RT Machine Co

CNC

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Drill bit replacement

3/10/15       
Bill

We use dowel construction on a nested router. We bore 8mm holes with carbide tipped bits. In our brief experience when the bits get dull they tend to wander and the hole becomes too large and inaccurate. Our solution is to swap out the bits based on time. We selected 1 month as that interval. We also found sharpening the bits was as expensive as buying new.

This can get expensive. Does anyone have a better approach?

3/10/15       #2: Drill bit replacement ...
B.H. Davis Member

I would first ask how many holes you are drilling in that one month period. If it is tens of thousands you are probably getting good life out of the bit if the change is only once a month.

Also what material you are drilling. Particle board will be much harder on bits that MDF. Plywood might be somewhere in the middle.

Then what feed and RPM rates you are using. You could be feeding too slow for the spindle RPM rate. Carbide doesn't hold up well to heat.

We actually do most of our hardwood cutting with high speed steel bits. This is because the way we need to hold down our solid wood parts would lead to failure at a high feed rate. As such we have to go at a slow feed rate with a higher than recommended RPM for the spindle. This makes for over heated bits. Since HSS stands up to overheating better than carbide we get just as much life from HSS bits as carbide bits at about 1/3 the cost.

Finally if all the above are all being properly handled then you could consider going to brad point instead of standard point bits. While more expensive, and no longer lasting than a standard bit, the points should keep the bit from wandering when it begins to dull.

BH Davis

3/10/15       #3: Drill bit replacement ...
Larry

You will get better life from solid carbide bits. That said I suspect you are using too slow of a Z-axis move or your machine is hesitating at the bottom of the cut. We also nest for dowel construction and get much longer life out of standard tipped dowel bits. Our machine runs 8 to 10 hours a day.

3/10/15       #4: Drill bit replacement ...
rich c.

Are you using a pecking cut, or one motion?

3/11/15       #5: Drill bit replacement ...
Bill

Using some fancy math we use 10,000 dowels a month. So we drill 10,000 vertical holes a month. We have 7 - 8mm drills in the drill head so each drill is boring around 1,500 holes a month. That is in theory, the drill head does not use the bits evenly.

We are using brad point bits @ 4500 rpm penetration of 2.5 m/min and exit of 2 M/min with 0 dwell.

We drill in one motion no pecking.

Our monthly change is fine, I believe we are well within the life of the bits. To find out the tipping point I would have to stretch it out until the holes get sloppy which is a problem when it happens.

Solid carbide is pricey we run those in our bore and Insert machine.

The material we are boring has a 1/8" MDF outer layer and a fir ply core. I think it is relatively hard on bits.

Are there any glaring errors here?

3/12/15       #6: Drill bit replacement ...
Mike

When I read your first post, my thought was tolerance in the drilling head. Are you able to tell if there is wear in the gearbox? I had a machine years ago that had drilling block issues. It was a bad design, and we changed out 3 or 4 of them. MP27 might ring a bell for those unlucky Busellato owners that had this particular multispindle unit. First thing I would do is check for any runout on each individual spindle in the extended position. Obviously the tools won't be under load, but it is a good place to start. Also, some of the drill spindles could have more wear than others. Good luck.

3/12/15       #7: Drill bit replacement ...
Larry

I checked to see about what we were getting for life on 8mm dowel bit. Our router has a small drill block so we only use one 8mm bit. Dowel useage is between 3 & 4000/ month. We process quite a lot of HPL laminated board and went to a kind of slow Z-move of only 50"/min. On melamine it is run @ 100"/min....4500 rpm, no dwell at bottom. Since the holes don't show the bit is run until it starts to chip the entry hole quite a bit. 3 months +- So we are getting around 10,000 holes per bit change. No exact records have been kept but I can look up how many dowels are bought and how many bits are bought and the results are similar. The bore and insert machine gets even longer life, but it doesn't have to drill through much melamine & no HPL. It also drills a lot faster, less than a second per hole.

3/13/15       #8: Drill bit replacement ...
cabinetmaker

We use dowel construction, also

4000 rpm for us. You really need to verify if all bits are being calibrated @ 70mm or 57mm or whatever all at the same time, then inserted into the head and verifying that all are drilling the same depth. I have 13 spindle head and a 20 spindle on our router. We change about every quarter and run up to 3 shifts when swamped including weekends.

Check the speed and length

3/16/15       #9: Drill bit replacement ...
Bill

We do very carefully calibrate the length of this bits. I picked one month after we ran into problems. I think I will move it to two and make sure the assemblers know we did that. If the holes start to become "loose" we will have to dial it back.

7/5/16       #10: Drill bit replacement ...
Aleks  Member

Hi Bill , maybe you need choose one TC grade speical for your own MDF material , tungsten carbide has so many grade and you can choose special one .


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.
    Sponsors
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • Colonial Saw
      North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
    • Onsrud Cutter
      Router Tooling for Woodworking, Plastic and Non-Ferrous Metal Manufacturers
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Machinery Associates
      Used Woodworking Machinery marketplace
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Holz-Her US Inc.
      Custom Edgebanders, Vertical Panel Saws, CNC Beam Saws, Wide Belt Sanders, CNC Point to Point Boring Machines, CNC Routers
    • JKL Machinery
      US Exclusive Importer Casadei, Busellato, Vitap, Bonacin - Machinery Dealer representing New & Used Woodworking Machinery
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.

    Become a Sponsor today!