Have any of you ever experimented with a slight chamfer style relief cut around your dowel hole end drilling to get a tighter joint? When the units are in the case clamp, everything looks tight but when they come out, I'm occasionally getting some very slight gaping that probably most wouldn't notice - but I do and it's bothering me. Or, is this indicative of another issue I'm not seeing here? Thanks for the help!

1/13/20       #2: Slight relief around dowel drilling ...
Nathan W Member

Hi Stewart,

It could be a number of things causing your gap. I would look at your hole depths, you neet a little bit of room, about 1mm, of clearence at the bottom of your hole. This leaves room of a bit of extra glue to go. You also need to ensure that there isnt to much glue that your extra depth cant handle. You could also be seeing your scoring if parts a being flipped over. Another thing our guys do is run the air gun across the joints after they are put in the clamp, but before they are squeezed, just to blow any dust or junk out of the joint. Also be sure to blow your holes out before applying glue at the assembly bench.

1/13/20       #3: Slight relief around dowel drilling ...
Matt

We don't use dowels and case clamps for assembly so I cannot speak from firsthand experience, but I can appreciate what you're talking about.

I know that the Grass Ecopress machine uses 10mm forstner style bits with a relief chamfer, but I'm not sure if that bit has the right geometry for your situation.... especially the depth, you have to stop the hole at something like 12mm deep to get the chamfer right.

But it does basically what you're fighting-- helps prevent wood from pooching out when the dowel gets inserted, and also helps center the dowel at assembly which makes life easier.

1/13/20       #4: Slight relief around dowel drilling ...
Matt

And the Ecopress I'm talking about is for drilling the backside of drawer fronts for drawer systems like Zargen, just for clarity. So definitely not the same machine you're doweling with, but perhaps they off the bits you'd need to get that chamfer.

1/13/20       #5: Slight relief around dowel drilling ...
Stewart Member

Thanks for the responses! I do allow a 2mm gap on each end of the dowel for excess glue/water and we use our blow nozzles religiously to clear debris from the holes and joints. I might try slightly turning down the glue dose to see if that does anything but I'm really thinking it has more to do with the edge itself. The machine shoots water into the end holes before firing the dowels and I have noticed that, when using plywood, I get several drips to come out each hole after the dowel is inserted. This doesn't seem to be as much of an issue with the particle board core products. I'm wondering if that extra water is causing some slight swelling and making my plywood joints not quite as tight.

1/14/20       #6: Slight relief around dowel drilling ...
Nathan W Member

I find plywood to not perform aswell as, say particle or mdf core materials, I find that the water runs out of holes in plywood as well. In my experience plywood cases never keep joints tight as well as other materials. Ive never figured out why, justdoent seem to hold the dowel as well. We only use ply construction if absolutly need, or if a customer is dead set on it, the quality and consistency just isnt there, and its a pain to work with warped panels and panel thickness variations, thats a different topic all together. Anyways back on topic, if using plywood i would double check the hole depth in the gable, if your programs are set to 19mm and you panels come in thin, I've seen import plywood sold as 3/4" come in at 17mm, your holes may be shollow. Having said that, more often than not, regardless of how tight the joint is in the clamp, plywood cases do open up a bit for us as well. We have yet to find a solution.

1/14/20       #7: Slight relief around dowel drilling ...
Bruce H

I am guessing you are using an 8mm dowel. You can get a countersink for your bit, I uses a set screw so can be adjusted to provide a small or large sink. Most euro bit suppliers will have a sink. I am using one when I drill HPL doors as it helps with the ram in hinge.

1/14/20       #8: Slight relief around dowel drilling ...
Derrek

Anybody have a source for the grass ecopress 10mm bit with the countersink on it? I can’t find anything online for it but I have been looking for that. We put thousands of rafix fittings in and have a 20mm with a slight countersink and it goes in so much smoother. Would like a 10 set up same way

1/14/20       #9: Slight relief around dowel drilling ...
Stewart Member

Nathan, I'm glad to hear I'm not the only one with this issue - not that I would wish an "issue" on anyone else but it does mess with you when you have chewed on it for a while and can't seem to figure out where it's coming from. The dowel protrusion to depth of hole is just fine. I'm thinking for my plywood projects, I will dial the water dosage back and see if I can find an 8mm bit with a slight countersink to relieve any inconsistency right at the joint. Other than that, the only thing I can conclude is there must be a little amount of natural "springback" once the plywood case comes out of the clamp. Again, joints look great in the clamp and then occasionally gap once the pressure is off. Cases are left in the clamp for about 5 minutes.

1/15/20       #10: Slight relief around dowel drilling ...
Alan F.

I don't think 5 minutes is long enough for the glue to set.

1/16/20       #11: Slight relief around dowel drilling ...
Stewart Member

5 minutes actually works really well in most cases, but just for grins, I've tried up to half an hour to see if I could achieve a tighter joint. It doesn't make a difference at all. The "springback" is still there.

1/16/20       #12: Slight relief around dowel drilling ...
cabinetmaker

if you are having a problem with plywood, then check the thickness and depth you are boring into an end, meaning that you accommodating for its actual thickness. IT could be 18.5 and melamine is 19.3

1/17/20       #13: Slight relief around dowel drilling ...
Stewart Member

Thanks, cabinetmaker! I have checked and double checked to make sure I wasn't missing anything. I actually have my boring set up for an 18 mm panel since that is the thinnest we would work with. So, anything thicker obviously isn't a problem and if, by chance, the panel was a scant 18, then I have a 2 mm gap programmed on each end of the dowel to accommodate any further variations.

1/20/20       #14: Slight relief around dowel drilling ...
Matt

Derrek, you asked where to get the Ecopress bit, we buy them from True32.com

10mm Dowel bit with countersink


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!