6/28/20       
ennisdavis Member

Is it possible to remove plastic laminate from existing particle board cabinet doors without destroying them. Most cabinet shops never do this, they just use new MDF. Dont want to laminate over the old stuff either.

6/28/20       #2: resurfacing cabinet doors ...
rich c.

Particleboard is dead cheap. Why waste labor? The customer will appreciate the smaller bill of starting with new sheet stock.

6/29/20       #3: resurfacing cabinet doors ...
Mark B Member

You can strip off the laminate with acetone but as rich says, seems a lot of work. Assuming your trying to just replace the outer face and edges but....

6/29/20       #4: resurfacing cabinet doors ...
Leo G Member

MEK (Methyl Ethyl Keytone) is better than Acetone. Wear protection.

6/29/20       #5: resurfacing cabinet doors ...
Mark

If you're doing one or two maybe.
Still easier to just cut new door blanks.

6/29/20       #6: resurfacing cabinet doors ...
Scott

We always used lacquer thinner for removing plam, it was mainly used when a mistake was made on plam projects. The glue we used was 3m water base, so the lacquer thinner worked really well, but it still left a lot of the softened glue on the work piece, which was a lot of work to clean up. I am not sure how it would work on older solvent based contact cement that has been sitting for a long time.

The guys in this forum like Rich and Mark have given you some excellent advice, it will be a lot cheaper to buy and cut new cores then to remove the laminate and clean the old ones.

6/29/20       #7: resurfacing cabinet doors ...
pat gilbert

Another vote for buying new PB.

If you use solvent to take off existing laminate there is a good chance that the solvent will wick back out delaminating the new laminate.

6/29/20       #8: resurfacing cabinet doors ...
MarkB Member

Stripping the laminate off sucks period but its not uncommon (of course always avoided) to remove a bad/broken with solvent. All solvent sucks, but MEK as Leo mentions, or Acetone, will not be there for long. They will be gone in no time. I avoid the MEK, not that the Acetone is any healthier. Lacquer Thinner is too slow and definitely does leave a bit of residue behind.

I cant imagine stripping a face and edges off a set of doors and fronts that way, but..

6/29/20       #9: resurfacing cabinet doors ...
ennisdavis Member

Wont the solvents get into the wood and cause warping or other problems. These doors are wide and I am not setup for a sled on my table saw. Some people laminate over laminating, how do you guys feel about that.

6/29/20       #10: resurfacing cabinet doors ...
Leo G Member

I feel it's going to make the door wider, taller and thicker.

6/29/20       #11: resurfacing cabinet doors ...
rich c.

Not sure what kind of professional shop you are running, but not even having a sled on a table saw must make profits really thin!

6/30/20       #12: resurfacing cabinet doors ...
scott brady

Save yourself the headache literally, order laid up panels for almost the same cost as your price of laminate and with a hard glue line. Cut , band, hinge and be on your way with no call backs on delaminating new plastic.

7/1/20       #13: resurfacing cabinet doors ...
Bruce H

getting laminate off doors will depend on what glue was used in the first place. Mine are cold pressed, it's not coming off with MEK or any other solvent. Unless you are a home owner doing it yourself with no time value the effort to remove laminate would far exceed new material.

7/1/20       #14: resurfacing cabinet doors ...
pat gilbert

One other thought

The cost of laminated sheets is usually less than if you buy the material loose.

7/1/20       #15: resurfacing cabinet doors ...
Jim Kolar

Yes you can but some skins will break free easy and some won't. If these are layed up panels with a press you won't get the laminate off.

7/2/20       #16: resurfacing cabinet doors ...
ennisdavis Member

I agree with you guys, new material for the doors but I really want to use 5/8" MDF and its impossible to get. For kitchen cabinet doors 1/2" wont cut it and 3/4" is too beefy.

7/2/20       #17: resurfacing cabinet doors ...
pat gilbert

I have found that although hard to do, the most efficient thing to do is Change Your Mind

7/2/20       #18: resurfacing cabinet doors ...
rich c.

Your industrial sheet goods supplier doesn't have 5/8? You need to find a new supplier!

7/3/20       #19: resurfacing cabinet doors ...
ennisdavis Member

I use a major US supplier, just the local one has a hard time getting 5/8" needs to be ordered.

7/3/20       #20: resurfacing cabinet doors ...
ennisdavis Member

Speaking of MDF, I have been reading about alot of people having screw pull out on hinges, they are using plastic dowels. Is this common.

7/3/20       #21: resurfacing cabinet doors ...
Alan F.

Use 11/16" core, VG laminate with CL or VG back and you get a slightly less than 3/4" thick panel.

If you want to re-laminate in the field use something like Wilsonart Recover, it is peel and stick and designed for re-laminating in the field

WILSONART® RE-COVER™

7/5/20       #22: resurfacing cabinet doors ...
Scott

Why do you want to use mdf? I would use particle board, it is way cheaper, lighter, adhesive sticks to it better and like others said use the inserts with your hinges. You can get a pb core that is around 11/16 thick, works wonderful for laminate and veneers.

What kind of edgebander do you have?
The production shops glue up sheets , cut it and then run it through the edgebander.
You need a decent edgebander for this process. If you are only doing a few jobs like this or don’t have a good edgebander I would Edge the presized panels first and then glue the faces. It is a lot more labour , but if you are using a laminate trimmer it is way easier to get a good job this way.

7/6/20       #23: resurfacing cabinet doors ...
ennisdavis Member

MDF is more stable due to the resin content, flatter and more water resistant then PB. The edges on PB is lousy, porous and rough. $19 for a 4x8 sheet of MDF 5/8, can you get cheaper then that?

7/6/20       #24: resurfacing cabinet doors ...
rich c.

In reply 16 you said 5/8 MDF was impossible to get. Now you are shopping for price? What gives? Seems like you would be thrilled you found it at that price!

7/7/20       #25: resurfacing cabinet doors ...
ennisdavis

It was a figure of speech. I can order it, not that convenient. It is a great price.

7/11/20       #26: resurfacing cabinet doors ...
Jeff

With your comments about mdf vs pb it is obvious you are new in the game of plastic laminate work.

With all your comments it sounds like you are just building this for your garage or basement storage room, so I guess it doesn’t matter what you use.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!