Subject: Re: Tool life problems with laminated plywood

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Tool life problems with laminated plywood

4/4/21       
Arto Member

Hello.
Starting a production of hpl laminated 12mm birch plywood parts.
The nesting of the parts is real tight, so im using a 6mm tool.
The tool is a 2flute upcut carbide,im going 12m/min 18000rpm, straight through.

The problem is the spots where the tool touches the hpl wear ridiculously fast. I get like 120meters of cut out of a tool. Some of the cut is full width and some is not.

With a diamond tool of this size the machining speed would be ridiculously slow.

Any recommendations on this?

4/4/21       #2: Tool life problems with laminated p ...
Rob Young  Member

Website: http://www.nutekmachinery.com

You're running the feed rate at the upper limit according to chip load charts. To find the sweet spot for tool life you also need to consider the machine you are using. What make and model of CNC are you using? What is the acceleration/deceleration times for your machine? If you are using a smaller machine that requires more time and distance to speed up and slow down, you will be spinning the tool far too fast when cornering resulting in heat and tool wear. You may find that slowing down the spindle rpm and running at a lower feed rate will result in less heat on your cutting tools when cornering and longer tool life since the rpm will be closer the appropriate feed rate when cornering. All that being said, it is quite normal to see more tool wear where the tool cuts the laminate due to the abrasive nature of laminate. It may be possible for you to experience longer tool life though with tweaks to your spindle rpm and feed speeds.

4/4/21       #3: Tool life problems with laminated p ...
Oggie Member

Take a look at these posts/articles bellow and see if anything applies to your case.
As the Rob has said, most likely the heating of the bit is what needs to be addressed.

https://www.woodweb.com/knowledge_base/CNC_Bits_for_Cutting_HPL_Lami
nate.html

https://www.woodweb.com/knowledge_base/Extending_Bit_Life_in_Laminat
es.html

https://www.axyz.com/us/2018/04/23/how-to-cut-high-pressure-laminates/

https://www.woodweb.com/knowledge_base/Tooling_and_Settings_for_Machining_Lam
inated.html

https://www.woodweb.com/forum_fdse_files/cnc/795780.html

4/4/21       #4: Tool life problems with laminated p ...
routalot Member

I've found that PCD tools are the answer to materials that dull an ordinary edge.Whether you could find one with the ability to cut through your material is a different matter as the online information is a bit limited.

4/4/21       #5: Tool life problems with laminated p ...
BH Davis  Member

Website: http://www.bhdavis.net

Have you tried a vertical oscillation on the z-axis while cutting? This will spread the wear over a larger area of the bit and may reduce the heat build up.

BH Davis

4/6/21       #6: Tool life problems with laminated p ...
Arto Member

Thanks for the responses. The machine is a Homag baz.

In 2 of oggies links people recommended straight flute router bit style cutters. I think im gonna give those a go.

4/7/21       #7: Tool life problems with laminated p ...
Chuck Hicks Sponsor - Southeast Tool

Website: http://www.southeasttool.com

Have you tried any of the longer wear carbide spirals or coated tools?


View higher quality, full size image (1200 X 800)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.
    Sponsors
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • Colonial Saw
      North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
    • Onsrud Cutter
      Router Tooling for Woodworking, Plastic and Non-Ferrous Metal Manufacturers
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Machinery Associates
      Used Woodworking Machinery marketplace
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Holz-Her US Inc.
      Custom Edgebanders, Vertical Panel Saws, CNC Beam Saws, Wide Belt Sanders, CNC Point to Point Boring Machines, CNC Routers
    • JKL Machinery
      US Exclusive Importer Casadei, Busellato, Vitap, Bonacin - Machinery Dealer representing New & Used Woodworking Machinery
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.

    Become a Sponsor today!