We are cutting 1.5" deep X .5" mortises in solid wood. (hickory cherry and maple) Can anyone share best router bit recommendation that has worked well for them? I am using a standard compression cutter that is designed for sheet stock and although it gives us a good finish we get some chatter and I feel a cutter with a shallower helix might be better? We are using a Thermwood CS45 router.

TIA
Gerry

3/21/18       #2: deep mortise bit ...
Jared Emery

If the mortises need to be dead on .500 wide, get an Onsrud 60-907 heavy hogger and have it sharpened down to .485 or so. It gets you the cutting length you need, and the larger diameter will minimize chatter. It won't give you the best finish, but if it's a mortise for gluing it won't matter. If you need a better finish get a 60-957, which is a chipper / finisher. These are both upcut bits, for use only if your hold-down method can hang onto the parts. Downcuts are also available, but you'll generate a lot of heat if you're packing chips into your mortises. If you haven't tried a hogger / chipbreaker, they're awesome at devouring wood quietly.

3/21/18       #3: deep mortise bit ...
Gerry

Thanks Jared that helps. I am cutting both .474" and .551" mortises 1.5" deep. I have been using a .5" compression cutter that is sharpened down to .460" The mortises are for loose tenons so finish is not a concern. I will try the serrated tooth design. I hate to have a new cutter ground down but it looks like that is the only option to get the .47" mortise 1.5" deep.

3/21/18       #4: deep mortise bit ...
SG

Machinist supply places (MSC, etc.) have end mills of more types, sizes, etc. than you can imagine. There are 15/32" end mills with 2" loc., and .5" shank that might work for you. There are roughing (serrated) versions, too, if you want to go that way - I'd be a little concerned about compromised glue surface, however. I've used 1" dia. 6" loc mills to mortise small timbers on my router and have had good results - but as Jared notes, be sure your fixturing is very secure when using up-flute bits. Chatter should be avoidable with less aggressive cut levels (again, as long as the fixturing is good). I don't think a down-flute would be advisable - lots of chips and heat.

3/22/18       #5: deep mortise bit ...
Paul Miller

Website: http://MCCWOODWORKING.COM

Definitely an upcut bit. I am not familiar with Thermwood, but are you cutting this in one pass or are you stepping it down? I always cut a mortise like this is two or even three passes. I might even stop the route to clean out the mortise.

3/22/18       #6: deep mortise bit ...
Gerry

Hi ,
SG, I will give that a look, there is a shop I buy aluminum bits from that has a good stock of end mills. I don't know how they differ from wood bits but maybe I can get some info from them.

Paul, I do cut the mortise in multiple passes and have gone to climb cut and this seems to reduce the chatter. I think the noise I am hearing may be because of the compression cutter not clearing the chips as it is the full depth pass where I hear it more. We have a vacuum table so I have a jig I built to hold the parts and it is vacuumed down to the table. It seems good and solid but it could allow some vibration I suppose.
Thanks,
Gerry

3/26/18       #7: deep mortise bit ...
Gary Dunne  Member

Website: http://www.shutterrevolution.com

We cut mortises that deep regularly. For 1/2" and wider we use a 1/2" 60-909 3 flute hogger. For the 3/8" and up mortises we use a 60-037 3/8" 3 flute hogger. The cut depth is limited to 1.125" but you can just cut the first 3/8" depth at -.005 stock to be left. This will create the clearance for the cutter shank without compromising the joint.

3/27/18       #8: deep mortise bit ...
Gerry

Gary,

So you over cut by .005 for the first .375" depth? Or am I not understanding.

Thanks,
Gerry

3/28/18       #9: deep mortise bit ...
Gary Dunne  Member

Website: http://www.shutterrevolution.com

That is correct. It is a way to create the mortise with a stock bit that has a limited cutting length. In your case the the depth of cut for the mortise exceeds the cut length of most of the off the shelf cutters. The initial 3/8" deep cut is to create clearance for the cutter shank. You can dial it down to just a couple of thousandths if needed.

On another note, we generally use a helical toolpath when making mortises.

3/29/18       #10: deep mortise bit ...
Gerry

Thanks Gary now I just need to find how to do a helical toolpath with Aspire.

Gerry


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA Limtech Industries, Inc.