We use 3/4" UV Ply for our cabinet boxes. We paint our face frames separately and attach them to the boxes with pocket screws. Our finish ends get screwed from inside the cabinet.

Our problem is the joint between the finished end and the face frame. On the rare occasion we do an unfinished set, it's easy. Everything gets secured and v-grooved or sanded flush.

How are you attaching finished ends to boxes and what are you doing where the finished end meets the face frame?

5/12/21       #2: Finished Ends on Prefinished Cabine ...
Jim Herron

Why not vee groove it as well?
Finish the end panel and end of the face frame, attach end panel, and done.

5/13/21       #4: Finished Ends on Prefinished Cabine ...
Guinea Member

We pre-finish and have the same issue as Kalvin; our solution has been to flush trim/v-groove the exposed end(s) post-assembly, but this requires respraying the trimmed FF edges. I like Jim's idea of pre-trimming/grooving, but it seems like even a little waviness in the panel could mess with the alignment, not sure.

5/14/21       #5: Finished Ends on Prefinished Cabine ...
Chris H.

Website: https://www.csaw.com/lamello/

Hi Kalvin,
You may want to check out the Lamello P-System. Installing face frames and finished end panels are two very common, successful applications for it. You can type in 'Lamello Zeta' here on Woodweb and see what other customers have said about it too. Reach out if you'd like to learn more.
Chris

Link to a related Instagram posts from other customers below, plus you can copy and paste these as well:

https://www.instagram.com/p/COmDxqbDevV/

https://www.instagram.com/p/C
I34ub6jEoS/

Link

5/15/21       #6: Finished Ends on Prefinished Cabine ...
Jeff

Make sure you are sitting down when you look at the Lamello, You get totally scammed when you buy the machine, and then you get scammed when you purchase the fasteners for it.
I hate companies like that. I will try 50 different things to make that end connection work before being ripped off.

5/16/21       #7: Finished Ends on Prefinished Cabine ...
cabinetmaker

We dado the back of our face frames 1/4 deep with 1/4 on the unfinished sides using 3/4” width.

On the finished end we dado a 1/2” with and rabbit 1/4 x 1/4 on the finished ends

This is all on 3/4” ply. We use uv for all parts and but one side coated or clear the inside of stained work.

We don’t dado shelf of deck pcs. Mainly pocket screw or staple with 5/8” x 5/8” cleat.

Good luck

5/21/21       #8: Finished Ends on Prefinished Cabine ...
Peter Rusterholz  Member

Jeff,
Using the Zeta would not necessary be my preferred method for this application but i definitely have to disagree with your
rather slanderous description of the Lamello Zeta tool and fasteners.
The machine has evolved into one of my most valuable assets at my shop.
Time saved utilizing the fasteners has compensated the relative expensive of them by multiples. Especially for clamp less field assembly of finished components
And no, I'm not associated with Colonial Saw in anyway.

5/21/21       #9: Finished Ends on Prefinished Cabine ...
Jeff

Peter,
In no way am I trying to slander the tool, I think it is a fantastic tool.
However the price is absolutely out of line, the company probably has a patent that is good for x amount of years and then other companies may try produce it. How can you justify charging $2500 for a glorified biscuit jointer? The company is just taking advantage of the consumer.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors

    Become a Sponsor today!