floating panel paint issue

11/12/19       
frank Member

really trying to improve finish and i'm wondering if my door making is a problem.

paint grade shaker mold, flat panel (1/4" mdf)

complaints are the area where the panel insets in to the shaker mold ; paint pools up and bubbles, or when panel shifts you see cracking.

my question is; outside of trying to reduce the millage of top coat..is there a better way to make the door? for instance making the channel in the shaker mold wider, sloped, etc?

i do think doing that would simply let the paint pool in the area easier...

anyone have this floating panel and paint issue? how did you solve it?

much thanks in advance.


View higher quality, full size image (640 X 480)

11/13/19       #3: floating panel paint issue ...
Matt Calnen

How about a picture with out paint, so we can see your profile and tolerances. Why does your panel shift if it is made of mdf? Whether you glue the panel in, or use space balls, the panel should not shift enough to be noticeable. What kind of paint are you using?

11/13/19       #4: floating panel paint issue ...
Kevin Dunphy

Caulking and Caulking its that simple there a but its a skill to do it and leave no lines so pratice with a rag and a bucket of water.

I found out by trail and eror use 1/2 mdf for panel with water base primer swells up a little for a tight fit .The 1/2 also makes the door feel heavier

11/13/19       #5: floating panel paint issue ...
Frank

thanks for responses...the issue is that the paint "pools" in the slot area , then if the float panel moves even a little you get that pooled solid paint to crack.

i'm considering 1mm less thick MDF, painting with less mills for top coat (the primer is so good its hard to tell the difference from top coat)

finish used is Sherwin waterborne primer and top coat

but currently i'm very stumped and want this solved as i fear call backs building.

see attached


View higher quality, full size image (791 X 927)


View higher quality, full size image (803 X 755)

11/13/19       #6: floating panel paint issue ...
Matt

You need to put a backbevel on your stiles and rails (along the inner bead, where the panel is dadoed into the stile/rail) instead of leaving that corner sharp.

There shouldn't be a sharp corner where the panel fits into the dado. Put a backbevel on both long edges of that dado (front and back of the door).

This puts a visible, but intentional and elegant visible gap between the panel and the stile/rail.

When painting, be sure to shoot some paint up underneath that backbevel. Tricky if you aren't familiar with how to do it, but easy to do once you get used to it.

Also, you appear to be allowing way too much paint to be laid down.

Caulking in the panel might sound like a good idea, and it might work once in a while, but eventually wood movement will tear that caulk just like it can tear a paint layer. Also, it's way the hell more work than just doing a backbevel.

11/13/19       #7: floating panel paint issue ...
Adam

Our shaker doors are 3/4” soft maple. 3/8” mdf. The edges are perfectly square made with a typical Freeborn shaper set. The fit is tight. Typical .002”. We glue the mdf panels into the frames. We’ve never caulked in 30yrs. They don’t crack or move. We finish in both solvent and wb. It makes no difference.

11/14/19       #8: floating panel paint issue ...
Ken Member

Hey Kevin, "I found out by trail and eror use 1/2 mdf for panel", are you just rabbeting in the panel? Are you using a 3/4" frame or thicker?

11/14/19       #9: floating panel paint issue ...
Matt Calnen

Matt, this is Matt:) It looks to me that he has a back bevel on his sticking profile. I do mine similar to Adam’s, but i have moved to 1/4” panels as i have found them to be a perfect fit in my Freeborn Groove. I have never liked the backbevel or under cut, I feel it looks to factory made. I agree it looks like a way to heavy finish coat.

11/15/19       #10: floating panel paint issue ...
frank Member

thanks guys for response so far.

main question again is the "pooling" of the paint where the panel and framing meet up.

putting glue in the channel though imo is odd as it defeats the float. i do understand mdf does not expand (in theory) but will avoid that move. (we have been at this 47 yrs)

i'm just reviewing every process we do currently.

for now i think the beveling of the frame as Matt suggested is in play..and already pushing my spray guys to pop on less top coat mills.

11/15/19       #11: floating panel paint issue ...
Adam

We use 10mm mdf or 1/2” wood veneer for the weight. 1/4” always seem a little light especially when compared to a raised panel door.

After looking at your pic, I believe the primary issue is your profile. The groove edges have a serious radius. The paint will try to puddle in that gap. In some places it will bridge, in other places it will not and leave little voids like your pic.

All of our door cutters have sharp/square groove cutters. Some of the sets have a slight eased edge on the outside of the profile, but not the groove.

11/16/19       #12: floating panel paint issue ...
Harold

Website: http://morantzcsninets.com

One piece mdf is only way to go. No joints and if primed and painted properly you can put them
In a bucket of water and nothing swells.


View higher quality, full size image (3308 X 2481)

11/17/19       #13: floating panel paint issue ...
Steve Member

Seems to me your first call should be to Sherwin's technical support, dealer can put you in touch. No offense intended to to other respondents here.

5/8/20       #14: floating panel paint issue ...
Al Gerhart Member

What is your paint? Lacquer? Been doing paint grade doors for years and never seen that kind of build up.

Spray two coats, sand between coats, laid flat so you have to spray four times. Same Freeborn cope and stick cutters as the others have talked about, either 1/4" veneered MDF or just plain 1/4" MDF center panels or RP.

5/9/20       #15: floating panel paint issue ...
Steve Member

If the panel leaves a space, in my opinion it should be pressed to the front face leaving any gap in the rear. Squirt a dot of hot glue in the gap to hold the panel forward if you can't get the proper snug fit in the first place. Do not caulk.

Any talk of puddling and cracking to my thought is simply excess paint volume. And, I'm with Steve - the other Steve :) - first call to Sherwin tech support, no offense to anyone here.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!