Subject: Re: light weight MDF spoil board causing problem?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

light weight MDF spoil board causing problem?

9/16/15       
Derek S.

For the first time, we have brought in some light weight MDF to use as our spoil board material. We are using this on a KOMO VR510 , single zone, flat bed router with a 40hp Traivaini vacuum. We received an error message that basically indicated there was a hole in our vacuum system, which there is not. It would not allow us to continue, so we threw the new panel down onto the old one, and have been running it that way.

Is it possible that the light weight MDF is so porous, the KOMO thinks the vacuum system has a hole?

9/16/15       #2: light weight MDF spoil board causin ...
Scott

I have had the same results with LDF i would suggest to switch back to MDF quickly.

9/16/15       #3: light weight MDF spoil board causin ...
Mike

Derek,
You are correct. If you want to use, LDF, I suggest starting with 1.5" thick. That will work until is thins too much and becomes more porous than at thicker dimensions. My opinion is, unless you have a lot of it, toss it in the dumpster, or make something out of it. Some guys really need the stuff based on their machine, but with a Komo and Travaini, you might just stick to regular MDF.

9/16/15       #4: light weight MDF spoil board causin ...
Derek S.

Interesting. Who would have thought you can have too much vacuum. We still lose parts from time to time, seems like a software change would allow us to maximize the benefits of 40hp and LDF.

Thanks for the feedback.

9/16/15       #5: light weight MDF spoil board causin ...
Stuart

Benefits?
There are no benefits using ldf.
I can only think of benefits when using mdf.
ldf is just a bad idea all round.

9/16/15       #6: light weight MDF spoil board causin ...
Derek S.

I assume that others are also using tactics such as onion skinning for parts under a specific square footage in order to avoid part loss. Would I not be able to decrease the required square footage for onion skinning if I had more suction? Afterall, onion skinning takes time. Or, would I not be able to decrease the loss of parts without changing my onion skinning setup? Isn't zero percent part loss the ultimate goal? Has everyone else achieved this and nobody bothered to tell me?

What are the other drawbacks to LDF? It's lighter and easier to handle, that seems like a positive.

9/16/15       #7: light weight MDF spoil board causin ...
Mike

I think we covered why LDF is not good. Tactics? Onion skin small parts, obviously, choose proper lead in places on the part, and order of which parts get cut from first to last. If you are willing to take the time to do that with logic, you will lose close to zero parts.

9/17/15       #8: light weight MDF spoil board causin ...
Snaglpuss

Covered how?
Just people saying it's no good and a bad idea.
Specifics?

9/17/15       #9: light weight MDF spoil board causin ...
Mike

Covered in that it is too porous in standard thicknesses. At 1.5" thick it is hard to find and expensive. I know, I used to source it at a previous company. At best, the parts held as well as MDF using a liquid ring pump, but as it thinned from surfacing, parts would begin to move even after banding the edges to minimize vacuum flow.

If you aren't sure, buy some yourself and give it a go.

9/17/15       #10: light weight MDF spoil board causin ...
Snaglpuss

Have been using 3/4 Lt.Weight with a 40hp pump for years.
Don't have anything moving unless the surface is extremely worn and munged up.
The only drawback I could see is it costs more than regular mdf or particle board, but the low number of sheets used makes that kind of a non-issue.

9/30/15       #11: light weight MDF spoil board causin ...
Evan Member

Website: http://www.near-west.com

The problems with LDF are partly related to its dimensional instability. It can gain or lose significant thickness with minor humidity changes throughout the day. This occurs with MDF as well but the higher resin content decreases the change somewhat.

While a rotary vane vacuum is capable of achieving a high maximum pressure, it falls off quickly once a few pieces have been cut through. The higher density spoilboard helps slow the volume of air therefore maintaining a higher hold down pressure.

My CNC uses a regenerative blower which supposedly can maintain a higher vacuum at a increased flow volume, so it works fine with LDF. In fact my machine seems to hold better with LDF (why I'm not sure). Since I started onion skinning anything under 2 square feet, I've hardly lost any parts.

10/1/15       #12: light weight MDF spoil board causin ...
Larry

I've got a KOMO 510 and a 40hp Quincy screw. Tried the LDF didn't see any advantages. We run 3/4" MDF Put a coat of finish on the edges and run it until its too thin to use. There seems to be a minimum penetration into the spoil board necessary to get a really clean bottom edge cut. I suspect it has to do with the dulling of the bit on the very bottom corners. So you have another trade-off, cut deeper or change bits more often. We have our software set to onion skin below a certain area. A lot less than 2 sq. ft. Long skinny parts are worse. I installed a large vacuum gage on the 4" line to the pump. The operator can see at a glance if it falls below 15". That seems to be the magic # for us.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.