Edge Stop Grooving

10/6/18       
Brandon

Looking to make 5 piece doors with textured melamine and am having trouble figuring out the most efficient way to do the groove for the panels. The pieces are doweled together and then banded all 4 sides for added strength.

Need the groove to not go end to end, only where the center panel will slide in.

Need a setup that will work for high production.

Any ideas/suggestions?

10/7/18       #2: Edge Stop Grooving ...
D Brown

Tenon the rail ends, you can still dowel if you want to.That way you can run the groove all the way.

10/7/18       #3: Edge Stop Grooving ...
Brandon

The rail ends get edge banded, so tenoning them is not an option.

10/8/18       #4: Edge Stop Grooving ...
Stewart Member

Unfortunately (because they're pricey), the best solution for precise stopped edge routes is a horizontal cnc router machine. I don't personally own one but have seen several of them in action. They are fast, very accurate, and will do most any kind of tenon or groove you can program. Might be worth a look if you are in a high production facility.

10/8/18       #5: Edge Stop Grooving ...
Gary Balcom Member

Brandon,

Unless you're setting up to do a lot of these, regularly, I suggest you consider outsourcing them. There are several reputable companies, including ours that can make these for you.

If outsourcing isn't an option for whatever reason, I bet you could pull off a small project with a router table and some stop blocks.

10/8/18       #6: Edge Stop Grooving ...
Brandon

Horizontal cnc is the only option I could think of as well, seems like a lot to spend for such a simple cut but I have yet to think of another way that would be time efficient.

10/8/18       #7: Edge Stop Grooving ...
David R Sochar  Member

Brandon - Regarding terminology in D Brown's response: "Rails" are parts that run from stile to stile, so the ends of the rails are always butted, dowelled or tenoned. Stiles are vertical parts that run the full height of the door.

Edge band for strength?

Doors from textured melamine? Is there anything else worse to use? Where is the pride in craft?

10/8/18       #8: Edge Stop Grooving ...
D Brown

Acorn, I was trying to picture a banded rail end,,, was gonna ask for a picture.

regards

10/8/18       #9: Edge Stop Grooving ...
Brandon

I think the below pictures will add to the clarity. The rails are banded on the two ends and inside edge, the stiles are banded on the inside edge. Once the door is pieced and glued together with dowels, or dominoes, the door is banded on all four sides.

I have yet to find a method for medium scale production other then a customized horizontal CNC machine.

David - I know what a rail and stile is, and I think this forum is not best utilized to criticize other people. TFL doors have become very popular in European style cabinets and has its place. Many customers prefer a product that is easy to clean, wont warp or shrink, and is water rated - not to mention made from 100% post consumer recycled material.

10/8/18       #10: Edge Stop Grooving ...
duster

Mitered frame, doweled together at the joints. That would make the edgebanding and grooving much simpler, with no need to do a stopped groove.

10/9/18       #11: Edge Stop Grooving ...
Brandon

The only issue with that is textured melamine needs finished edge or you are inviting chipping. Otherwise I would say that is a great idea.

10/9/18       #12: Edge Stop Grooving ...
D Brown

Brandon, after looking at your picture I would still give the same suggestion to tenon the rail ends ,since they get covered with edge banding nothing will show. However you trim the doors to apply the edge band will be the same.

10/9/18       #13: Edge Stop Grooving ...
Brandon

please note the rail ends are edge banded before the 5 pieces are assembled. If I were to tenon the rail ends, that would machine off the edge banding.

10/9/18       #14: Edge Stop Grooving ...
D Brown

So are your dowels going through the rail end edge banding ?

10/9/18       #15: Edge Stop Grooving ...
Brandon Member

Yes, that is correct, dowels go through the edge banding on rail end and stiles.

10/9/18       #16: Edge Stop Grooving ...
Dave L

Splines matching panel thickness or I/H shaped panel?

10/9/18       #17: Edge Stop Grooving ...
Hen Bob Member

Dedicated Shaper? get a nice insert style groover with spurs, couple index marks on a zero clearance fence, wood guard over cutter and a competent operator. since they don't have to be super accurate that should work.

If that ins't productive enough just buy the right machine, probably cheaper than they guy running the shaper in the long run

10/10/18       #18: Edge Stop Grooving ...
Jeff Thomas

The suppliers that make these all the time have a shaper head built into the edgebander, it automatically plunges and pulls out a set distance from the end.

Outsource them.

10/13/18       #19: Edge Stop Grooving ...
Gary Balcom

Jeff is correct, that is how we're setup. Each of our doors has 16 edges banded. It's a better look than the ones that are banded around the perimeter after assembly.

11/11/18       #20: Edge Stop Grooving ...
Madera

Website: http://www.maderakitchenandbath.com

I’m curious as to what type of bander you are running. We have been playing with doing a line of these doors as well. I always thought id just groove through the stiles and edge band all 4 sides after assembly.

Interested to know how you are making out with these.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello