about the multi hole discs.
Maybe Mirka Gold has gotten better but i used to hate Mirka Gold.
Carborundum Premier Red is also REALLY good sandpaper and i use it for my Dynabrades on the downdraft machine but they do not offer them in a multi hole.
I never thought that an 8 hole disc would work good on a Mirka Ceros.
I use an older Fein Turbo 2 on my Ceros.
Im always looking but i still have not found a disc that i like more than the Wurth Emerald Multi Hole.

3/17/18       #7: Sanding preferences? ...
Mike Fuson

Door shop guy, the Deros seems to basically be the same sander as the ceros as far as functioning. It’s just like anytime you get a new tool, you have to get used to it. Once you have gotten used to the larger back piece it’s second nature. I will point out that it does have a smaller diameter cord which is less heavy than that of the ceros, I seem to notice that more than anything. It makes it more comfortable to use in my opinion, plus I thinks it’s longer if I remember right. As far as the way it performs I can’t tell much difference between the two, but I do have limited exposure to it, the guy that sands the doors is the main one that uses it
I hadn’t thought about Baer sanding disks, and I do order from them. I used that emerald paper years ago but don’t remember how they did, ive ordered a box each of 80-150-180 of the Mirka Gold to try. I actually think I tried it years ago as well but can’t remember how it did either.
Grainger has the 3m disks listed on their website by the way.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello