We don't do a lot of melamine work but occasionally run into a project that requires it. No cnc in shop so it gets broke down and cut on table saw and slider. In the past we had decent luck controlling chip out using a melamine blade with a zero clearance insert on saws but the last job we did it didn't do a very good job. Almost seemed like the melamine was thinner coating than ever before. Am I imagining things here or have others seen this too? Our slider has a scoring blade but the motor went and its an older model, no longer available so was hoping for a better solution. Maybe I can get it rebuilt at a motor shop.
If that doesn't pan out, I had thought about oversizing and trimming cuts with a carbide cutter on a shaper, maybe 1/16". Any other ideas other than outsourcing? If we did lots of it I'd get an edgbander that also did this but not for a once in a blue moon project.

2/27/20       #2: Melamine question ...
Jared E

If it's not a lot of parts, a good track saw might do a better job than your table saw if you can't get your scoring blade working. I have a Festool and its guide rail prevents chipout pretty well.

2/27/20       #3: Melamine question ...
John B Member

Jared, yeah, for just a few pieces that could work. I've done it before, but not practical for the number of parts usually. We have a Festool 75 and it does work fairly well although mine is ready to have the edge strip replaced. Im also wondering if and brands of melamine seem to have thicker coatings. This last batch chipped on edges just handling it. Not sure of brand off hand, but got it through Atlantic Plywood.

2/27/20       #4: Melamine question ...
MarkB Member

We have a lot of issues with commodity melamine even with CNC. Parts through the bander, on and on. The standard stuff can be super fragile.

I would suggest at least trying if possible to change your melamine supplier and get a better product. A few dollars a sheet will be far cheaper than any re-tooling option based on what youve said about your capacity. Moving from 23$ a sheet to 40$ a sheet material would be money in the bank compared to re-tooling your saw, slider/blades, and so on.

If it was getting you by before something has changed and thats likely the material. Deal with that first and spend your money on tooling later. Sounds like melamine/laminate may not be the strong suit for your capacity but we all do what we have to when jobs land.

2/27/20       #5: Melamine question ...
Jim Member

We have much better luck with mdf core melamine.

2/28/20       #6: Melamine question ...
Thomas Gardiner

I cut melamine with a high ATB blade and mostly avoid using my scoring unit. I have found that a sharpening lasts about 30 sheets. The other thing is the quality of cut is affected by the height of the blade. Lower the blade to improve the bottom edge. Raise the blade if you start to get chips on the top. No zero clearance required.
And yes, try a different board some are way better than others.

2/28/20       #7: Melamine question ...
dan summerhill Member

Has there been a drastic temperature change where you are? We had a huge problem when we were setting up our panel saw. It was a hot, humid summer and no blade we tried would get a clean cut. Turns out, the delivery truck was cooking the melamine. The warehouse was humid so the core picked up water, the truck heated it up and our saw was making it explode. At least we got a bunch of Greenlee blades out of it.

2/28/20       #8: Melamine question ...
Scott

My recommendation would be to get a used motor or the one you have rebuilt and use your scoring blade. The second option would be to get a blade designed for cutting melamine, it will give you a good quality cut on the underside . Make sure your blades are sharp as dull blades will give a very poor result.

I cut jobs for years on a sliding table saw with great quality blades, the edges come out nicer and you have less tear out than a cnc. The other nice thing is you can cut a job fairly quickly with a little practice and organization.

The last option would be sub it out.

In my opinion a track saw and cutting bigger and running through a shaper are last resorts as there will be huge labour costs involved with these slow and inaccurate methods.

2/29/20       #9: Melamine question ...
Oggie Member

Use appropriate blades. I use Diablo D1296L blades for double sided melamine. There are also 10" versions. Lasts about 15-20 sheets, before it needs to be resharpened. New blade from store cuts best. Sharpening company that I use is not doing great job (although they are certified Freud sharpeners recommended at Freud website) because my blades start to vibrate after they sharpen them, and then they vibrate more and more with each additional resharpening. Blade vibration is not good for chipping.
I also use blade disk stabilizer, seems to help.

I get best results when my 12" blade sticks around 1-3/4" above table saw surface (about 1-1/2" for a 10" blade). A little bit higher and I start getting chipping on the bottom side, a little bit lower and chipping starts to occur on the top side.
Bottom side is a lot more sensitive to chipping then top side.

I always buy same types of melamine from same two suppliers and sometimes top and bottom cuts are perfect and indistinguishable from each other, one would need strong magnifying glass to find out which one was top and which one was bottom, other times bottom one visibly chips no matter what.

Sometimes, the sound of blade cutting through the sheet is uniform and mellow, and I know that there would be no chipping at the bottom, other times I hear cracks and snaps that sound like the blade teeth are hitting some hard particles inside the melamine board (like small stones) and than chipping occurs.
If the blade is not very sharp, slower feed speed may help.

I never have problems with top side, it's always the bottom one.
Here are few tricks that could help:

1. I always cut most important parts first, like doors and drawer fronts, when the blade is still very sharp and produces good results on both sides of the cut.

2. Most other parts, like case parts, have only one cut that really matters, and that is the one on the front side of the cabinet. Other cuts are usually not visible from both sides when the cabinets is assembled, and the one that is can be the top side cut, which usually has no chipping.
So, when cutting front side cut, lower you blade to, let's say 1/8", and use it as a scoring blade. Once the piece is scored on one side, rise the blade, turn over the piece and make final cut.

3. If even the new blade would not give you good cuts on bottom side, cut parts oversized (e.g. add 1/2") and use scoring technique from No. 2 for final cuts that will bring the piece to it's final size.
That would be wasting of time for everyday operations, but if it's something that you do once in a blue moon, could actually work.
3. Some people claim they avoid chipping by gluing the painter's tape along the cut area before cutting. Never tried that.

Sometimes, when my newly sharpened blade accidentally cuts through 16GA or 18GA nail or staple it starts making better cuts than before the accident.

Anyway, I would try to repair the scoring blade function if possible. It can lower your stress level significantly by releasing you from dealing with all that "black magic" mentioned above, which I had to endure for 2 years.

2/29/20       #10: Melamine question ...
bob

solid carbide knives in your joiner
thats how we handle smaller pieces
i do not allow cuts less than 12" on the slider
1/32" pass should clean your chips

2/29/20       #11: Melamine question ...
Paul Miller

Website: http://MCCWOODWORKING.COM

Getting your electric motor rebuilt should not be a problem. Plenty of electric shops can do that.

When I first started to cut melamine, I did not have a scoring blade and chipping was a problem. To avoid this, I would cut the panel twice, with the first cut going a little more than 1/2 way through and then to flip it over and cut it again. The chipping is caused by the hard melamine blowing out the bottom side. Obviously, you have to lower your blade to about 7/16" for 3/4" board. Also, not all parts need to be chip free. Sides that go up against other sides do not need to be chip free and neither do tops that face up.

3/14/20       #12: Melamine question ...
John B Member

Thanks for all of the input. I have been using Freud, CMT, and Tenryu blades that are made for melamine cuts, all of which did good work until the last couple jobs. Blades were new and still had problems so leads me to believe this is more material related. What better brands of melamine has anyone had good luck with? My main suppliers are Atlantic Plywood and Richelieu. I will check with their sales guys too but input from here would help. Thanks again.

8/5/20       #13: Melamine question ...
D Conti

different melamine has different thickness paper on the them. The thicker the paper the less chipping but also the higher cost. Trying to cut melamine without chipping requires a machine that is designed for that, either a cnc router, high quality slider or a beam saw,


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!