I tried to post this before, but my post seems to have disappeared. I apologize if this is a double post.

I need to edge band a small amount of walnut plywood on a regular basis, roughly 100 linear feet once a week. I've tried ironing on edge banding with pre applied adhesive, but the adhesive is white which makes the glue line very visible. The adhesive is also gummy which creates trimming issues.

Is there a better way to do this? A machine seems like more trouble than it's worth for the volume I am doing. Gluing the edgebanding with wood glue looks great but is labor intensive.

6/4/21       #2: Low volume edgebanding ...
Mark B Member

Im sure farming it out to a local shop would with a large bander in worthwhile lots would be a suggestion but perhaps no one in your area or you cant process larger runs and inventory.

Fast edge tape from fastcap is often mentioned but ive never been impressed with it.

You might do some calling around to varuous suplliers as i know ive seen preglued and even prefinished dark banding somewhere that called out dark glue but cant remember exactly where at the moment.

One other is you may try more heat and a hard steel roller with your current banding and a lot of roller pressure to tighten up your glue line.

6/4/21       #3: Low volume edgebanding ...
chris barnard

have you thought about a hand held bander like a festool conturo?

6/4/21       #4: Low volume edgebanding ...
Bill

Here is a second vote for a Festool bander. It is expensive for what it is but it does a good job and you can use it on curved work. If this project ever stops it is easily sold.

We have one mounted in a table for curved work.

6/4/21       #5: Low volume edgebanding ...
Derrek

Festool handhelds bander
5 minutes to warm up, run natural glue pucks, cut banding to length plus about 1’
Edgeband trim and put away. This is the best handheld bander out there

6/4/21       #6: Low volume edgebanding ...
Nick Member

Ok, thanks guys.

I will look for edgebanding with dark colored adhesive, this sounds like a good solution for the moment.

I will also consider the Festool. Are there any compact floor machines that would be a good alternative? I don't need the capability to do curves and I would prefer something that is easier to work on.

6/4/21       #7: Low volume edgebanding ...
Matt calnen

Edgeco is the company I get my preglued banding from, they have great service and will make whatever you need. I bought a used Virtex EB 25 for $1800 and has been great for my low volume needs.

6/4/21       #8: Low volume edgebanding ...
daniel

find someone in your area with a bander. should'nt cost that much if they would agree on you bringing in your parts and banding.

6/4/21       #9: Low volume edgebanding ...
rich c.

If I only needed 100' a week, I would rip 1/8" thick strips of solid walnut and glue it on. The you have a hardwood edge that is far superior to glue on edge banding. If you do that every week, I'd make up a glue up table for easy loading and clamping. Using Titebond, you only need to leave it in the clamps for 15 minutes. Don't machine it right away, but it's stuck really well in that time.

6/4/21       #10: Low volume edgebanding ...
Derrek

“I will also consider the Festool. Are there any compact floor machines that would be a good alternative? I don't need the capability to do curves and I would prefer something that is easier to work on.”

You can table top mount the festool. If your referring to maintenance, it’s basically maintenance free and you don’t have to work on it other than just a little clean up

6/5/21       #11: Low volume edgebanding ...
Nick Member

Matt, thank you, I will give edgeco a call.

Daniel, I live just outside of San Francisco where prices are off the charts insane. I no longer bother getting quotes for stuff like this.

Rich, I may end up doing 1/8th inch strips. I find solid wood easier to work with anyway.

Derrek, I'm sure the festool is fine, I just prefer simple things that appear to be made of off the shelf parts. Eg I have two laser cutters, one is a $10000 epilog laser and the other is a $1000 no name chinese laser. They both have problems but the Epilog laser has proprietary ($$$) parts.

6/6/21       #12: Low volume edgebanding ...
Kevin

Website: http://www.kdunphy

I do the same use 1/8 solid wood use a pin nailer to hold down you can't see the pins

I think iron edging doesn't stay very well on plywood .Also it look great

6/6/21       #13: Low volume edgebanding ...
Bill

Depending on the length of the parts you can use a heat bar to glue on strips. Is speeds that process but it is no where near as fast as edge banding.

6/6/21       #14: Low volume edgebanding ...
Chris Member

Nick, if you change your mind on the festool option I am over in the tri-valley if you want to come over and take a look at mine. I agree it’s not cheap but it’s been a good tool for the few years I have had it. I picked it up from festools refurbished sale a few years back.

6/29/21       #15: Low volume edgebanding ...
matt

We use the Festool Conturo at our shop, although we have a nice Brandt edgebander. We use the Conturo specifically for curved stuff.

However, the Conturo is a legitimately good piece of equipment.

There are some smaller dedicated EB machines that would probably suite you but most of them I'm aware of run preglued EB, so you're back to your issue with the glue color. I'm pretty sure you can get dark glue for the Conturo just fine.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!