7/1/21       
RODNEY BLACKERBY Member

Anyone have any experience with taping the end grain on solid wood? builder saying his painters never fill the endgrain good enough.

7/1/21       #2: shaker doors ...
Leo G Member

Should be easy to fill the end grain with a brush.

If they are spraying on site then they need to prime better or with a higher solids primer.

Orrrrr..... You need to sand the end grain of the doors better. I use an edge sander and that closes the grain very well.

What species wood are said Shaker doors?

7/1/21       #3: shaker doors ...
rich c.

Taping the end grain? You mean edgebanding? Why don't you just use some high fill primer on the top and bottom of the door and back charge the builder.

7/2/21       #4: shaker doors ...
Edi Silva  Member

Website: silvawoodworking.com

Edge sander while fitting the doors. Works very well with either Paint Grade or Stain Grade doors.

7/2/21       #5: shaker doors ...
RODNEY BLACKERBY Member

We use use a shelix head on shaper and then clean up on edgesander. one of the problem's is we are in texas very high humidity and we install the cabinet's and they are left sitting unfinished in the houses to long. we are using Beech lumber.

7/3/21       #6: shaker doors ...
Jim H

I'm in Texas.
Your builder needs a different painter if they're edge sanded.
Get them under a high solids primer at least until they paint.

7/4/21       #7: shaker doors ...
TonyF

Rodney:

Taping is a bad idea. It sounds more like a painter's problem than your problem, although the builder wants it to be someone else's problem other than his problem, which is why you are hearing about it at all.

If you need to do something about, you might consider a glue size on the end grain, letting it dry before final sanding. But this may come back to bite you if the paint doesn't stick.

Better to stand your ground and tell the builder that you are supplying cabinets sanded and ready to paint, and that painters are responsible for the finish quality after that.

That is the definition of finish-ready, which sounds as though that is the extent of your responsibility.

Unless you want to paint them. Or miter the corners of the doors for a small fee, which is also a bad idea. If you are living up to your contract, then your end is done.

TonyF

7/4/21       #8: shaker doors ...
Leo G Member

Slather the end grain with putty before you edge sand them. Best you can do for the builder until he gets painters that will take the time to do it correctly.

Mitered doors as Tony mentioned are another way to do it. I personally don't do mitered doors, only cope and stick.

7/6/21       #9: shaker doors ...
JR Rutter

Website: http://harmonicdesignworks.com

Is it the end grain porosity, or is it the cope/stick joint telegraphing through?

I only ask because you mention environmental factors and time delay before paint. The delay can definitely cause enough dimensional change in the rails to undo the nice flush edge from the sander.

7/7/21       #10: shaker doors ...
RODNEY BLACKERBY Member

cope and stick joint is the problem.

7/7/21       #11: shaker doors ...
Leo G Member

If the cope and stick joint is the "problem" then it's not a problem. It's what wood does. And there isn't a thing you can do about it if you continue to use that type of joint.

The only other option is a mitered door which has no end grain showing. They have their own issues of the miter opening up over time, but no end grain showing.

7/8/21       #12: shaker doors ...
David R Sochar Member

Bad idea on all counts. The builder's inability to control his painters is not your problem, tho he would like you to take it on for him.

Upgrade your end grain sanding so he has nothing for the painters to complain about.

In my experience, solving the builder's problems should happen with superior products and service. Not with gimmics and jimcrack.

7/9/21       #13: shaker doors ...
Scott

What kind of wood are you using? bamboo?
You sand a door on the edge sander like everyone has mentioned , your job is done. If the painter can’t make it look good after that, he needs a new painter.

I would tell him to get a bag of sand and a hammer, dump the sand on the ground and start pounding it.

7/9/21       #14: shaker doors ...
RODNEY BLACKERBY Member

We are using beech, we outsorce some doors from time to time we used a local repitable shop that make a lot of doors and same results.. i will try to post some picture's

7/9/21       #15: shaker doors ...
RODNEY BLACKERBY Member

edge sanded shaker door


View higher quality, full size image (640 X 480)

7/9/21       #16: shaker doors ...
Scott

Rodney,
How are you cutting or sizing your doors?
The picture you posted, to me there appears to be tear out, or at least that’s what it looks like to me.
I would maybe try making your doors a little long and cut them down to size on a sliding table saw if you have one.
You could put a coat of filler on before you edge sand, maybe something quick drying. I am not a fan of edge banding solid wood, especially the end grain like that, all your movement in your wood is parallel to your edge tape.

7/10/21       #17: shaker doors ...
TonyF

Rodney:

I agree with Scott, it appears that there is tearout on the rail component, almost as though the rails were left alone after machining, where some tearout occured, and the stiles were flush trimmed to the rails, with none of the rail being removed in the process.

The result appears such that while having been sanded, it is not necessarily smooth, as any paint would not fill those tearout areas, and they would stand out once everything was the same color.

As Scott mentions, you may consider making the doors a bit larger in all directions, and trim the doors on a panel saw, or a table saw with a sled, such that the excess stile and a bit of the rail are sawn off, and then sand the edge smooth after that.

Hope this helps. Good luck.
TonyF

7/12/21       #19: shaker doors ...
RODNEY BLACKERBY Member

We run all edge's with a shelix cutter head and then edgesand with 120 grit.

7/13/21       #20: shaker doors ...
Jim H

From the picture you posted, you've still got some end grain edge sanding to do.
I build doors 1/4" oversize, trim 1/8" off all sides on panel saw, then edge sand with 80 grit on four all four edges.
After that, it's on the finisher.

7/13/21       #21: shaker doors ...
Leo G Member

80 grit is a bit on the rough side.

I do 1/16" over and sand 1/32" from the top and bottom.

I do about 1/32" over size in width, sometimes more and sand that off. If it's more I run it through the jointer .007-.015" off per pass.

I edge sand with 120


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Western Dovetail
      Custom Made Dovetail Drawers
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • Centex Automation
      New and Used Machinery sales and service
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection

    Become a Sponsor today!