Ok, here's my problem. I'm a woodworker with many years experience making custom furniture. I've taken a job for a whole house of cabinets. I've already completed the vanities, utility cabinets, etc. The plans call for floor to ceiling cabinets across a whole wall, no counter top, just cabinets and a refrigerator. and they are the FULL DEPT OF THE FRIDGE (approx 28" deep), (see pic I made from Cabinet Planner software, which may not be the final design). The wall is 156" (13 ft) by 10 ft. tall.

So, how do you join the faceframes for a seamless (or near seamless) monolith look. I plan to spray all cabinets with a pigmented catalyzed lacquer, so I prefer to do it all in the shop.

Some specific questions:
- do you use narrow FF at the joints?
- do you ease the edge (slight grove) at the joints rather than trying to hide them.
- how would you build the boxes, i.e., I was thinking about 4 tall vertical cabinets 28"-30" wide and one over the fridge, (30" x 115" x 28" deep would be some large cumbersome cabinets to build, finish, haul, and install) or how could I make multiple stacked boxes, etc.,

I'd appreciate any help I can get, and especially like to see pictures of your work for similar projects, and some close ups of joints.

Many thanks,
Dave B.


View higher quality, full size image (2016 X 1512)

9/22/20       #2: Floor to Ceiling Wall of Cabinets ...
mike  Member

Website: http://distinctivekb.net

i'll be the 1st to respond and just say that one option is to screw the cabinets together in the shop (laying on their back )before finishing, sand the face frames then finish as usual. When you go to install you will have perfectly mating face frames and predrilled screws to speed work on the jobsite. Also if you use full overlay doors you could keep close consistent gaps between doors thus hiding the joint. just make sure you use the right hinges that open within themselves.

9/22/20       #3: Floor to Ceiling Wall of Cabinets ...
Kip

For many years I tried to hide all joints. But for the last few years I have started easing the edges to create a very shallow line between joined cabinets. It’s actually a nice look

9/23/20       #4: Floor to Ceiling Wall of Cabinets ...
Leo G Member

Make cabinets 6, 13, 1 a single cabinet

Same with 7, 5, 12

8,10.14

9, 11, 15

Then you can just stack them with a horizontal line to deal with. Cover it with a bead or nothing. Same with the other cabinets.

9/23/20       #5: Floor to Ceiling Wall of Cabinets ...
Tom Gafgen

Why not build them frameless and just stack boxes ? That way there's no face frame seam deal with .

9/23/20       #8: Floor to Ceiling Wall of Cabinets ...
Chris H.

Website: https://www.csaw.com/lamello/p-system/lamello-tens...

Just thought I'd throw this out there for consideration: One of the main applications for our Lamello P-System connectors (and specifically the Tenso P-14 with pre-load clips) is for flat-finished, flat-packed, site-installed, monolithic face frame construction. One of our customers says it best in the video below, but call me at 781.585.4364 x.206 to discuss further if you'd like. Colonial Saw is the US importer and master distributor of Lamello.

Lamello on Instagram

9/23/20       #9: Floor to Ceiling Wall of Cabinets ...
Tom Gardiner

First of all I would build the cabinets 24" deep because any deeper is impractical storage. I would build beams of plywood 4 x 4" section and screw to the wall to mount the cabinets to.
I would raise the upper cabinet line to the height of the fridge opening to achieve a consistent horizontal line. If you are concerned with a seam being visible you could add a bead at that horizontal to hide it such as a bead.
You would end up with four face frames applied onsite - upper and lower bank of 3 x 2 cabinets to the right , 2 x 2 cabinets above and left of fridge and two lower cabinets to left.

9/23/20       #10: Floor to Ceiling Wall of Cabinets ...
Ryan

If you normally use 1.5" stiles uses 3/4" where that come together so all door revels are the same. Hiding joints is not a huge deal most people will never notice.

9/23/20       #11: Floor to Ceiling Wall of Cabinets ...
Oggie Member

Even if you need face-frame look, I would build frameless cabinets with oversized doors that protrude beyond edges of the cabinets (not a problem for upper and lower edge, and I think hinges exist for more than full overlay), and then I would put horizontal and vertical beams between cabinets during the installation.
That way, doors would cover seams between cabinets and beams, and the only seams visible would be short lines where vertical beams meet horizontal ones, provided that the horizontal ones run in one piece all the way from left to right.

See the quick sketch on pictures bellow for details (I omitted vertical beams for clarity).


View higher quality, full size image (2167 X 1352)


View higher quality, full size image (2167 X 1352)

9/23/20       #12: Floor to Ceiling Wall of Cabinets ...
Oggie Member

Also, I think the design would look nicer is all the upper cabinets have same height and if the fridge is in the middle, if possible.

9/23/20       #13: Floor to Ceiling Wall of Cabinets ...
D Brown

There are so many ways to do things, what I have done depending on design is to stagger the cabinet depths where they come together. Then wrap your crown molding around the face for a very nice look. Good luck

9/23/20       #14: Floor to Ceiling Wall of Cabinets ...
pat gilbert

What D Brown said

9/23/20       #15: Floor to Ceiling Wall of Cabinets ...
Adam

Follow Leo’s cabinet layout. It’s always easier to build long units vs tall.

Pack the wall out so you can use standard 24” deep cabs. It will save the customer $2k in plywood. They will barely use the 24” depth.

Two basic options with the face frames. Easy option is to frame each unit then add a little astragal trim piece. The harder option is to temporarily fix the cabinets together in the shop. Apply your face frames so that the upper units frame over laps the lower. You glue, screw or nail The frames on. Do not glue the overlapped joint or butts. Let it dry. Sand it all flat. Disassemble, paint install. If done properly this will look really good. We do this with bookcases all the time. Even beaded face frames.

9/23/20       #16: Floor to Ceiling Wall of Cabinets ...
Dave Baker  Member

Thank you all for time spent composing such thought provoking solutions. You guys are amazing, I always get great ideas from this forum.

Leo G. I think your idea for combining cabinets is spot on. Makes sense to me to build them horizontal rather than tall, as you and others have also suggested.

Good idea to raise the line of the second tier to be even with the fridge. I'll try to get the customer to live with the 24" cabinets, we'll see how that goes.

Tom Gardner, I'd love to see a pic. of the bead you you suggest, is it an integral bead routed on the FF, or applied?

Oggie, I think your on to something with the doors covering the seams, I just need to think through it some more.

Adam, I like your idea to let the FFs overlap, I'd love to see some pics. with details of how you do that.

Again, thank you all for your input.

Dave

9/23/20       #17: Floor to Ceiling Wall of Cabinets ...
Leo G Member

I think between my idea of long horizontal cabinets and Oggie's overlapping door idea would make the horizontal line between cabinets nearly invisible.

9/23/20       #18: Floor to Ceiling Wall of Cabinets ...
rich c.

First thing to talk to the customer about is a library ladder rail in there somewhere with a rolling ladder so they can even use the top cabinets. Second is make sure you don't make a full height cabinet, or you may not be able to pivot it up at the install without the corners of the cabinets getting stuck to the ceiling and floor. I usually do a ladder toe kit, so I can have shorter cabinets to tilt up and then slide onto the installed and leveled toe kick. Then add the crown.

9/24/20       #19: Floor to Ceiling Wall of Cabinets ...
Adam

I recommend that you buy the Builtin Furniture book. It’s got good ideas and plenty of pictures.

Don’t forget to keep the top rail a couple of inches lower than the ceiling. Let the crown cover the space. It makes it easier in the install and saves material. Likewise think about the edges if they need scribes.

As to materials. Avoid painting the boxes. Get yourself some prefinished maple plywood. Paint the frames seperately. Install them after building the boxes.

Painting boxes sucks, costs a ton of money, and is not as good as the uv ureathane.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors

    Become a Sponsor today!