Door/drawer front panel.

10/18/22       
Jeff

So I don’t have much experience with garbage compactor panels, not a lot with cabinet panels in my area. The installation appears to be gimmicky as it is, there is so much play in the way the drawer moves in and out.
The owner wants the panel to look like a door and a drawer front. There is no support for the drawer front part, I am looking for some ideas on how to attach the drawer front to the top pf the door with a 3 mm gap in between them. I need something that provides a clean look. I was thinking of routering a piece of metal or aluminum in the back of the stiles and painting the metal the same color as the door. If anyone has any ideas or experience it would be appreciated.

10/19/22       #2: Door/drawer front panel. ...
Adam B

Is this panel painted or is it stained? If wood that is stained does grain direction matter? If possible I would build as 1 piece and route the groove you mentioned to make it appear that it is 2 pieces.

10/19/22       #3: Door/drawer front panel. ...
Tom Gardiner

I have routed two 2" wide grooves in the back of door drawers and glued in 3/8" thick hardwood leaving a gap between the doors. It works well to make a stiff structure. Good for stained or natural doors if you prefinish the doors, not so good for white doors because the bridging material shows if you paint it white or black.
I have also tried dominoes and they aren't strong enough to stiffen the door combo.

10/19/22       #4: Door/drawer front panel. ...
Jeff

Thanks for the info, the doors are white, regardless of what I use you will see something in the crack.
I was thinking of using dominos and also thinking of using dowels. Thanks for the information Tom, I only have the small domino so that definitely would'nt be strong enough. I do like the idea of the hardwood, that would finish up nicer than the metal or aluminum I was thinking of using, also easier to install as glue would be used instead of screws.

10/19/22       #5: Door/drawer front panel. ...
Leo G Member

Depending on the style of the door and drawer front I've made them as a single unit and then did a shallow saw kerf in place of the gap between them.

Or route a 1/4" deep section out of the back of the top of the door and bottom of the drawer front and glue a 1/4" pc of plywood in it.

10/20/22       #6: Door/drawer front panel. ...
Jeff

Leo,

I built the door and drawer front separate, I do like your idea and others about building one panel with a saw cut. In hind sight I would do that.

The piece of plywood sounds Like a good idea as well.

Thanks for the suggestions.

10/20/22       #7: Door/drawer front panel. ...
Leo G Member

Take a 3mm pc of wood and glue them together using it as a spacer. Maybe using a domino or two to provide a little extra strength.

Really depends on the stresses the two separate door/drawer fronts will be receiving. If they are secured nicely to the appliance door you don't have to worry much. If not, and you suspect they will use the drawer handle to open up the appliance then you might need a little more strength.

But we all know how strong glue is and a 3mm pc of wood is going to have almost zero flex.

10/25/22       #8: Door/drawer front panel. ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

Here's a good example.

The far left opening at the bottom is a trash roll out made to look like two paneled drawer fronts.

The next opening to the right, the top two are one unit for a dishwasher.

It does work better with paint obviously.


View higher quality, full size image (1024 X 683)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors

    Become a Sponsor today!