RT Machine Co

CNC

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: compression bits

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

compression bits

12/18/24       
Eric Smith

We cut primarily commercial cabinets parts out of 3/4" thick laidup panels with liner on the back and plastic laminate on the face, also white melamine.

On a Weeke and a new Morbidelli X100. Currently using Vortex 3130XP compression bits.

Do you guys have any suggestions for a better / longer lasting bits? What about using bits designed to cut metal?

Thanks!

Eric

12/18/24       #2: compression bits ...
Stuart Douglas

We are using the same bit (xp) for 2 side prelams, and get about 15 sheets before the cut edge quality becomes burred. Using a Thermwood CS43. I use a regular 3830 on the white melamine and get about 50-60 sheets. I've thought about using a diamond bit, but our dust collection is less than stellar and I fear that I'll just cook that expensive bit rather than get increased cutting yield. Curious to hear what others are getting too...

12/18/24       #3: compression bits ...
Dropout Member

If you do 2 passes, use different bits. The finish one will last longer. When it wears out move it to roughing.

12/18/24       #4: compression bits ...
Karl E Brogger

Laminate is so hard on tools.

I use a 3189XP for mdf, melamine and laminate panels. 800ipm. I'd have to look in the controller but probably 16k rpm. I try and do arc'd toolpath corners as much as possible to eliminate dwell time. I believe that helps with tool longevity.

Laminate just piss pounds carbide.

If I did a lot, I'd switch to PCD, but I rarely cut much laminate, some melamine, and a fair amount of mdf.

If stay down is an option in whatever you're generating programs with, I believe that also helps a lot with tip wear not having to plunge as much

12/18/24       #5: compression bits ...
Mike

Karl,
If 16k is accurate, that is a big chipload(0.025). How is quality of cut and life of the bit? I have always tried to keep it at 0.0185- 0.020.

12/18/24       #6: compression bits ...
Mike McClaran

Best way is to decrease rpm until the cut is no good, then bump it back up by 500 rpm. Your chip should be cool and increase your bit life. Most wood workers are spinning 5k too much. The tooling guys love you the most.

12/18/24       #7: compression bits ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com
Mike, I'll have to look tomorrow at rpm. I meant to after I posted, and failed.

Life is acceptable. Never as much as you want, but what I can realistically accept? I rarely do a big run of any one material other than plywood which I've two tools that is all they cut. So I don't have hard data numbers. I feel like I'm in the ballpark with Stuart.
12/19/24       #8: compression bits ...
Chad R  Member

Website: http://www.northwayind.com
We have 5 nested base routers, Homag and Northwood. We also have a host of other cnc machines including 3 Homag BAZ's. I started testing PCD tooling many years ago with many vendors. I started testing with Leitz when a gentleman that I had known from the past stopped in working for Leitz at the time. Started testing 191031. It had a high squealing sound like it was going to break. We ended up sending our material to Germany for them to test. Our material turned out to be 20% more dense then German material. They came back to me with 22000 RPM and 20 MPM on their tool 191031. I'll admit, the tools get discolored when they are dull, probably the high RPM, but we are still way ahead of running carbide. We normally get 3 sharpening's on 12mm PCD. I discovered over the years to have one tool dedicated to melamine, and one tool dedicated to laminated material. The melamine tool lasts for weeks running 2 shifts a day. Don't ask me panel numbers, I don't know. We are a contract manufacturer, running different product every job. The tools are logged by machine and operator, and I see the tooling costs every week. I know we are way ahead of the carbide days. I've been working with another company called Wirutex. We are running a couple of their tools now. S14300 is their 12mm nested PCD tool. Having great success with that tool also. Forgot to mention, we are running all shrink fit HSK63F tool holders also.


View higher quality, full size image (1620 X 864)

12/19/24       #9: compression bits ...
Dylan Bayliss  Member

Website: http://www.machineconsult.com

Great post Chad, would love to connect on your success, we sell tools online and are a Leitz/Wirutex dealer, never had much success with PCD..if you have time would appreciate your insight to help others..
dylan@machineconsult.com
www.cnc-tool.com

12/19/24       #10: compression bits ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

Mike. Confirmed. I'm running those tools at 16k rpm
Makes me wonder if I should bump the rpm up 500 to see what affect it has.

I'm running my chip breakers for plywood at 18k rpm and around 600 IPM. Unless we hit something stupid in the plywood, I'm usually getting 100+ sheets out of the plywood tools.

I haven't touched the speeds and feeds on those tools in five or six years. One of those, "it's working, don't dick with it", things.

The shrink to fit tool holders intrigue me. I like the idea of taking some of the rotating mass out of the equation, and removing fail points. Removing mass has to help with spindle life and just overall smoothness. Not having to worry about a collet being worn, or somebody not torqueing something correct, or not cleaning the assembly prior to torqueing would be good as well.
What are the downsides?
I haven't looked to see what it costs to get setup with it.

12/19/24       #11: compression bits ...
Mike

Karl,
500rpm won't make much difference
800ipm with 2 flute @17k =0.0235
800ipm with 2 Flute @18k =0.022
800ipm with 2 flute @20k = 0.020
All spindles have a bell shaped power curve, so you lose significant horse power at higher rpm. Thats the downside of quicker speed. You might consider a 3 flute tool.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.
    Sponsors
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • Weinig Group-USA
      Wood Moulders and Knife Grinding Equipment
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • Mereen-Johnson Machine Company
      Manufacturers of High Production Woodworking Machinery
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Country Saw and Knife
      Complete Sharpening Services for Wood and Metal Saw Blades, Jointer Knives, and Bandsaw Blades
    • Onsrud Cutter
      Router Tooling for Woodworking, Plastic and Non-Ferrous Metal Manufacturers
    • ETK International
      New and Used Woodworking Machinery, Spare Parts and Superior Service
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!

    Become a Sponsor today!