Euro/PB Core in older masonry home

8/16/19       
MarkB Member

Site visit with a contractor we feed. Their customer is wanting a frameless kitchen in an older masonry home. Were talking the old hollow high fired masonry block walls, zero insulation, zero vapor barrier, partial basement, partial crawl space, and even with HVAC and extra dehumidification the home is damp. The basement area while not wet, is clearly just damp even with many coats of interior damp-proofing rolled on the walls. I peeked under the crawlspace and there is zero vapor barrier (bare dirt). The area under the kitchen will be completely vapor barriered and sealed internally when the kitchen is gutted but the remainder of the crawlspace will be left or they may try to lay poly on grade but it wont be sealed to the walls in the rest of the crawl space. They have no plan to fur out the interior face of the exterior walls (cabinet walls) in the kitchen but will likely apply roll on damp proofing (drylock) before plastering (which is a mistake in my opinion but..)..

My concern is the PB core cabs given the moisture. I dont have cost effective access to veneer core in the material they would like not that that would make completely comfortable either especially pertaining to the cab backs directly against the exterior walls on the north side of the home (shady). We kicked around reducing the cab depth by whatever is needed to apply sheetgoods/vapor barrier to the exterior walls behind the cabs. The kitchen is a tight galley style and the homeowner is very reluctant to frame in the walls even by an inch. Again, major mistake in my opinion. Risking your cabs, and to improve the health of your home by losing an inch (or less) doesnt make sense.

Moisture is completely covered in our contract and the contractor has had the conversation with the owner and of course we have had convo with the contractor.

I have not had the opportunity to leave a hygrometer in the space for a period of time but I really dont need to to know that the home is damp.

We can most definitely walk away, and have expressed strong concern, but wondering what input anyone working with the PB core melamine (this would be Tafisa) for years would be. For residential work we are typically prefinished maple interiors (columbia purebond) as we dont often do a lot of frameless on residential work.

8/16/19       #2: Euro/PB Core in older masonry home ...
Alan F.

Use Medex MDF cores, laminate instead of melamine, edge parts all 4 edges with PUR or equivalent resistant glue.

If there are wood doors / fronts. you may want to use an exterior coating that is waterproof.

A typical finish is not moisture proof.

Or you really need an air tight waiver that addresses that cause is difficult and costly to determine and the cost of all testing is by others. That Proof and analysis is at the cost of a mutually approved lab capable of stereomicroscopy evaluation.

That the owner wants to assume all risk to reduce future costs.

8/16/19       #3: Euro/PB Core in older masonry home ...
MarkB Member

Thanks Alan,
I already have the waiver covered though air tight is always a perforated concept.

I dont think the job will ever pay for anything in the realm of a custom/upgraded core and face material. My concern with this job is that I have had sheets/scraps of standard PB core material both raw and banded that we have intentionally exposed to moisture (excessive) and its not a pretty sight though none of them have been banded with PUR. Banding all exposes sides of the carcass parts was an option I floated but again its nothing I would ever stand behind.

Thanks for the input. Its greatly appreciated.

8/17/19       #4: Euro/PB Core in older masonry home ...
Dan

35 years. Done a few of these. Band all edges and drill minimum holes. If the home continues to be excessively damp you'll find more damage over the years in rusted hardware than core failure.
If you've given the lectures and had an 'understanding' signed you've done your job.

8/18/19       #5: Euro/PB Core in older masonry home ...
Adam

Keep in mind how damp a well used bathroom with a shower can get. As Dan mentioned, rusting euro hinges is more common than panels being damaged.

8/18/19       #6: Euro/PB Core in older masonry home ...
rich c.

I'd bring up the fact that mold will likely be growing on the wall and cabinets where there attach to the outside wall. Of course they will likely see that when to old cabinets come out. At a minimum, a 1/4" shim out should be done when mounting the cabinets for air circulation.

8/19/19       #7: Euro/PB Core in older masonry home ...
MarkB Member

Im right with you there Rich. That, and the floor, were my areas of concern beyond the overall humidity level in the house. The cab backs was the reason I had floated even the possibility of making the bozes 22.5" or 23" to allow for some proper vapor barrier behind though as you say the mold will be on the exterior side of the VB at that point.

We are all confident that when they gut the entire floor and completely seal the crawlspace to the exterior foundation it will eliminate a lot of the moisture in the space but there is still a substantial remaining crawl space as well as the exterior walls in the entire home so I dont expect the overall internal humidity to drop all that much.

The homeowner is aware of the problem as they are in the habit of keeping all furniture off the exterior walls by an inch or two to allow air flow.

Its a less than ideal situation but its their home and they love it so you make due.

Thanks a bunch for all your input. I ordered in some PUR for the bander and we will give it a go.

8/19/19       #8: Euro/PB Core in older masonry home ...
Alan F.

I would still document the potential for failure and the owners, and future heirs, assigns etc acceptance with it being the owners responsibility to disclose.

I am trying to eliminate the warranty call / fight 5 years down the road when for some future circumstance the owner has sold / moved and the new owner takes the position you shouldn't have installed to begin with and the new owners don't want to pay 30k to replace 5 year old cabinets.

8/20/19       #9: Euro/PB Core in older masonry home ...
MarkB Member

Fully agree and got that covered Alan. And where we are feeding the contractor he would also be covering the same issues in his contract. While I would never let it go undocumented, I am comfortable that the homeowner is well aware of everyone's concern but the contract end of it is a given.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello