Edgebander Temperature

4/14/18       
Larry

Whats a good low/high temperature to run an edgebander gluepot for Jowat unfilled 280.90?

4/15/18       #2: Edgebander Temperature ...
stu

https://www.richelieu.com/documents/docsPr/JW/28/09/04/4/JW2809044/1366828.pdf

4/15/18       #3: Edgebander Temperature ...
Larry

Ive got the spec from Jowat, but the temperature for my glue pot seems too high. They show 210 as the high limit. My pot is set at 205. The glue burns too much. Thought I might set it a little lower. Maybe 200.

4/15/18       #4: Edgebander Temperature ...
Rob Young  Member

Website: http://www.cmsrepair.com

There are two major components to consider when setting the temperature of your glue pot.
1. The speed of your track.
2. The application temperature range of the glue you've selected

You'll notice on the glue manufacturer's spec sheets that these are given in ranges not definitive numbers. The temperature and track speed for the glue you are asking about is:

Application Temp: 190-210 C (374-410 F)
- Feed Speed: roller application: 18-60 m/min (50-180 ft/min).

The amount of time it takes the board to reach the first pressure roller after glue is applied at the pot is known as "open time". This determines what you set the temperature of the glue at. The temperature needs to be within the range the manufacturer recommends.

If your track speed is on the low end, in this case 18 meters/minute you would set the glue temperature at the high end of the recommended temperature range or 210 degrees.

If your track speed is on the high end listed 60 meters/minute you would set the glue temperature at the low end of the manufacturer's recommendation or 190 degrees. The goal is for the glue to be hot enough to squeeze out top and bottom at the pressure roller station, giving a smooth appearance, and be set to avoid de-lamination as the board travels through the various stations. If you set the temperature too hot the banding can slip on the edge or be pulled loose especially in the case of 3mm. Set the temperature to low and the glue doesn't squeeze out properly giving you a poor appearance and de-lamination problems in the field.

Selection of the glue you use is based on the type of edge you are applying and the limitations of your machine.

I normally recommend Jowat 280.3 to my customers. The operating range is:

- Application Temp: 180-200 C (356-392 F)
- Feed Speed: roller application: 5-40 m/min (15-120 fpm)

The feed speed on the 280.3 is typically in a more appropriate range for most edgebanders.
When selecting glue look first at the track speed on your edgebander to make certain the glue is appropriate for your machine and within your machines capabilities. If the glue is appropriate for your machine then look second at the material you are applying to make certain the glue is appropriate for the edging.

4/15/18       #5: Edgebander Temperature ...
Larry

I'll try the 280.3. The feed speed is 12.5m, an old Basic 2. I am still concerned about the burning glue. I seem to have to clean the glue pot too much. Of course, this happens in the middle of a run of edgebanding where the glue pot starts clogging.

4/16/18       #6: Edgebander Temperature ...
Dan

Without knowing the machine...
Check your machine's temperature (actual) to what is set. Take some readings around the pot with a laser meter. If you don't have access, call an appliance servicer, they're usually armed.You could have an issue with the pot's sensor or a heating rod near the sensor. That can cause the rest of the pot to overheat and burn glue.

4/16/18       #7: Edgebander Temperature ...
Rob Young  Member

Website: http://www.cmsrepair.com

Larry, Here are a few tips to reduce burning in your pot.

1. Don't over fill it. If you aren't running parts through your machine 8 hours a day everyday you want to limit how full you keep the pot. You don't want to be guilty of filling the pot all the way up on Monday and running for an hour ever day through Friday with the same glue. There's no reason to have a cycle where the same glue in the pot is heated cooled and reheated unnecessarily. I'm a huge fan of a premelt station and keeping the glue level in the pot as low as possible. Should you ever replace your Basic2 make certain your new machine has a premelt.

2. Make certain the glue temperature goes into a standby mode if you won't be running it for a half hour or more. The temperature should be 140 to 150 C. This will allow a quick heat up and you won't cook the glue in the pot. If you don't plan on running for several hours turn the glue pot off.

3. Clean your pot as needed. Once the glue begins to burn it will continue to build up and cause heating issues in the pot.

4. It's not a bad idea to bring in a tech from SCM or a reputable independent that knows edgebanders. You're machine is an older one that most companies have already replaced. If you want to continue to produce good parts without big frustrations a well tuned machine is critical. At some point you'll draw the line on putting money into an older machine and simply replace it with a more productive newer machine. That point in time will be determined by your production needs and how much money you find yourself putting into your Basic2. I've worked on dozens of brands so I'm more then happy to share my observations with you should you get to the point that replacing your machine becomes an option.

4/25/18       #8: Edgebander Temperature ...
Matt

We determine our required glue temperature in the following way. Has always worked for us.

1) Must be within the bounds specified by the glue manufacturer for that glue.

2) Use the lowest possible temp you can use without having adhesion problems, or "stringy mess" buildup near the glue applicator.

In other words, set your machine to the lowest setting of your chosen glue and start there. Do peel tests. If they feel strong, move forward with production and keep an eye out for stringy glue strands, which indicate that your glue is a bit too cool. Bump it up by 5 degrees Celsius each time.

If getting a good strong glue bond requires you to set the temp so high that it's burning the glue, you are using the wrong glue. Or you have old PVC edgeband with deteriorated primer coating on the back.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello