Gluing face frames

10/30/19       
Pinetree

I have always put my face frames on to the carcass with some kind of spline ,biscuit and or pocket screws. The place I am at now they attach the frames with just glue and clamps to the carcass and just glue to the stile and rail. Does anyone else use this technique and if so have had any trouble with it.

10/30/19       #2: Gluing face frames ...
DJS

We've been gluing and clamping faceframes onto our 3/4" boxes for with no additional splines or biscuits for 25 years and have never had a failure. And if a mistake is made and the faceframe needs to come off after 24 hours forget it, just start over. Splines and biscuits are unnecessary.

10/30/19       #3: Gluing face frames ...
Mark B Member

Same here. Only difference is we opt for pocket screws rather than waiting on clamp time. A shop we cut for has been gluing and clamping for 25 years or more as well with zero issues.

I could see biscuits/splines/dado being helpful with registration or making for idiot proof assembly but zero need from a quality/structural standpoint for me.

10/30/19       #4: Gluing face frames ...
Leo G Member

Glue only here too. On occasion I'll use a biscuit or three for lining something up. Usually when the FF needs to be attached in the field.

10/31/19       #5: Gluing face frames ...
SteveL Member

Just Glue. As mentioned above frames are impossible to get off after the glue sets. I have considered dados for speeding up assembly and consistent reveals but its not needed for strength.

10/31/19       #6: Gluing face frames ...
Matt Calnen

Did I understand you correctly that before the faceframe is put on, it is just glued together with a plain butt joint? That would be the biggest area of concern for me. At the minimum pocket screws should be used there.

10/31/19       #7: Gluing face frames ...
Leo G Member

The cured glue joint is stronger than the wood. Only thing biscuits, dadoes do are alignment. It might be stronger, but who cares when it destroys the wood taking it apart?

10/31/19       #8: Gluing face frames ...
DJS

Matt,

I was talking strictly about the faceframe attached to the cabinet. The joints of the faceframe itself are glued and pocket screwed, in our case.

DJS

10/31/19       #9: Gluing face frames ...
Guinea Member

Glue and pocket screws. Clamps in situations where the pocket holes would be a cosmetic issue. Since we finish prior to assembly, non-marring blocks or pads are used where the clamps are necessary.

10/31/19       #10: Gluing face frames ...
aj

Switched to Lamello Zeta a couple years ago - amazing system, makes finishing and install a breeze

10/31/19       #11: Gluing face frames ...
Adam

Guinea described our method word-for-word.

11/1/19       #12: Gluing face frames ...
Chris H.

Website: https://www.csaw.com/lamello/

To build a little upon AJ's success with using the Zeta P2 machine/P-System for attaching face frames, here are a couple of Instagram posts of other customers who have used it for the same application:

https://www.instagram.com/p/BzJp8gThBFk/

https://www.instagram.
com/p/B1XPomrgXqI/

Lamello Tenso P-14 connector

12/9/19       #13: Gluing face frames ...
JeffM

Just screws...no glue! No mess, no clamps...on to the next box.

12/9/19       #14: Gluing face frames ...
Leo G Member

And cracked paint in your future.

12/9/19       #15: Gluing face frames ...
JeffM

All stain. What would cause paint to crack on FF's if not glued?? I don't do much paint at all, but have never had a problem. I always put a separation joint from frame to case side if that's what you're talking about.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello