Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Plunging a moulding face into a shaper cutter

10/3/19       
KCR

HI all,
I have to mill some reeded moulding 4 3/8" wide and at the top end I need to mill off the reeds down to create a flat face to mount an acanthis leaf onlay. The best way to do this seems to me to plunge the face of the moulding into a straight knife shaper head. I have never plunge cut on the face of a board before so I am looking for input on the safest way to do this. How do I support the work piece so the shaper doesn't shoot the moulding across the room, should I attach the moulding to a backer etc. Any advice will be greatly appreciated.

10/3/19       #2: Plunging a moulding face into a sha ...
TonyF

KCR:

I don't think I would try it that way. Something you might try is to bring the reeding cutter through a scrap fence on the shaper, so that the scrap board creates a chipbreaker for the molding.

Using a powerfeeder, run the molding as you would any molding, then before you get to the end, stop the feeder first, then turn the shaper off. Give yourself extra length so that you can cut both the flat and the reeds to the correct size.

If the reeding has flats on both edges, you could also run the reeding, rip off the flats to either side, cut the end and attach the flat for the carving block, and then attach flats that extend the entire length. This would end the reeding abruptly at the carving block face, rather that have the reeding curve up to a flat.

I must confess that in 42 years I have never seen the reeding curve up to a flat as a pilaster design feature.

Your mileage may vary, and others may disagree with these methods. Hope this helps.

TonyF

10/3/19       #3: Plunging a moulding face into a sha ...
KCR

I never gave thought to stopping the reeding instead of milling it off but I do think I like the idea. I'm milling in Cherry so it will be a challenge to stop without burning at the stop end of the reeds but I'm using a new set of cutters so it may just cut clean for the few I am cutting. Great Idea Tony, thanks!

10/3/19       #4: Plunging a moulding face into a sha ...
Leo G Member

At a shop I worked at long ago they had a 9 bead cutterhead that they put in a shaper and did a stop reed for pilasters. The plunge was only about 5/32" deep because the bead was 5/16".

They had stop lines on the fence and the board to be run and they would just plunge it and push and then stop and lift. They use to screw a board on each end to use as a handle.

10/3/19       #5: Plunging a moulding face into a sha ...
KCR

This process scares me a little but you also make a good point Leo in that the actual load on the cutters is minimal because there just isn't a lot of knife in the wood. Now not as scary to me trying to plunge in. But still, if I have to hand feed the plunge, should I use a stop on the infeed fence to support the work piece during the initial plunge?

10/3/19       #6: Plunging a moulding face into a sha ...
Larry Schweitzer Member

This is a risky operation. I too would use a stop block for the initial plunge so it couldn't get away from you. This probably means extending the fence to be long enough. Cherry will be a challenge to prevent burning, be fast but careful. Adding hand holds to the back of the work seems like a good idea also. Will make it easier to be fast enough to keep from burning.

10/4/19       #7: Plunging a moulding face into a sha ...
Adam

In the past I would have thought about doing this on the shaper if we had a pile to do.

The router is the obvious choice for less than a pile.

If I had a pile I would either do it on my own cnc or sub it out to another shop with a cnc.

We’ve done a bunch on our Woodmaster. Those were tapered.

The quantity of a pile is determined by oneself.

10/19/19       #8: Plunging a moulding face into a sha ...
Jeff Duncan

Late to the party, but figured I'd throw this out if it may help anyone else.

When I do fluted work it's almost always going to be a stopped cut, and it's almost always going to be a rounded v-shape as I don't like the all to common half round shape.

So how to run them.... actually very easy. I set up in-feed and out-feed tables for my shaper.... useful for many other tasks BTW. Then I clamp start and stop blocks to the tables. This allows me to very safely feed the blank into the knives. It cannot kick back as the stop block is there and it also ensures each groove is in exactly the same place.

good luck,
JeffD

10/21/19       #9: Plunging a moulding face into a sha ...
David R Sochar Member

FWIW, the rounded ends of flutes or reeds is considered more desirable than 'points'. The rounded ends must be carved, requiring more time and more skill.

I mention this even though most readers will see the rounded ends not as more desirable, but more work, and therefore rule them out. 'Less work is better' has become the mantra. Between outsourcing and omitting details like carved reed ends, we wonder why the craft appears to be diminishing. The wood industry as a whole, and the architectural producers specifically really do a terrible job of marketing. We spend most of out time trying to make it cheaper to sell it, no time is spent on making it better by using better methods.

Rant over.

10/21/19       #10: Plunging a moulding face into a sha ...
Leo G Member

I've never carved out the box core bit flutes at the stop end. If they burn I will use a rounded scraper to clean them up and then sand them a bit.

I hate through flutes, looks cheap.

With reeds I will make a length and round over the ends and then round over the edge and slice them off so the ends are finished.

10/21/19       #11: Plunging a moulding face into a sha ...
Jeff Duncan

Hey David, I'm not sure I've ever seen a carved rounded flute end? If your using a half round bit to run them, (as seemingly most do), the end is already round... so I'm sure your describing something else. On the reeds I get it. I'd have to see a pic to get on the same page I think.

The v- style, (well actually more a spade shape I guess), grooves are pretty rare in modern work that I've seen. Possibly b/c no-one makes a cutter for them? I ground my own to match a set from an early 20th century piece, as I don't like the typical half round grooves prevalent in modern work. And b/c I run them in a decent sized head the ramps are perfect..... to my eye at least.

JeffD

10/21/19       #12: Plunging a moulding face into a sha ...
Pat Gilbert

I'm missing something, why would you even consider doing them on anything but a cnc?

10/22/19       #13: Plunging a moulding face into a sha ...
KCR

I am making reeded moulding not fluted but that's beside the point, Pat, I don't have a CNC. I have routers and shapers.

10/22/19       #14: Plunging a moulding face into a sha ...
Pat Gilbert

Fair enough, that would be tough to do without burning


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello