We are running 3/4" thick laidup panels with white liner on the back, 11/16" pb substrate, and plastic laminate on the face - typically vertical grade. Cutting with a 3/8" compression bit, usually Amana.

We are buying a lot of new bits.

How many sheets should we get out of a bit? They can be sharpened, yes? How many sheets after sharpening?

Cutting speed and feed rate?

Thanks!

7/25/17       #2: bit life ...
Dropout Member

Lots of people will have lots of answers.

I like the coated FS tool bits.

They can be sharpened, and supposedly they run longer after sharpening. I don't keep track that closely. I just run them until the edge finish goes away.

16K RPM, 800 IPM, 2 passes mostly for dust control and because of small parts. Can easily run 1 pass.

7/25/17       #3: bit life ...
Stuart Douglas Member

I cut similar material and standard industrial grade melamine, as well as plywood. I've been using the Vortex tool 3130 and the 3130XP. I prefer the 3130 because the XP just seems to be a harder, and thus more brittle, grade of carbide. I had been using the Amanas but the vortex bits seem to last longer. I push these 2 flute bits @ full depth 600IPM, 14000 RPM. I get about 2 hrs of run time, or about 40 sheets. If you buy 25 at a time, there is a significant price reduction from vortex making these very economical. I get about 2 resharps out of them, and they are nearly as good as new each time.

7/26/17       #4: bit life ...
Chuck Hicks Member

Website: http://www.southeasttool.com

Eric,

Its hard to put a firm number on the number of sheets that you will get. Everyone's application is so different.
I will say that we are flute sharpening the coated bits which does not remove the coating on the diameter which does make them last longer.

We have had great results with our new coated bits in the 2017 catalog. We have had feed rates well over 1000 IPM. Feedback from the AWFS show, people are saying they went from running 40 boards to over 300.


View higher quality, full size image (1200 X 800)

7/30/17       #5: bit life ...
Maurice Phelps

Has any one thought of where the material is coming from, a lot of the material coming out of China has a lot of trash in its' composition, that I have seen contribute to reduced tool life.

Even a standard 123-MW from onsrud should give you a hundred plus panels with the right feeds and speeds.

7/31/17       #6: bit life ...
Larry

We have switched to the Onsurd Marathon coated bits. 16,000 @ 600", 2 flute. Much better life in HPL laminated panels. Any coated bit will lose its advantage when sharpened. How many sheets you can get depends a lot on what you consider an acceptable finish cut.

2/28/19       #7: bit life ...
Matt

This is an old thread but worth commenting on.

Our experience cutting melamine with 3/8" mortise compression bits like Vortex XP or Onsrud Marathon has shown us that the characteristics of the melamine you're cutting has as much to do with bit life as anything.

Overnight we went from getting 200+ sheets to barely 20. Sometimes only 5 or 6. This was domestic melamine (I won't name names or try to assasinate any brand, this was several years ago).

We switched melamine brands but left all other variables the same. Still a domestic melamine. Sheet count rose to a predictable 40, sometimes 60, but still DISMAL.

We then started suspecting our bits, so we tried several, none of them gave us better than 40-60 sheets.

Finally out of exasperation we tried a very high quality import from Chile. I've been cutting this product for 2 solid years now and I have only good things to say. We consistently exceed 200 sheets and rarely have defects in the melamine.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    ecabinet systems.com Thermwood Limtech Industries, Inc.